热词
    • 6. 发明申请
    • TITANIUM ALLOYS
    • 钛合金
    • WO2012021186A2
    • 2012-02-16
    • PCT/US2011/034608
    • 2011-04-29
    • QUESTEK INNOVATIONS LLCWRIGHT, James, A.SEBASTIAN, JasonJOU, Herng-Jen
    • WRIGHT, James, A.SEBASTIAN, JasonJOU, Herng-Jen
    • C22C14/00B22D25/06
    • B22D25/00C22C1/02C22C14/00C22F1/183
    • Provided herein are titanium alloys that can achieve a combination of high strength and high toughness or elongation, and a method to produce the alloys. By tolerating iron, oxygen, and other incidental elements and impurities, the alloys enable the use of lower quality scrap as raw materials. The alloys are castable and can form -phase laths in a basketweave morphology by a commercially feasible heat treatment that does not require hot-working or rapid cooling rates. The alloys comprise, by weight, about 3.0% to about 6.0% aluminum, 0% to about 1.5% tin, about 2.0% to about 4.0% vanadium, about 0.5% to about 4.5% molybdenum, about 1.0% to about 2.5% chromium, about 0.20% to about 0.55% iron, 0% to about 0.35% oxygen, 0% to about 0.007% boron, and 0% to about 0.60% other incidental elements and impurities, the balance of weight percent comprising titanium.
    • 本文提供了可实现高强度和高韧性或延伸率的组合的钛合金以及制造这些合金的方法。 通过耐受铁,氧和其他附带元素和杂质,这些合金能够使用低质量的废料作为原材料。 这些合金是可铸造的,并且可以通过商业上可行的热处理形成织网形态的相板条,所述热处理不需要热加工或快速冷却速率。 所述合金包含按重量计约3.0%至约6.0%的铝,0%至约1.5%的锡,约2.0%至约4.0%的钒,约0.5%至约4.5%的钼,约1.0%至约2.5%的铬 ,约0.20%至约0.55%的铁,0%至约0.35%的氧,0%至约0.007%的硼和0%至约0.60%的其他附带元素和杂质,其中重量百分比包括钛。 >