    • RADIATION-CURABLE RESIN COMPOSITION, RADIATION-CURABLE COATING MATERIAL, AND METHOD FOR FORMING PROTECTIVE LAYER
    • 可辐射固化树脂组合物,可辐射固化涂料和形成保护层的方法
    • US20100104765A1
    • 2010-04-29
    • US12530070
    • 2008-03-04
    • Yohzoh YamashinaHiroyuki TokudaYouichi Tanimoto(none) DavidNobuyuki Koike
    • Yohzoh YamashinaHiroyuki TokudaYouichi Tanimoto(none) DavidNobuyuki Koike
    • C08L77/00C08F20/00C08G18/67C08J7/04
    • C09D175/16B05D3/067C08G18/3853C08G18/672C08G18/8125
    • An object of the present invention is to provide a radiation-curable coating material which forms a cured coating film having high hardness and low curing shrinkage, a radiation-curable resin composition for obtaining the radiation-curable coating material, and a method for forming a protective layer using the radiation-curable coating material. The present invention provides a radiation-curable resin composition including an urethane (meth)acrylate (A), which is obtained by reacting a bicyclo ring-containing polyisocyanate compound (a1), a hydroxyl group-containing, trifunctional or higher polyfunctional (meth)acrylate (a2) and a tris(2-hydroxyalkyl)isocyanurate di(meth)acrylate (a3); a radiation-curable coating material including the above resin composition; and a method for forming a protective layer, which includes: applying the above radiation-curable coating material onto a support to form a layer of the radiation-curable coating material thereon; and irradiating the layer of the coating material with radiation thereby curing the layer of the coating material to form a protective layer.
    • 本发明的目的是提供一种形成具有高硬度和低固化收缩率的固化涂膜的可辐射固化涂料,用于获得可辐射固化涂料的辐射固化树脂组合物,以及用于形成 使用可辐射固化涂层材料的保护层。 本发明提供一种含有双环环的多异氰酸酯化合物(a1),含羟基的三官能以上的多官能(甲基)丙烯酸酯化合物(甲基)丙烯酸酯(A) 丙烯酸酯(a2)和三(2-羟烷基)异氰脲酸酯二(甲基)丙烯酸酯(a3); 包含上述树脂组合物的可辐射固化涂料; 以及形成保护层的方法,其包括:将上述可辐射固化涂层材料施加到支撑体上以在其上形成可辐射固化涂层材料层; 并且用辐射照射涂层材料层,从而固化涂层材料层以形成保护层。
    • 43. 发明申请
    • Method of producing powdery coating material
    • 生产粉状涂料的方法
    • US20050218550A1
    • 2005-10-06
    • US11144011
    • 2005-06-03
    • Nobuyuki KoikeShojiro Kuwahara
    • Nobuyuki KoikeShojiro Kuwahara
    • C09D133/12C09D133/14B29B9/00C08L63/00
    • C09D133/14C08L2666/28
    • Disclosed is a method of producing a powdery coating material by using: a curable acrylic resin (A) having a number average molecular weight of from 2,000 to 20,000 and a glass transition temperature of from 30 to 90° C. obtained by polymerizing a starting monomer containing from 15 to 50 mol % of an unsaturated compound which contains at least a glycidyl group and/or a methylglycidyl group, and from 20 to 50 mol % of methyl methacrylate; a curing agent (B) capable of being reacted with the glycidyl group or the methylglycidyl group constituting the curable acrylic resin (A); and an alcohol solvent (C) having a boiling point under normal pressure of from 70 to 120° C.; said method comprising a kneading step of so kneading the curable acrylic resin (A), the curing agent (B) and the alcohol solvent (C) that at least the curing agent (B) is dissolved in the alcohol solvent (C) at a temperature of not higher than 130° C., and a vapor-removing step of continuously vapor-removing the alcohol solvent (C) under a reduced pressure at a temperature of not higher than 130° C.
    • 本发明公开了一种粉末状涂料的制造方法,其特征在于,使用下列方法:将数均分子量为2,000〜20,000,玻璃化转变温度为30〜90℃的固化性丙烯酸树脂(A) 含有15〜50摩尔%的至少含有缩水甘油基和/或甲基缩水甘油基的不饱和化合物和20〜50摩尔%的甲基丙烯酸甲酯; 能够与构成可固化丙烯酸树脂(A)的缩水甘油基或甲基缩水甘油基反应的固化剂(B) 和在常压下的沸点为70〜120℃的醇溶剂(C)。 所述方法包括将可固化丙烯酸树脂(A),固化剂(B)和醇溶剂(C)捏合的捏合步骤,至少将固化剂(B)溶解在醇溶剂(C)中, 温度不高于130℃,以及在不高于130℃的温度下在减压下连续蒸汽除去醇溶剂(C)的蒸气去除步骤。