    • 12. 发明专利
    • Foam and method of manufacturing the foam
    • 泡沫和制造泡沫的方法
    • JP2009220355A
    • 2009-10-01
    • JP2008066399
    • 2008-03-14
    • Oji Paper Co Ltd王子製紙株式会社
    • ISHIDA TATSUJISHIMIZU JIRONISHIGORI YOSHIHARUOKAWA AKANEHIRANO DAISHINMUTO KUNIAKIMAEDA SHUICHI
    • B32B27/30B32B5/18C08J9/06
    • PROBLEM TO BE SOLVED: To provide a foam in which a support containing a polyester resin being inexpensive and excellent in solvent resistance and a foamed layer are adhered to each other with high adhesion and to provide a method of manufacturing the foam.
      SOLUTION: The foam 1 has the foamed layer 20 and the support 10 which are laminated through an anchor layer 30, wherein the support 10 contains at least polyester resin on its surface, the anchor layer 30 contains polycarbonate urethane resin and/or a polyether-polyurethane resin. Alternatively, the foam 1 has the foamed layer 20 further contains a structural unit derived from (meth)acrylic monomer. The method of manufacturing the foam 1 includes: a step of forming the anchor layer 30 on the support 10; a step of forming a foamable layer comprising a foamable composition on the anchor layer 30; and a step of obtaining the foamed layer 20 by foaming the foamable layer.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种泡沫,其中含有廉价且耐溶剂性优异的聚酯树脂的载体和发泡层彼此以高粘合性粘合并提供制造泡沫的方法。 解决方案:泡沫1具有通过锚定层30层压的发泡层20和支撑体10,其中支撑体10在其表面上至少包含聚酯树脂,锚定层30包含聚碳酸酯聚氨酯树脂和/或 聚醚 - 聚氨酯树脂。 或者,泡沫体1具有发泡层20还含有衍生自(甲基)丙烯酸类单体的结构单元。 制造泡沫1的方法包括:在支撑体10上形成锚定层30的步骤; 在锚层30上形成包含可发泡组合物的可发泡层的步骤; 以及通过使可发泡层发泡来获得发泡层20的步骤。 版权所有(C)2010,JPO&INPIT
    • 13. 发明专利
    • Coating solution for inkjet recording medium, and inkjet recording medium
    • 喷墨记录介质的涂料溶液和喷墨记录介质
    • JP2007118403A
    • 2007-05-17
    • JP2005314117
    • 2005-10-28
    • Oji Paper Co Ltd王子製紙株式会社
    • OKAWA AKANEMINAMI TAKEHIRO
    • B41M5/00B41J2/01B41M5/50B41M5/52
    • PROBLEM TO BE SOLVED: To provide a coating solution for an inkjet recording medium which forms a crack-free coating layer, increases a printing density on the inkjet recording medium having this coating layer, and also is excellent in the stability of itself, and also to provide the inkjet recording medium using this coating solution.
      SOLUTION: The coating solution of pH 8.0-9.5 is provided for forming the coating layer of the inkjet recording medium wherein the coating layer is formed on a base. The solution used herein contains at least a silica component having an average particle diameter of 10-700 nm, a binder component and an alkaline component which consists of a volatile alkaline component and a nonvolatile alkaline component.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供形成无裂纹涂层的喷墨记录介质的涂布溶液,增加了具有该涂层的喷墨记录介质上的印刷密度,并且其自身的稳定性优异 并且还提供使用该涂布溶液的喷墨记录介质。 解决方案:提供pH 8.0-9.5的涂层溶液,用于形成喷墨记录介质的涂层,其中涂层形成在基底上。 本文所用的溶液至少含有平均粒径为10-700nm的二氧化硅组分,由挥发性碱性组分和不挥发性碱性组分组成的粘合剂组分和碱性组分。 版权所有(C)2007,JPO&INPIT