    • 53. 发明申请
    • Stabilizers for use in substantially light-insensitive thermographic recording materials
    • US20050255415A1
    • 2005-11-17
    • US11127645
    • 2005-05-12
    • Frank LouwetJohan Loccufier
    • Frank LouwetJohan Loccufier
    • G03C1/00G03C1/498
    • G03C1/4989G03C1/49845Y10S430/165Y10S430/166
    • A substantially light-insensitive black and white monosheet thermographic recording material comprising a support and a thermosensitive element, said thermosensitive element containing a substantially light-insensitive organic silver salt, an organic reducing agent therefor in thermal working relationship therewith, at least one binder and at least one stabilizer represented by formula (I): wherein R1, R2, R3 and R4 are independently selected from the group consisting of a hydrogen atom, halogen atoms and aliphatic, alkoxy, nitro, acyl, sulfonyl, nitrile, alkaryl, aryl, amino, thioalkyl, aldehyde, urea, —O—(C═O)-alkyl, —O—(C═O)-aryl, —O—(C═O)—O-alkyl, —O—(C═O)—O-aryl, —NH—(C═O)-alkyl, —NH—(C═O)-aryl, —(C═O)—NH-alkyl, —(C═O)—NH-aryl, —NH—(SO2)-alkyl, —NH—(SO2)-aryl, —(SO2)—NH-alkyl, —(SO2)—NH-aryl groups; X is represented by -A(-M)n or is selected from the group consisting of substituted aliphatic groups, unsubstituted aliphatic groups, substituted cycloaliphatic groups, unsubstituted cycloaliphatic groups, substituted aromatic groups and unsubstituted aromatic groups where in each of said groups one or more of the chain or ring carbon atoms may be substituted by one of more atoms selected from the group consisting of S, O, Si, N and P atoms; n is 2, 3 or 4; A is selected from the group consisting of substituted aliphatic groups, unsubstituted aliphatic groups, substituted cycloaliphatic groups, unsubstituted cycloaliphatic groups, substituted aromatic groups and unsubstituted aromatic groups where in each of said groups one or more of the chain or ring carbon atoms may be substituted by one of more atoms selected from the group consisting of S, O, Si, N and P atoms; each (-M) is independently a substituted or unsubstituted group selected from the group consisting of -(2-S-imidazole) groups and -(2-S-imidazole) groups annelated with an aromatic ring system, the optional substituents for -M being selected from the group consisting of halogen atoms and aliphatic, alkoxy, nitro, acyl, sulfonyl, nitrile, alkaryl and aryl groups.
    • 55. 发明授权
    • 3,4-alkylenedioxythiophenedioxide compounds and polymers comprising monomeric units thereof
    • 3,4-亚烷基二氧基噻吩二氧化物化合物和包含其单体单元的聚合物
    • US06927298B2
    • 2005-08-09
    • US10649761
    • 2003-08-27
    • Bert GroenendaalFrank LouwetHieronymus Andriessen
    • Bert GroenendaalFrank LouwetHieronymus Andriessen
    • C07D333/36C07D333/64C07D495/02C07D495/04C08G61/12C08G65/34C08G75/00C08G75/32
    • C07D495/04C08G61/126H01G11/48Y02E60/13
    • A 3,4-alkylenedioxythiophenedioxide compound represented by formula (I): in which: A represents a C1-5-alkylene bridge; R represents an optionally substituted C1-24-alkyl, C3-18-cycloalkyl, C1-18-alkoxy or polyethylene oxide group (optionally with at least one substituent selected from the group consisting of an alcohol, amide, ether, ester or sulphonate group) or an optionally substituted aryl group; a polymer comprising monomeric units represented by formula (I); an aqueous dispersion of a polymer comprising monomeric units corresponding to at least one compound according to formula (I) and a polyanion; a chemical polymerization process for preparing the aqueous dispersion comprising the steps of: (i) providing a solution of a polyanion; (ii) adding a compound according to formula (I) and a thiophene or pyrrole compound to the solution provided in step (i); and (iii) adding an oxidizing or reducing system to the mixture provided in step (ii); a printable paste containing the aqueous dispersion; an electroconductive layer containing the polymer; the use of the electroconductive layer in a light emitting diode; an antistatic layer containing the polymer; and an electroconductive pattern and a process for preparing the electroconductive pattern.
