    • 1. 发明申请
    • CONVERSION TREATMENT METHOD AND COMPOSITION FOR ALUMINUM AND ALUMINUM ALLOYS
    • 铝和铝合金的转化处理方法和组合
    • WO1991013186A1
    • 1991-09-05
    • PCT/US1991000965
    • 1991-02-13
    • HENKEL CORPORATIONYOSHIDA, MasayukiNAKADA, Kazuya
    • HENKEL CORPORATION
    • C23C22/38
    • C23C22/38
    • The paint adhesion and corrosion resistance of surfaces of aluminum and its alloys, particularly when using a paint based on poly(vinyl chloride), is improved by using a conversion coating solution having a pH in the range from 1.0 to 3.0 and containing: (A) an amount of phosphate ions that is stoichiometrically equivalent to at least 5.0 g/L of phosphoric acid; (B) at least 1.0 g/L of hexavalent chromium; (C) at least 0.1 g/L of fluoride ions; and (D) a complex fluoride ion component selected from the group consisting of: (i) at least 4.0 g/L of fluosilicate ions, (ii) at least 0.5 g/L of fluoborate ions, (iii) at least 2.0 g/L of fluozirconate ions, and (iv) at least 2.0 g/L of fluotitanate ions.
    • 通过使用pH为1.0-3.0的转化涂层溶液,并且包含:(A(A)),改善了铝及其合金表面,特别是使用基于聚(氯乙烯)的涂料时的表面的油漆附着力和耐腐蚀性。 )磷酸盐离子的化学计量相当于至少5.0g / L的磷酸; (B)至少1.0g / L六价铬; (C)至少0.1g / L的氟离子; 和(D)选自以下的复合氟离子组分:(i)至少4.0g / L的氟硅酸盐离子,(ii)至少0.5g / L的氟硼酸根离子,(iii)至少2.0g / L的氟锆酸根离子,和(iv)至少2.0g / L的氟钛酸根离子。
    • 5. 发明申请
    • COMPOSITION AND PROCESS FOR TREATING TINNED SURFACES
    • 用于处理钢化表面的组合物和工艺
    • WO1997004144A1
    • 1997-02-06
    • PCT/US1996011535
    • 1996-07-19
    • HENKEL CORPORATIONYOSHIDA, Masayuki
    • HENKEL CORPORATION
    • C23C22/23
    • C23C22/23
    • A surface of predominantly tin metal is brought into contact at 35 to 65 DEG C for 5 to 60 seconds with a surface treatment bath with a pH value not less than 6.0 that contains orthophosphate ions, condensed phosphate ions, and a water soluble polymer in the following weight proportions: 0.5 - 30 : 0.1 - 10 : 0.2 - 20. Preferably, contact between the surface treatment bath and the treated metal surface is established by intermittent spraying over a period of 5 to 60 seconds total. This is followed by a water rinse and drying by heating. The water soluble polymer has a chemical structure conforming to formula (I), in which (i) each of X and X represents a hydrogen atom, a C1 to C5 alkyl group, or a C1 to C5 hydroyalkyl group; (ii) each of Y and Y represents a hydrogen atom or a moiety "Z" that conforms to formula (II) or (III), wherein each of R , R , R , R , and R represents a C1 to C10 alkyl group or a C1 to C10 hydroxyalkyl group; (iii) the average value for the number of Z moieties substituted on each aromatic ring in the polymer molecule is from 0.2 to 1.0; and (iv) n is a positive integer, the average value for n being from 2 to 50.
    • 主要是锡金属的表面在35〜65℃下接触5〜60秒,pH值不小于6.0的表面处理液含有正磷酸根离子,缩合磷酸根离子和水溶性聚合物 以下重量比:0.5-30:0.1-10:0.2- 20.优选地,表面处理浴与经处理的金属表面之间的接触通过间歇喷涂总共5至60秒的间隔来建立。 然后通过加热进行水冲洗和干燥。 水溶性聚合物具有符合式(I)的化学结构,其中(i)X 1和X 2各自表示氢原子,C 1至C 5烷基或C 1至C 5烷基烷基 ; (ii)Y 1和Y 2各自表示氢原子或符合式(II)或(III)的部分“Z”,其中R 1,R 2,R 3, R 3,R 4和R 5代表C 1至C 10烷基或C 1至C 10羟基烷基; (iii)在聚合物分子中在每个芳香环上取代的Z部分数目的平均值为0.2-1.0; 和(iv)n是正整数,n的平均值为2至50。
    • 7. 发明申请
    • SURFACE-TREATMENT METHOD FOR TIN-PLATED DRAWN AND IRONED CANS
    • 表面处理和镀锌罐的表面处理方法
    • WO1991010756A1
    • 1991-07-25
    • PCT/US1991000202
    • 1991-01-10
    • HENKEL CORPORATIONTANAKA, ShigeoAOKI, TomoyukiYOSHIDA, Masayuki
    • HENKEL CORPORATION
    • C23C22/08
    • C23C22/08C23C22/23
    • A surface which has excellent adhesivity to paint, good corrosion resistance, and low friction may be obtained on drawn and iron tin plated cans by spraying the can surface for a time between 5 and 60 seconds at a temperature between 40 and 60 DEG C with an aqueous treating liquid having a pH between 4 and 6 and comprising (i) orthophosphoric acid and/or condensed phosphoric acids and (ii) a concentration of at least 0.1 w/o of a water soluble oligomer according to general formula (I) wherein n is a number with a value between 10 and 30 and each of X and Y independently represents hydrogen or a group Z, wherein Z has a chemical composition conforming to general formula (II) wherein each of R1 and R2 is an alkyl or hydroxyalkyl group having from 1 to 5 carbon atoms, except that at least 25 % of the total of all the X and Y groups in the oligomer are Z rather than hydrogen; and drying the surface thus sprayed, optionally after having first rinsed the sprayed surface with water.
