    • 32. 发明授权
    • Grinding body for on-line roll grinding
    • 研磨体用于在线辊磨
    • US06220949B1
    • 2001-04-24
    • US09365714
    • 1999-08-03
    • Kanji HayashiMakoto SuzukiHiroshi Katagiri
    • Kanji HayashiMakoto SuzukiHiroshi Katagiri
    • B23F2103
    • B24D7/18B21B28/04B24B5/16B24D7/02
    • A grinding body for on-line roll grinding has a grindstone of a cup shape. The grindstone is on a surface portion, and near a peripheral edge, of a circular support base plate, so that a peripheral edge portion of the circular support base plate has on a surface side thereof a two-layer structure. This two-layered structure includes a flat ring-shaped portion jutting toward an inner periphery so as to define a groove opening inward. The grindstone is mounted on the flat ring-shaped portion; and a damping material is filled and mounted into the groove. This grinding body can effectively prevent the formation of a spiral mark and a pitching surface mark, improve the grinding power and grinding accuracy, and prolong the life of the grindstone.
    • 用于在线辊磨的研磨体具有杯形的磨石。 磨石位于圆形支撑基板的表面部分的周缘附近,使得圆形支撑基板的周边部分的表面侧具有两层结构。 该双层结构包括向内周侧突出的平坦的环状部分,以限定向内开口的槽。 磨石安装在平环形部分上; 并且阻尼材料被填充并安装到凹槽中。 该研磨体可有效防止形成螺旋痕和俯仰痕迹,提高研磨力和研磨精度,延长磨石寿命。
    • 34. 发明授权
    • Ink cartridge, process for forming it and liquid ink feeder
    • 墨盒,其成型工艺和液体墨水进料器
    • US6109743A
    • 2000-08-29
    • US998754
    • 1997-12-29
    • Masaki TakatsugiMakoto Suzuki
    • Masaki TakatsugiMakoto Suzuki
    • B41J2/175
    • B41J2/17523B41J2/17513
    • An ink cartridge takes the form of a bag, and is formed out of a laminate which includes films laminated together. Compressive stress exists in one of the films. Therefore, when a hollow needle pierces the bag, the stress causes this film to function in such a manner as to block the pierced hole. This brings the film into close contact with the needle, preventing ink leakage securely. It is also possible to prevent the cracks developed in the laminate by external injuries from progressing. It is possible to form the laminate by bonding a plurality of films having different coefficients of thermal expansion together at high temperature, and cooling the bonded films. It is possible to form the bag by heat-sealing the laminate.
    • 墨盒采取袋子的形式,并且由层叠在一起的层压体形成。 一种电影中存在压力应力。 因此,当中空针刺穿袋时,应力使得该膜以阻挡穿孔的方式起作用。 这使得胶片与针紧密接触,防止墨水泄漏牢固。 也可以防止由于外部伤害而在层压板中产生的裂纹发展。 可以通过在高温下将具有不同热膨胀系数的多个膜结合在一起形成层压体,并冷却粘合膜。 可以通过热封层压体来形成袋子。
    • 35. 发明授权
    • Toner fixing heater device having inclined heater electrode ends
    • 具有倾斜加热器电极端的调色剂定影加热器装置
    • US5958269A
    • 1999-09-28
    • US961026
    • 1997-10-30
    • Makoto SuzukiRikuzou Kouzuki
    • Makoto SuzukiRikuzou Kouzuki
    • G03G15/20H05B3/00H05B3/02H01R39/04
    • H05B3/0095G03G15/2053
    • In a toner-fixing heater device, a heater strip in a meandering pattern and a pair of heater electrodes are formed on an insulator film which is in turn fixed to a cylindrical roller body. Each heater electrode which slidably contacts a brush electrode has a leading and trailing edges formed inclinedly at an inclination angle .theta., e.g., 50.degree.. The axial width Wd of the heater electrode 14, the circumferential width Wg of a spacing between the leading and the trailing edges, and the circumferential width Wb of the brush electrode are determined to satisfy (Wd/tan .theta.+Wd).gtoreq.Wg. This arrangement assures a continuous sliding contact between the heater electrode and the brush electrode.
    • 在调色剂定影加热器装置中,在绝缘膜上形成蜿蜒图案的加热条和一对加热电极,绝缘膜又固定到圆柱形辊体上。 可滑动地接触刷电极的每个加热器电极具有以倾斜角θ(例如50°)倾斜地形成的前缘和后缘。 加热器电极14的轴向宽度Wd,前缘和后缘之间的间隔的周向宽度Wg和刷电极的周向宽度Wb被确定为满足(Wd /tanθ+ Wd)> / = Wg 。 这种布置确保了加热器电极和刷电极之间的连续的滑动接触。
    • 40. 发明授权
    • Resin composition for low expansion moldings
    • 低膨胀成型用树脂组合物
    • US5712319A
    • 1998-01-27
    • US523983
    • 1995-09-06
    • Makoto SuzukiOsamu Matsumoto
    • Makoto SuzukiOsamu Matsumoto
    • C08J9/06C08J9/00C08L27/06C08L33/04C08L33/06C08L51/00C08L51/04C08L51/06C08F16/06
    • C08J9/0061C08L27/06C08J2327/06C08L33/06C08L51/003
    • A resin composition for low expansion moldings which comprises (A) 20 to 80 parts by weight of a vinyl chloride resin having an average degree of polymerization of from 500 to 1700 and (B) correspondingly from 80 to 20 parts by weight of a copolymer made of 60 to 90 parts by weight a polymerizable monomer mixture consisting of 20 to 40 wt % of acrylonitrile, 20 to 60 wt % of .alpha.-methylstyrene and 20 to 40 wt % of styrene and, correspondingly, 40 to 10 parts by weight of a crosslinked acrylic rubber. The resin composition further comprises (C) 0.5 to 30 parts by weight of an acrylic resin having a reduced viscosity of not less than 3.0 dl/g when measured by use of a chloroform solution of the acrylic resin at a concentration of 0.1 g/100 ml, (D) 0.1 to 10 parts by weight of a thermally decomposable rosining agent, and (E) from 1 to 10 parts by weight of a stabilizer, each based on 100 parts by weight of a mixture of the components (A) and (B).
    • 一种低膨胀成型用树脂组合物,其包含(A)20〜80重量份的平均聚合度为500〜1700的氯乙烯树脂和(B)相应地为80〜20重量份的共聚物 60至90重量份由20至40重量%的丙烯腈,20至60重量%的α-甲基苯乙烯和20至40重量%的苯乙烯组成的可聚合单体混合物,相应地,40至10重量份的 交联的丙烯酸橡胶。 该树脂组合物还含有(C)0.5〜30重量份的当浓度为0.1g / 100的丙烯酸树脂的氯仿溶液测定时,比浓粘度不小于3.0dl / g的丙烯酸树脂 ml,(D)0.1〜10重量份的可热分解的发泡剂,和(E)1〜10重量份的稳定剂,各自基于100重量份的组分(A)和 (B)。