    • 1. 发明申请
    • PROCESS FOR PRODUCING SILVER NANOWIRES
    • 用于生产银纳米线
    • WO2012022332A3
    • 2012-07-05
    • PCT/DE2011075155
    • 2011-07-01
    • RENT A SCIENTIST GMBHNUSKO ROBERTMAIER GEORGKAISER THEO
    • NUSKO ROBERTMAIER GEORGKAISER THEO
    • B22F9/24B22F1/00
    • B22F1/0025B22F9/24B82Y30/00
    • The present invention provides a process for producing silver nanowires. The process comprises the steps of: a) providing a reaction mixture comprising a polyol, an organic chemical which is adsorbed on a silver surface, a chemical which forms a halide and/or one which forms a pseudohalide, the halide-forming chemical being a salt of one of the halides Cl-, Br- and/or I-, and the pseudohalide-forming chemical being a salt of one of the pseudohalides SCN-, CN-, OCN- and/or CNO-, a chemical which forms a redox pair and is selected from the group consisting of bromine, iodine, vanadium and mixtures thereof, b) adding a silver salt in an amount such that the concentration of silver in the reaction mixture is at least 0.5% by weight, based on the total weight of the reaction mixture, the silver salt being added at a temperature of the reaction mixture of at least 100°C, c) maintaining the temperature of the reaction mixture of 100°C for the duration of the reaction.
    • 本发明提供了一种生产可用的银纳米线的方法。 该方法包括以下步骤:a)提供一种反应混合物,其包含多元醇,吸附到银表面有机化学,卤化物和/或拟卤化物形成化学,其中该卤化物形成化学是卤化物中的一个的盐 Cl,Br和/或I是和其中形成拟卤化物化学品是一种拟SCN,CN,OCN和/或CNO,氧化还原对形成化学的从所选择的一种盐 自由溴,碘,钒和它们的混合物)的基团为b的量加入银盐,使得基于反应混合物的总重量,添加银盐的至少0.5重量%的银的在反应混合物中的浓度 在至少100℃的反应混合物温度下进行,c)保持至少1的反应混合物温度 00℃进行反应的持续时间。