会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明授权
    • Glass composition, glass substrate for flat panel display using the same, flat panel display, and method for producing glass substrate for flat panel display
    • 玻璃组合物,使用其的平板显示器用玻璃基板,平板显示器以及用于制造平板显示器用玻璃基板的方法
    • US08575050B2
    • 2013-11-05
    • US12969080
    • 2010-12-15
    • Akihiro KoyamaMikiko Hashimoto
    • Akihiro KoyamaMikiko Hashimoto
    • C03C3/091
    • C03C3/091
    • Provided is a glass composition suitable for a glass substrate for a flat panel display such as a liquid crystal display. This glass composition has high thermal stability, and is substantially free of BaO but has a low devitrification temperature. It is suitable for the production of a glass substrate by a downdraw process. This glass composition contains, in terms of mass %; 54 to 62% of SiO2; 4 to 11% of B2O3; 15 to 20% of Al2O3; 2 to 5% of MgO; 0 to 7% of CaO; 0 to 13.5% of SrO; 0 to 1% of K2O; 0 to 1% of SnO2; and 0 to 0.2% of Fe2O3, and is substantially free of BaO. In this glass composition, the total content of alkaline earth metal oxides (MgO+CaO+SrO) is 10 to 18.5 mass %. The devitrification temperature of the glass composition is 1200° C. or lower.
    • 提供一种适用于液晶显示器等平板显示器的玻璃基板的玻璃组合物。 该玻璃组合物具有高的热稳定性,并且基本上不含BaO但具有低失透温度。 适用于通过下拉工艺生产玻璃基板。 该玻璃组合物以质量%计含有 54〜62%的SiO2; 4〜11%的B2O3; 15〜20%的Al2O3; 2〜5%的MgO; 0〜7%的CaO; 0〜13.5%的SrO; 0〜1%K2O; 0〜1%的SnO2; 和0〜0.2%的Fe 2 O 3,并且基本上不含BaO。 在该玻璃组合物中,碱土类金属氧化物(MgO + CaO + SrO)的总含量为10〜18.5质量%。 玻璃组合物的失透温度为1200℃以下。
    • 4. 发明申请
    • Glass Article and Method of Producing the Same
    • 玻璃制品及其制造方法
    • US20090181843A1
    • 2009-07-16
    • US12084072
    • 2006-10-31
    • Hiromitsu SetoAkihiro KoyamaYukihito Nagashima
    • Hiromitsu SetoAkihiro KoyamaYukihito Nagashima
    • C03C3/095
    • C03C3/087C03C4/02Y10T428/315
    • The present invention provides a glass article using a glass composition including a base glass composition and colorants. The base glass composition includes, expressed in mass %: 65 to 80% of SiO2; 0 to 5% of Al2O3; 0 to 10% of MgO; 0 to 15% of CaO; 5 to 15% of MgO+CaO; 10 to 18% of Na2O; 0 to 5% of K2O; 10 to 20% of Na2O+K2O; and 0 to 5% of B2O3, and the colorants consist essentially of, expressed in mass %: 0.6% to 1.0% of T-Fe2O3; 0.026 to 0.8% of TiO2; 0 to 2.0% of CeO2; 0.01 to 0.03% of CoO; 0 to 0.0008% of Se; and 0.06 to 0.20% of NiO. The glass article has a grayish color tone, and has a visible light transmittance in a range of 15% to 40%, which is measured with the illuminant A at a thickness of 3.1 mm.
    • 本发明提供一种使用玻璃组合物的玻璃制品,所述玻璃组合物包括基础玻璃组合物和着色剂。 基础玻璃组成包括以质量%表示:65〜80%的SiO 2; 0〜5%的Al2O3; 0〜10%的MgO; 0〜15%的CaO; 5〜15%的MgO + CaO; 10〜18%的Na2O; 0〜5%K2O; 10-20%Na2O + K2O; 和0〜5%的B2O3,着色剂基本上由质量%表示:0.6%〜1.0%的T-Fe2O3; 0.026〜0.8%的TiO2; 0〜2.0%的CeO2; 0.01〜0.03%的CoO; 0〜0.0008%的Se; 和0.06〜0.20%的NiO。 玻璃制品具有灰色色调,并且具有15%至40%范围内的可见光透射率,其以3.1mm的厚度用光源A测量。
    • 10. 发明授权
    • Glass composition and substrate for information recording medium
    • 用于信息记录介质的玻璃组合物和底物
    • US06399527B1
    • 2002-06-04
    • US09401126
    • 1999-09-22
    • Shoichi KishimotoAkihiro KoyamaJunji KurachiNobuyuki Yamamoto
    • Shoichi KishimotoAkihiro KoyamaJunji KurachiNobuyuki Yamamoto
    • C03C3085
    • C03C3/085C03C3/087
    • A glass composition having a high Young's modulus and a low density is disclosed which can be mass-produced by a continuous process and easily made to have high surface smoothness. Also disclosed are a substrate including the glass composition and reduced in bending and resonance even upon high-speed rotation, a recording medium usable at a lower flying height, and an information recording device having a higher recording capacity and a shorter access time. The glass composition includes, in terms of mol %, 40 to 55% silicon dioxide (SiO2), 0.5 to 6% aluminum oxide (Al2O3), 2 to 20% lithium oxide (Li2O), 0 to 10% sodium monoxide ((Na2O), 2 to 30% R2O (R2O=Li2O+Na2O), 5 to 25% magnesium oxide (MgO), 0 to 25% calcium oxide (CaO), 0 to 10% strontium oxide (SrO), 10 to 40% RO (RO=MgO+CaO+SrO), 0 to 10% titanium dioxide (TiO2), and 0 to 5% zirconium oxide (ZrO2).
    • 公开了具有高杨氏模量和低密度的玻璃组合物,其可以通过连续工艺大量生产并且易于制成具有高表面平滑度。 还公开了包括玻璃组合物的基底,即使在高速旋转时减少弯曲和共振,可以在较低飞行高度下使用的记录介质,以及具有较高记录容量和较短访问时间的信息记录装置。 玻璃组合物以摩尔%计包含40至55%的二氧化硅(SiO 2),0.5至6%的氧化铝(Al 2 O 3),2至20%的氧化锂(Li 2 O),0至10%的一氧化钠((Na 2 O) ),2〜30%的R2O(R2O = Li2O + Na2O),5〜25%的氧化镁(MgO),0〜25%的氧化钙(CaO),0〜10%的氧化锶(SrO),10〜40%的RO (RO = MgO + CaO + SrO),0〜10%的二氧化钛(TiO 2)和0〜5%的氧化锆(ZrO 2)。