热词
    • 1. 发明申请
    • COMPOSITION FOR SOLIDIFYING SOLID FOSSIL FUELS
    • 用于固体固体燃料的组合物
    • WO2008146977A1
    • 2008-12-04
    • PCT/KR2007/003430
    • 2007-07-13
    • YI, Kap Sok
    • YI, Kap Sok
    • C10L5/10
    • C10L5/105
    • Disclosed herein is a solidifying composition, which is added to a single solid fossil fuel or a mixture thereof to solidify the solid fossil fuels. The solidifying composition contains 34-52 wt% of straight asphalt, 0.1-0.3 wt% of an emulsifier for asphalt, 0.2-0.4 wt% of hydrochloric acid, 0.03-0.05 wt% of calcium chloride, and the balance of water. When this solidifying composition is used, a single solid fossil fuel or mixture thereof, including bituminous coal, anthracite coal and powdery coke, can be used as a raw material for coke. Also, even when the prior coke equipment, incurring a high equipment cost, is not used, it is possible to prepare coke, which can maintain the durability and high-temperature stability of coke prepared using the prior coking coal as a main raw material and which has a high heating value.
    • 本文公开了一种固化组合物,其被添加到单一固体化石燃料或其混合物中以固化固体化石燃料。 固化组合物含有34-52重量%的直沥青,0.1-0.3重量%的沥青乳化剂,0.2-0.4重量%的盐酸,0.03-0.05重量%的氯化钙和余量的水。 当使用这种固化组合物时,可以使用单一固体化石燃料或其混合物,包括烟煤,无烟煤和粉末状焦炭作为焦炭的原料。 此外,即使不使用现有的焦炭设备,导致高设备成本,也可以制备焦炭,其可以保持使用现有焦化煤作为主要原料制备的焦炭的耐久性和高温稳定性, 其具有高热值。
    • 3. 发明申请
    • COMPOSITION FOR SOLIDIFYING SOIL AND INDUSTRIAL WASTE
    • 用于固体土壤和工业废物的组合物
    • WO2008146979A1
    • 2008-12-04
    • PCT/KR2007/003432
    • 2007-07-13
    • YI, Kap Sok
    • YI, Kap Sok
    • C04B18/16
    • C04B26/26B09B3/0033B09C1/08C04B2111/00732C04B2111/00767C08L95/005C09K17/40Y02W30/91Y02W30/93Y02W30/94Y02W30/95C04B18/0418C04B18/12C04B18/14C04B18/16C04B22/062C04B22/124C04B24/085C04B24/24C04B24/2676C04B24/36C08L53/02
    • Disclosed herein is a composition for solidifying soil and industrial waste. The solidifying composition contains 16-24 wt% of straight asphalt, 0.06-0.10 wt% of an emulsifier for asphalt, 0.8-1.2 wt% of light oil, heavy oil or a mixture thereof, 0.01-0.03 wt% of calcium chloride, 0.8-1.2 wt% of lignin, 0.7-1.3 wt% of an acrylic emulsion-based asphalt modifier, 0.13-0.21 wt% of sodium hydroxide, 0.22-0.34 wt% of oleic acid, and the balance of water. A solidified material formed using this solidifying composition has increased density, strength and elasticity, improved durability and a short curing time. Furthermore, the solidifying composition enables soil and industrial waste to be recycled as a substitute for stone materials, such that it allows material sources to be readily secured in public or construction work fields, leading to a reduction in construction cost, and can also contribute to the preservation of the natural environment.
    • 本文公开了一种用于固化土壤和工业废物的组合物。 固化组合物含有16-24重量%的直沥青,0.06-0.10重量%的沥青乳化剂,0.8-1.2重量%的轻油,重油或其混合物,0.01-0.03重量%的氯化钙,0.8 -1.2重量%的木质素,0.7-1.3重量%的丙烯酸乳液基沥青改性剂,0.13-0.21重量%的氢氧化钠,0.22-0.34重量%的油酸和余量的水。 使用这种凝固组合物形成的固化材料具有增加的密度,强度和弹性,改进的耐久性和短的固化时间。 此外,固化组合物可使土壤和工业废弃物作为石材的替代物,从而允许材料来源在公共或建筑工地上容易地固定,导致施工成本降低,并且还可以有助于 保护自然环境。
    • 4. 发明申请
    • METHOD FOR SOLIDIFYING SOLID FOSSIL FUELS AND SOLIDIFIED MATERIALS PREPARED THEREBY
    • 固体石油燃料及其制备的固化材料的方法
    • WO2008146978A1
    • 2008-12-04
    • PCT/KR2007/003431
    • 2007-07-13
    • YI, Kap Sok
    • YI, Kap Sok
    • C10L5/10
    • C10L5/105
    • Disclosed herein are a method for solidifying solid fossil fuel and a solidified material obtained thereby. The solidified material is prepared by mixing at least one solid fossil fuel with 5-8 parts by weight, based on 100 parts by weight of the solid fossil fuel, of a solidifying agent, and 1-4 parts by weight, based on 100 parts by weight of the solidifying agent, of aqueous acrylic resin. When this solidifying method is used, a solidified material, which can maintain the durability and high-temperature stability of a solidified material according to the prior furnace process using only coking coal as a raw material and has high heating value, can be prepared using a single solid fossil fuel or mixture thereof, including bituminous coal, anthracite coal and powdery coke.
    • 本文公开了固体化石燃料的固化方法和由此获得的固化材料。 固化材料通过将至少一种固体化石燃料与基于100重量份的固体化石燃料和固化剂相混合的5-8重量份和基于100重量份的1-4重量份混合来制备 的固化剂,水性丙烯酸树脂。 当使用这种固化方法时,可以使用以下方法制备固化材料,其可以使用仅使用焦煤作为原料,并且具有高热值,根据现有的炉法,可以保持固化材料的耐久性和高温稳定性 单一固体化石燃料或其混合物,包括烟煤,无烟煤和粉末状焦炭。