    • 48. 发明授权
    • Current collector for molten salt battery, process for producing
material for said current collector, and molten salt battery using said
current collector
    • 用于熔融盐电池的集电器,用于生产用于所述集电器的材料的方法,以及使用所述集电器的熔融盐电池
    • US5972538A
    • 1999-10-26
    • US856316
    • 1997-05-14
    • Kazuo SaitoAtsushi Hagiwara
    • Kazuo SaitoAtsushi Hagiwara
    • H01M4/80H01M4/66H01M10/39
    • H01M10/399H01M4/663
    • A current collector for a molten salt battery using liquid sodium as an anode active material, which current collector has excellent electrolyte resistance and low electrical resistance and is able to be produced simply and rapidly at a low cost, and includes a current collector material in which a carbon composite material obtained by calcining a mixture of expanded powder with a thermosetting resin under a non-oxidizing atmosphere is bonded to a porous carbon material having a porosity of 99 to 30% and an average pore diameter of 0.5 mm to 5 .mu.m. The above current collector is produced by a process including bonding a carbon composite material obtained by calcining a mixture of an expanded graphite powder with a thermosetting resin under a non-oxidizing atmosphere, to a porous carbon material having a porosity of 99 to 30% and an average pore diameter of 0.5 mm to 5 .mu.m, or alternatively, bonding a carbon composite material precursor composed of a mixture of an expanded graphite powder with a thermosetting resin, to the above porous carbon material and then calcining the resulting assembly under a non-oxidizing atmosphere.
    • 使用液态钠作为负极活性物质的熔融盐电池用集电体,该集电体具有优异的耐电解性和低电阻,能够以低成本简单快速地制造,并且包括集电体材料,其中 通过在非氧化性气氛下将发泡粉末与热固性树脂的混合物煅烧而获得的碳复合材料与孔隙率为99〜30%,平均孔径为0.5〜5μm的多孔碳材料接合。 上述集电体是通过将非膨胀石墨粉末与热固化性树脂的混合物在非氧化性气氛下进行煅烧而得到的碳复合材料粘合到孔隙率为99〜30%的多孔碳材料上的工序, 平均孔径为0.5〜5μm,或者将由膨胀石墨粉末与热固性树脂的混合物组成的碳复合材料前体粘合到上述多孔碳材料上,然后在非水溶液下煅烧所得组合物, 氧化气氛。