    • FRICTION STIR WELDING METHOD FOR STRUCTURAL STEEL AND METHOD OF MANUFACTURING JOINT FOR STRUCTURAL STEEL
    • 结构钢的摩擦焊接方法和结构钢制造接头的方法
    • WO2015045299A8
    • 2016-03-24
    • PCT/JP2014004657
    • 2014-09-10
    • JFE STEEL CORP
    • MATSUSHITA MUNEOTANIGUCHI KOICHIIKEDA RINSEI
    • B23K20/12
    • B23K20/1235B23K20/129
    • The purpose of the present invention is to advantageously address reverse flow failures due to insufficient heating of materials to be processed when carrying out friction stir welding of structural steel, to give sufficient strength, and also to improve connection construction. In the present invention, a preheating treatment process is carried out during friction stir welding of structural steel, said preheating treatment process being a process wherein a steel sheet (3), which is the material to be processed, is heated by a heating means (5) provided forward of a rotary tool (1) that moves in a joining direction. The present invention is configured so that the surface temperature, surface area, position, and the like for the heating region in the preheating treatment process are strictly controlled.
    • 本发明的目的是为了有效地解决由于在进行结构钢的摩擦搅拌焊接时提供待处理材料的不充分加热而产生的逆流故障,以提供足够的强度,以及改进连接结构。 在本发明中,在结构钢的摩擦搅拌焊接中进行预热处理工序,所述预热处理工序是将被加工材料的钢板(3)加热的方法( 5)设置在沿连接方向移动的旋转工具(1)的前方。 本发明被配置为严格控制预热处理过程中的加热区域的表面温度,表面积,位置等。
    • 3. 发明申请
    • RESISTANCE SPOT WELDING METHOD
    • 电阻点焊方法
    • WO2015083381A8
    • 2016-03-03
    • PCT/JP2014006074
    • 2014-12-04
    • JFE STEEL CORP
    • TANIGUCHI KOICHIOKITA YASUAKIIKEDA RINSEI
    • B23K11/16B23K11/11B23K11/24
    • B23K11/115B23K11/0026B23K11/166B23K2201/006B23K2201/18B23K2201/34B23K2203/04
    • When resistance spot welding a set of plates obtained by overlapping a plurality of steel plates comprising one or more steel plates having, on the surface thereof, a plating layer having zinc as the principal component thereof, a nugget having sufficient diameter is stably formed without any splashing, by: (1) starting conduction while in a state in which t and L satisfy the relational expression 0.9×t≤L≤1.1×t, given that the total thickness of the overlapping steel plates is t, and the distance of the center interval between top and bottom electrodes is L; and (2) dividing the conduction into a main conduction and an initial conduction preceding the main conduction, and with the initial conduction treated as two stages of conduction, setting the current value (I1) in the first conduction stage of the initial conduction so as to fall into a range satisfying, in a relationship with the current value (Im) of the main conduction, Im×1.1≤I1≤15.0kA, and setting the current value (I2) in the subsequent second conduction stage to be off or to be low-current conduction so as to satisfy 0≤I2≤Im×0.7.
    • 当通过重叠包含一个或多个在其表面上具有锌作为其主要成分的镀层的一个或多个钢板的多个钢板而获得的一组板的电阻点焊时,稳定地形成具有足够直径的熔核,而没有任何 通过以下方式飞溅:(1)在t和L满足关系式0.9×t≤L≤1.1×t的状态下,考虑到重叠钢板的总厚度为t,并且 顶部和底部电极之间的中心间隔为L; 和(2)将导通分为主导通和主导通之前的初始导通,并且将初始导通处理为两级导通,将初始导通的第一导通阶段中的电流值(I1)设置为 以与主导通电流Im的关系Im×1.1≤I1≤15.0kA为基准,并将随后的第二导通级中的电流值(I2)设定为截止或为 为低电流导通,满足0≤I2≤Im×0.7。