    • 通过在40和60℃之间的温度下将罐表面喷涂5至60秒之间,可以在拉伸和镀锡的罐上获得具有优异的涂料粘附性,良好的耐腐蚀性和低摩擦力的表面, 水溶液,其pH在4和6之间,并且包含(i)正磷酸和/或缩合磷酸,和(ii)至少0.1w / o根据通式(I)的水溶性低聚物的浓度,其中n 是数值在10和30之间的数字,X和Y各自独立地表示氢或基团Z,其中Z具有符合通式(II)的化学组成,其中R 1和R 2各自是烷基或羟烷基,其具有 1至5个碳原子,除了低聚物中所有X和Y基团的总和中至少25%是Z而不是氢; 并且任选地在首先用水冲洗喷射表面之后干燥所喷射的表面。
    • 8. 发明申请
    • POLYMER COMPOSITION AND METHOD FOR TREATING METAL SURFACES
    • 聚合物组合物和处理金属表面的方法
    • WO1995028449A1
    • 1995-10-26
    • PCT/US1995004435
    • 1995-04-14
    • HENKEL CORPORATIONYOSHIDA, MasayukiTANAKA, ShigeoMIYAFUJI, Kazutomo
    • HENKEL CORPORATION
    • C09D05/08
    • C23C22/34C09D5/12C23C22/08C23C22/48
    • A highly corrosion-resistant, paint-adherent, and lubricating polymer-containing coating on a metal surface can be formed by contact with an aqueous solution (pH = 2.0 to 6.5) that contains an acidic compound and polymer with formula (I) in which the X bonded to the phenyl ring in formula (I) represents a hydrogen atom, a hydroxyl group, a C1 to C5 alkyl group, a C1 to C5 hydroxyalkyl group, a C6 to C12 aryl group, a benzil group, a benzal group, an unsaturated hydrocarbon moiety condensed to the phenyl ring so as to form a naphthalene ring, or a group corresponding to formula (II) in which R and R in formula (II) each independently represents a hydrogen atom, a hydroxyl group, a C1 to C10 alkyl group, or a C1 to C10 hydroxyalkyl group; the Y and Y bonded to the phenyl ring in formulas (I) and (II) each independently represents a hydrogen atom or a group Z according to one of formulas (III) and (IV) in which each of R , R , R , R , and R in formulas (III) and (IV) independently represents a C1 to C10 alkyl group or a C1 to C10 hydroxyalkyl group; the X's bonded to the phenyl rings in the polymer molecule may all be identical or may differ from one another; each of the Y 's and Y 's bonded to the phenyl rings in the polymer molecule may all be identical or may differ from one another; the average value for the number of Z groups substituted on each phenyl ring in said polymer molecule is 0.2 to 1.0; and n has a value of 2 to 50.
    • 可以通过与含有酸性化合物的水溶液(pH = 2.0至6.5)和式(I)的聚合物接触来形成金属表面上的耐高度耐腐蚀,涂漆粘附和润滑聚合物的涂层,其中 与式(I)中的苯环键合的X表示氢原子,羟基,C1〜C5烷基,C1〜C5羟烷基,C6〜C12芳基,苯偶酰基,亚苄基, 或与式(II)中的R 1和R 2各自独立地表示氢原子的对应于式(II)的基团,其中R 1和R 2各自独立地表示氢原子, 羟基,C1〜C10烷基或C1〜C10羟烷基; 式(I)和(II)中与苯环键合的Y 1和Y 2各自独立地表示根据式(III)和(IV)之一的氢原子或基团Z,其中 式(III)和(IV)中的R 3,R 4,R 5,R 6和R 7独立地表示C 1至C 10烷基或C 1至C 10羟基烷基; 与聚合物分子中的苯环键合的X可以相同或可以彼此不同; 与聚合物分子中的苯环键合的Y 1和Y 2中的每一个可以相同或可以彼此不同; 所述聚合物分子中每个苯环上取代的Z基团的数目的平均值为0.2〜1.0; n的值为2〜50。