    • METHOD FOR MANUFACTURING A MINERAL PANEL
    • 制造矿物面板的方法
    • WO1988005097A1
    • 1988-07-14
    • PCT/US1988000158
    • 1988-01-12
    • USG INTERIORS, INC.
    • USG INTERIORS, INC.IZARD, David, GrahamENGLERT, Mark, Howard
    • D21D03/00
    • D21J1/20D21F11/02D21H13/40D21H17/375
    • Method for the manufacture of structural mineral panels on a foraminous support wire (40) forming a dilute aqueous dispersion of mineral fiber and/or lightweight aggregate with some fiber and binder solids in water. A small amount of cationic flocculant such as polyacrylamide is added sufficient to effect coating of the binder solids onto the mineral fiber materials and the slurry is passed to a first flooded section (42) of the support wire (40) to form an open, entangled, structural mass having water in interstitial spaces of the entangled mass. Water is stripped from the mass and the mass dried substantially without collapse of the open structure, first by application of brief pulses of high vacuum (44) followed by further vacuum (46) and passing heated dry air (49) through the open entangled structure. This produces a very uniform homogeneous panel core with very evenly spaced and uniformly sized voids in the open cored structure.
    • 在多孔支撑线(40)上制造结构矿物面板的方法,其形成矿物纤维和/或轻质骨料的稀水分散体,其中一些纤维和粘合剂固体在水中。 加入少量的阳离子絮凝剂如聚丙烯酰胺足以使粘合剂固体涂覆到矿物纤维材料上,并将浆料通入支撑丝(40)的第一淹没部分(42)以形成开放的,缠结的 ,在缠结块的间隙中具有水的结构物质。 水从质量中剥离,质量基本上干燥而不会破坏开放结构,首先通过施加高真空(44)的短脉冲,接着进一步的真空(46)并通过加热的干燥空气(49)通过开放的缠结结构 。 这产生非常均匀的均匀的面板芯,其在开放的芯结构中具有非常均匀间隔且均匀尺寸的空隙。