    • CONCRETE WITH A LOW CLINKER CONTENT
    • 低熟料含量的混凝土
    • WO2010112687A3
    • 2010-11-25
    • PCT/FR2010000243
    • 2010-03-23
    • LAFARGE SASCHWARTZENTRUBER ARNAUDMARTIN MYLENEBENARD PHILIPPESABIO SERGE
    • SCHWARTZENTRUBER ARNAUDMARTIN MYLENEBENARD PHILIPPESABIO SERGE
    • C04B28/04C04B40/00
    • C04B28/04C04B40/0042C04B2111/00051Y02P40/146Y02W30/92Y02W30/94C04B14/06C04B14/106C04B14/108C04B14/28C04B18/08C04B18/141C04B18/146C04B20/008C04B22/147C04B2103/0088C04B2103/32C04B24/2647C04B7/527
    • The present invention relates to a dry binder premix including, in weight proportions: Portland clinker with a Blaine specific surface area of between 4500 and 9500 cm2/g, preferably between 5500 and 8000 cm2/g, the minimum amount of said clinker in weight percent relative to the total weight of the premix being determined according to the following formula (I): [-6.10-3 x SSBk] + 75 where SSBk is the Blaine specific surface area of the clinker in cm2/g; fly ash; at least one alkaline sulphate, the amount of alkaline sulphate being such that the equivalent amount of Na2O in the premix is at least equal to 5 wt % relative to the weight of fly ash; at least one source of SO3, in an amount such that the amount of SO3 in the premix is at least equal to 2 wt % relative to the weight of the Portland clinker; additional materials having a Dv90 at most equal to 200 µm selected from among limestone powders, calcined schists, metakaolins, silica fillers, silica powders, pozzolanas, slag, fly ash and mixtures thereof; the amount of clinker plus the amount of fly ash being at least equal to 75 wt %, preferably 78 wt %, relative to the total weight of the premix; the total amount of clinker in the premix being strictly less than 60 wt % relative to the total weight of the premix. The invention also relates to a dry binder mix produced by mixing the preceding premix with aggregate, as well as to a wet concrete composition produced by mixing with water.
    • 本发明涉及一种干粘结剂预混物,其按重量比例包括:勃氏比表面积为4500-9500cm 2 / g,优选5500-8000cm 2 / g的波特兰熟料,所述熟料的最小量以重量百分比计 相对于预混物的总重量根据下式(I)确定:[-6.10-3×SSBk] +75其中SSBk是熟料的布莱恩比表面积,单位为cm2 / g; 粉煤灰 至少一种碱性硫酸盐,所述碱性硫酸盐的量使得所述预混物中等量的Na 2 O相对于飞灰的重量至少等于5重量%; 至少一种SO3源,其用量使得预混物中SO3的量相对于波特兰熟料的重量至少等于2wt%; 选自石灰石粉,煅烧片岩,偏高岭土,二氧化硅填料,二氧化硅粉末,火山灰,矿渣,粉煤灰及其混合物的Dv90最多等于200μm的其他材料; 熟料的量加上飞灰的量相对于预混物的总重量至少等于75重量%,优选78重量%; 预混物中熟料的总量严格小于预混物总重量的60重量%。 本发明还涉及通过将前述预混物与骨料混合而制得的干粘合剂混合物,以及通过与水混合制得的湿混凝土组合物。