    • 12. 发明专利
    • Organic arsenic compound-containing water treatment method
    • 有机砷化合物含水处理方法
    • JP2007038113A
    • 2007-02-15
    • JP2005224435
    • 2005-08-02
    • Kobe Steel Ltd株式会社神戸製鋼所
    • OTSUKA TSUYOKIIDA TORUANO SHINTARONAKAYAMA JUNPEI
    • C02F1/72C02F1/44C02F1/52
    • PROBLEM TO BE SOLVED: To provide a treatment method which can decompose water containing organic arsenic compounds derived from chemical weapons to a level harmless to the human body at a low cost regardless of the concentration of arsenic.
      SOLUTION: The treatment method of organic arsenic compound-containing water 1 containing one or more organic arsenic compounds selected from diphenylchloroarsine (DA), diphenylcyanoarsine (DC), bisphenyl arsineoxide (BDPAO), diphenyl arsinic acid (DPAA), and phenyl arsonic acid (PAA) comprises a first step for concentrating the organic arsenic compound-containing water 1 by a concentration means 2 to separate it into organic arsenic concentrated water 3 and detoxified water 4, and a second step for oxidatively decomposing the organic arsenic concentrated water 3 at a treatment temperature of 75-100°C by a chemical oxidation means 5 using an oxidizing agent.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:无论砷的浓度如何,都能以低成本提供一种能够将来自化学武器的含有机砷化合物的水分解成对人体无害的水平的处理方法。 解决方案:含有一种或多种有机砷化合物的选自二苯基氯胂(DA),二苯基氰基胂(DC),二苯基胂氧化物(BDPAO),二苯基亚砷酸(DPAA)和苯基的有机砷化合物的水1的处理方法 砷酸(PAA)包括通过浓缩装置2浓缩含有机砷化合物的水1以将其分离成有机砷浓缩水3和解毒水4的第一步骤,以及将有机砷浓缩水氧化分解的第二步骤 3,处理温度为75-100℃,使用氧化剂的化学氧化装置5。 版权所有(C)2007,JPO&INPIT
    • 14. 发明专利
    • Method for manufacturing solidified body
    • 制造固化体的方法
    • JP2003286066A
    • 2003-10-07
    • JP2002092063
    • 2002-03-28
    • Kobe Steel Ltd株式会社神戸製鋼所
    • IDA TORUNAKAO NOBORU
    • C04B28/18
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a solidified body by which hydrothermal solidified body of high strength can be manufactured by reducing blending amount of aggregate to the utmost and increasing blending amount of glass material.
      SOLUTION: The manufacturing method of the solidified body of high strength has a process in which the glass material, a calcium compound and water are blended to produce a mixture, a process in which the mixture is press-molded to produce a press-molding and a process in which the press- molding is subjected to hydrothermal solidification treatment to manufacture the solidified body. Further water content of the press-molding before the hydrothermal solidification treatment is adjusted to 10 to 40 mass%.
      COPYRIGHT: (C)2004,JPO
    • 要解决的问题:提供一种制造凝固体的方法,通过使玻璃材料的最大量和增加的共混量减少,可以通过降低骨料的混合量来制造高强度的水热凝固体。 解决方案:高强度固化体的制造方法具有混合玻璃材料,钙化合物和水以制备混合物的方法,其中将混合物压制成型以产生压制物的方法 以及将压制成型体进行水热凝固处理以制造凝固体的方法。 水热固化处理前的加压成形体的其他水分含量调整为10〜40质量%。 版权所有(C)2004,JPO
    • 15. 发明专利
    • Recovery method of permanent magnet, and device therefor
    • 永磁体的恢复方法及其装置
    • JP2012079947A
    • 2012-04-19
    • JP2010224297
    • 2010-10-01
    • Kobe Steel Ltd株式会社神戸製鋼所
    • YAMASHITA TAKESHIKAJIWARA KATSURAIDA TORU
    • H01F41/00B09B3/00H01F13/00H01F41/02H02K1/27H02K15/03
    • Y02W30/82
    • PROBLEM TO BE SOLVED: To provide a method capable of efficiently recovering a permanent magnet in a reusable form from a product including at least the permanent magnet, and to provide an useful device therefor.SOLUTION: The method comprises recovering a permanent magnet from a product after heat-treating in superheated steam the product including the permanent magnet as a component, such as a motor 10 or a dynamo. A device therefor comprises: a heat treatment furnace 11 in which the motor 10 or the dynamo including at least the permanent magnet is put and heated; a superheater 14 for generating superheated steam to be introduced into the heat treatment furnace 11; an exhaust pipe for exhausting the superheated steam supplied to the heat treat furnace 11 and an exhaust gas rising from a treated object; and a drain pipe for exhausting water stored in the heat treatment furnace 11.
    • 要解决的问题:提供一种能够从包括至少永磁体的产品中有效地回收可重复使用形式的永磁体的方法,并提供有用的装置。 解决方案:该方法包括在过热蒸汽中热处理产品中的永久磁铁,该产品包括作为组件的永久磁铁,例如电动机10或发电机。 其装置包括:热处理炉11,其中放置并加热至少包括永磁体的电机10或发电机; 用于产生将被引入到热处理炉11中的过热蒸汽的过热器14; 用于排出供给到热处理炉11的过热蒸汽的排气管和从被处理体上升的废气; 以及用于排出存储在热处理炉11中的水的排水管。版权所有(C)2012,JPO&INPIT
    • 16. 发明专利
    • METHOD FOR RECOVERING NbTi ALLOY
    • 回收NbTi合金的方法
    • JP2010132981A
    • 2010-06-17
    • JP2008311023
    • 2008-12-05
    • Kobe Steel Ltd株式会社神戸製鋼所
    • KUNII KAZUTAKAMIKI TAKASHIIDA TORU
    • C22B7/00C22B9/22C22B34/12C22B34/24C25C1/00
    • Y02P10/214
    • PROBLEM TO BE SOLVED: To provide a method for recovering an NbTi alloy where, when an NbTi alloy is recovered from an NbTi-based superconducting wire rod, which can be performed in a short time while evading the use of toxic gas and dangerous substance, and in which the residual concentration of Cu can be reduced as much as possible.
