    • 1. 发明申请
    • THE METHOD FOR MANUFACTURING THIN STEEL SHEET FOR DEEP DRAWING HAVING EXCELLENT WORKABILITY
    • 制造具有良好工作性能的深层薄钢板的方法
    • WO2008078901A1
    • 2008-07-03
    • PCT/KR2007006628
    • 2007-12-18
    • POSCOKANG HEE JAECHIN KWANG GEUNSOHN IL RYOUNG
    • KANG HEE JAECHIN KWANG GEUNSOHN IL RYOUNG
    • C21D8/02
    • C21D9/48C21D8/0426C21D8/0436C21D8/0463C21D8/0473C23C2/02C23C2/06C23C2/28
    • There is provided a method for manufacturing a thin steel sheet for deep drawing having excellent workability that is generally used for inner and outer panels of an automobile body. A method includes reheating steel slabs containing, by weight%, C: 0.010% or less, Si: 0.4% or less, Mn: 0.06-1.5%, P: 0.03-0.15%, S: 0.020% or less, Sol. Al: 0.40% or less, N: 0.010% or less, Ti: 0.003-0.05%, Nb: 0.003-0.05%, Mo: 0.10% or less, B: 0.0002-0.0030%, one or both of Sb: 0.005-0.10% and Sn: 0.005-0.10%, the balance Fe, and unavoidable impurities, completing finish rolling the reheated steel slabs at the single phase austenite region while a reduction ratio of rough rolling and finish rolling is in the range of 1.0 (50%:50%)-4.0 (80%:20%), and strip- cooling rate of final three pass is 30°C/sec or more during finish rolling, coiling the finish rolled steel sheet, cold rolling the coiled hot-rolled steel sheet at a cold rolling reduction ratio of 60% or more, and continuously annealing the cold-rolled steel sheet at a temperature of a range of 780-8600C, in which the average size of precipitates satisfies 20-60 nm. As described above, according to the embodiment of the present invention, it is possible to provide a thin steel sheet for deep drawing having tensile strength of 28-50 kg/mm and more excellent workability and galvanizing properties than a thin steel sheet for deep drawing according to the related art.
    • 提供一种用于制造用于深冲压的薄钢板的方法,该方法通常用于汽车车身的内外板。 一种方法包括以重量%计含有C:0.010%以下,Si:0.4%以下,Mn:0.06〜1.5%,P:0.03〜0.15%,S:0.020%以下的钢坯。 Al:0.40%以下,N:0.010%以下,Ti:0.003〜0.05%,Nb:0.003〜0.05%,Mo:0.10%以下,B:0.0002〜0.0030%,Sb:0.005〜 0.10%,Sn:0.005〜0.10%,余量为Fe和不可避免的杂质,在单相奥氏体区域中完成对再热钢坯的精轧,而粗轧和精轧的压下率在1.0(50% :50%) - 4.0(80%:20%),最终三遍的剥离冷却速度在精轧过程中为30℃/秒以上,卷取精轧钢板,冷轧卷取的热轧钢 在冷轧压下率为60%以上的条件下,在780〜8600℃的范围内连续退火冷却钢板,其中析出物的平均粒径为20〜60nm。 如上所述,根据本发明的实施方式,能够提供拉伸强度为28〜50kg / mm的深拉伸用薄钢板和与深冲的薄钢板相比具有更优异的加工性和镀锌性 根据现有技术。