    • 1. 发明申请
    • PHOSPHOROUS PENTOXIDE PRODUCING METHODS AND PHOSPHATE ORE FEED AGGLOMERATES
    • 磷酸二氢生产方法和磷酸盐饲料饲料
    • WO2013081999A1
    • 2013-06-06
    • PCT/US2012/066597
    • 2012-11-27
    • JDCPHOSPHATE, INC.MEGY, Jospeh A
    • MEGY, Jospeh A
    • C01B25/12
    • C01B25/12
    • A phosphorous pentoxide producing method includes forming a reducing kiln bed using feed agglomerates containing a lignin sulfonate both inside the agglomerates and coating a surface of individual agglomerates. Freeboard particulates are generated from the agglomerates, an amount of particulates generated being less than would occur in the method with no lignin sulfonate. Kiln off gas is generated and phosphorous pentoxide is collected from the kiln off gas. The kiln discharges a residue containing processed agglomerates, less than 20% of the agglomerates' phosphate input to the kiln remaining in the residue. The percentage of input phosphate that remains in the residue is less than would occur in the method with no lignin sulfonate. The method may include forming green agglomerates. Controlling a drying rate of the green agglomerates may wick some of the lignin sulfonate onto the surface of individual drying agglomerates without adhering the agglomerates together.
    • 五氧化二磷生产方法包括使用在附聚物内部含有木质素磺酸盐的进料团聚体并涂覆单个附聚物的表面来形成还原窑床。 从附聚物产生刨花板颗粒,所产生的颗粒的量少于在不含木质素磺酸盐的方法中发生的颗粒。 产生窑尾气体,从窑尾气中收集五氧化二磷。 窑炉排出含有加工过的附聚物的残留物,剩余残留物中残留的窑内少于20%的聚集体磷酸盐。 留在残留物中的磷酸盐的百分比小于不含木质素磺酸盐的方法。 该方法可以包括形成绿色附聚物。 控制绿色附聚物的干燥速率可将一些木质素磺酸盐吸附到各个干燥附聚物的表面上,而不将附聚物粘附在一起。