      SOLUTION: The method for recovering the NbTi alloy, in the method where the NbTi alloy is recovered from the superconducting wire rod comprising an NbTi alloy filament and Cu, comprises an electrolyzing process where the superconducting wire rod is electrolyzed so as to separate away Cu; and an electron beam melting process where the superconducting wire rod subjected to the electrolyzing stage is heated by an electron beam melting method so as to evaporate away Cu remaining in the surface of the NbTi alloy filament.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种回收NbTi合金的方法,其中当从NbTi基超导线材中回收NbTi合金时,其可以在短时间内进行,同时避免使用有毒气体, 危险物质,其中可以尽可能地减少Cu的残留浓度。 解决方案:NbTi合金从包含NbTi合金丝和Cu的超导线材回收的方法中的回收NbTi合金的方法包括电解过程,其中超导线材被电解以便分离 离开铜; 并且通过电子束熔化法加热经受电解阶段的超导线材的电子束熔化工艺,以便蒸发残留在NbTi合金细丝表面的Cu。 版权所有(C)2010,JPO&INPIT
    • 17. 发明专利
    • Method for treating waste
    • 处理废物的方法
    • JP2007268513A
    • 2007-10-18
    • JP2006175622
    • 2006-06-26
    • Earth Technica:KkKobe Steel Ltd株式会社アーステクニカ株式会社神戸製鋼所
    • NAKAO NOBORUIDA TORUTANAKA TAKESHIYAMAGISHI KENJI
    • B09B3/00B09C1/02B09C1/08C02F11/00C09K17/02C09K17/06C09K17/10C09K103/00
    • PROBLEM TO BE SOLVED: To provide a method for treating waste, by which a toxic substance can be restrained from being eluted from waste containing the toxic substance, particularly, boron, fluorine, selenium or chromium.
      SOLUTION: The method for treating waste comprises a mixing step of adding cement and lime to the waste containing the toxic substance and mixing them and a hydrothermal treatment step of subjecting the mixture obtained at the mixing step to hydrothermal treatment. The toxic substance is one or more of boron, fluorine, selenium and chromium. The ratio of the total amount of the cement and lime to be added to the waste to the amount of the waste is 5-60 mass%. The mass ratio of the amount of the lime to be added to the waste to the total amount of the cement and lime to be added to the waste is 0.1-0.9.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种处理废物的方法,通过该方法可以抑制有毒物质从含有毒物质,特别是硼,氟,硒或铬的废物中洗脱。 解决方案:处理废物的方法包括将混合步骤,将水泥和石灰加入到含有有毒物质的废物中并进行混合,并进行水热处理步骤,将混合步骤中得到的混合物进行水热处理。 有毒物质是硼,氟,硒和铬中的一种或多种。 要添加到废物中的水泥和石灰的总量与废弃物的量的比例为5-60质量%。 添加到废弃物中的石灰的质量比与添加到废物中的水泥和石灰的总量的质量比为0.1-0.9。 版权所有(C)2008,JPO&INPIT
    • 18. 发明专利
    • Treatment method of soil polluted with arsenic
    • 用ARSENIC污染的土壤处理方法
    • JP2006167617A
    • 2006-06-29
    • JP2004364404
    • 2004-12-16
    • Kobe Steel Ltd株式会社神戸製鋼所
    • IDA TORUMURAKAMI YUTAKAINADA YUTAKA
    • B09C1/02A62D3/33A62D3/38A62D101/24A62D101/43B09B3/00B09C1/06B09C1/08
    • B09C1/06B09C1/08
    • PROBLEM TO BE SOLVED: To provide a treatment method of soil polluted with arsenic by suppressing elution of arsenic to low enough to satisfy the ambient environmental quality standard by making the arsenic in the arsenic-polluted soil insoluble even if the compound form of arsenic in the arsenic-polluted soil is an organic arsenic compound or an inorganic compound of trivalent or pentavalent arsenic. SOLUTION: The treatment method of soil polluted with arsenic involves heating the arsenic-polluted soil at a temperature in a range from 200 to 700°C and adding and mixing a calcium compound and water to and with the heated arsenic-polluted soil. Alternatively, the treatment method of soil polluted with arsenic involves heating a mixture of the arsenic-polluted soil with a calcium compound at a temperature in a range from 200 to 700°C and adding and mixing water to and with the heated mixture. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:为了通过将砷的洗脱抑制到足够低以满足周围环境质量标准来提供用砷污染的土壤的处理方法,通过使砷污染土壤中的砷不溶,即使化合物形式 砷污染土壤中的砷是有机砷化合物或三价或五价砷的无机化合物。 解决方案:用砷污染的土壤处理方法包括在200〜700℃的温度范围内加热砷污染土壤,并向加热的砷污染土壤中加入和混合钙化合物和水 。 或者,用砷污染的土壤的处理方法包括将砷污染土壤与钙化合物的混合物在200-700℃的温度范围内加热,并将水与加热的混合物加入并混合。 版权所有(C)2006,JPO&NCIPI