    • 由式(I)表示的3,4-亚烷基二氧基噻吩二氧化物化合物:其中:A表示C 1-5烷基亚烷基桥; R代表任选取代的C 1-14 - 烷基,C 3-18 - 环烷基,C 1-18 - 烷氧基或聚环氧乙烷基 (任选地具有至少一个选自醇,酰胺,醚,酯或磺酸酯基的取代基)或任选取代的芳基; 包含由式(I)表示的单体单元的聚合物; 包含对应于至少一种根据式(I)的化合物和聚阴离子的单体单元的聚合物的水分散体; 用于制备水分散体的化学聚合方法,包括以下步骤:(i)提供聚阴离子的溶液; (ii)将式(I)化合物和噻吩或吡咯化合物加入到步骤(i)中提供的溶液中; 和(iii)向步骤(ii)中提供的混合物中加入氧化或还原体系; 含有水分散体的可印刷浆料; 含有聚合物的导电层; 在发光二极管中使用导电层; 含有聚合物的抗静电层; 导电图案和制备导电图案的方法。
    • 57. 发明授权
    • Light-sensitive emulsion having (100) tabular grains rich in silver
chloride and method for preparing said grains
    • 具有(100)富含氯化银的片状颗粒的感光乳剂及其制备方法
    • US6136524A
    • 2000-10-24
    • US256239
    • 1999-02-24
    • Peter VerreptAnn VerbeeckFrank Louwet
    • Peter VerreptAnn VerbeeckFrank Louwet
    • G03C1/005G03C1/46G03C5/16G03C1/015
    • G03C1/0053G03C1/46G03C5/16
    • A light-sensitive silver halide photographic emulsion has been described, said emulsion comprising a colloidally stabilizing binder and {100} tabular silver halide grains containing at least 50 mole % of silver chloride, wherein at least 70% by number of all grains is provided by said tabular grains, exhibiting an average aspect ratio of at least 5 and an average equivalent circular grain diameter of at least 0.3 .mu.m, wherein said tabular grains have an average thickness of less than 0.25 .mu.m for at least 75% by number of all tabular grains.In order to prepare said emulsion a method has been disclosed comprising performing at least three distinct precipitation steps in an aqueous medium in a reaction vessel, followed by desalting by means of washing after flocculation or by means of ultrafiltration, wherein said three distinct precipitation steps consist of a nucleation step followed by a first and a second growth step, said method being further characterized by introducing in the said reaction vessel, after the first growth step, of a block-copolymer according to the formula (I) as described in the detailed description and in the claims.
    • 已经描述了感光卤化银照相乳剂,所述乳液包含胶体稳定粘合剂和含有至少50摩尔%氯化银的{100}片状卤化银颗粒,其中至少70%的全部颗粒由 所述片状颗粒的平均纵横比至少为5,平均当量圆形晶粒直径至少为0.3μm,其中所述片状颗粒的平均厚度小于0.25μm,至少75% 片状颗粒。 为了制备所述乳液,已经公开了一种方法,其包括在反应容器中的水性介质中进行至少三个不同的沉淀步骤,然后通过絮凝后的洗涤或通过超滤进行脱盐,其中所述三个不同的沉淀步骤包括 的成核步骤之后是第一和第二生长步骤,所述方法的特征还在于在第一生长步骤之后在所述反应容器中引入根据式(I)的嵌段共聚物,如详细描述的 描述和权利要求。
    • 58. 发明授权
    • Self-supporting or supported phosphor screen or panel
    • 自支撑或支撑荧光屏或面板
    • US5663005A
    • 1997-09-02
    • US688097
    • 1996-07-29
    • Philip DoomsMarc Van DammeFrank Louwet
    • Philip DoomsMarc Van DammeFrank Louwet
    • C09K11/02G21K4/00H01J29/22B32B5/16
    • H01J29/22C09K11/02G21K4/00G21K2004/08
    • A screen, comprising a self-supporting or supported phosphor layer with phosphor particles (PP) dispersed in a polymeric binder (B), said phosphor particles (PP) being present in said binder (B) in a volume ratio PP/B of at least 80/20 is provided wherein the polymeric binder comprises at least one polymer (P) having a T.sub.g .ltoreq.0.degree. C., an average molecular weight (MG.sub.avg) between 5000 and 10.sup.7, being soluble in ethylacetate for at least 5% by weight (% wt/wt) and a self-supporting layer of said polymer P comprising 82% by volume of phosphor particles and having a tickhess so has to comprise 100 mg of phosphor particles per cm.sup.2, has an elongation at break of at least 1%.The screen or panel shows low screen structure mottle and a very good compromise between speed and resolution.
    • 一种屏幕,其包括具有分散在聚合物粘合剂(B)中的荧光体颗粒(PP)的自支撑或支撑的荧光体层,所述荧光体颗粒(PP)以所述粘合剂(B)的体积比PP / B存在于所述粘合剂 提供至少80/20,其中聚合物粘合剂包含至少一种具有Tg <0℃的聚合物(P),5000至107之间的平均分子量(MGavg),可溶于乙酸乙酯至少5% (%wt / wt),并且包含82体积%荧光体颗粒并且具有棋子的所述聚合物P的自支撑层必须包含每平方厘米100毫克荧光体颗粒,其断裂伸长率至少为 1%。 屏幕或面板显示低屏幕结构斑点和速度和分辨率之间非常好的妥协。