    • LONGEVITY AND PERFORMANCE IMPROVEMENTS TO FLARE TIPS
    • 长期和性能改进提示
    • WO2007085793A1
    • 2007-08-02
    • PCT/GB2007/000068
    • 2007-01-12
    • FOSBEL INTELLECTUAL LIMITED
    • ZHU, NaipingKARAMBIS, Louis
    • F23G7/08F23M5/00
    • F23G7/085F23D2900/00018F23M5/00F23M2900/05004
    • Low emissivity (low-E) coatings are applied onto surfaces of flare tips to achieve longer flare tip service life, improved flare tip structural integrity and/or a more stable flame pattern under a wide range of operating conditions. In accordance with some embodiments of the present invention, low-E coatings may be applied to the flare tip burner as well as associated internal and/or external component surfaces to reduce direct flame radiation and also conductive heat transfer. The low-E coating material preferably has an emissivity of less than about 0.80, more preferably between about 0.20 to about 0.78. The coating thickness of the low-E material is preferably between about 1 mil to about 25 mils, and more preferably between about 2 mils to about 8 mils. Coating densities of the low- E material in the coating will preferably be at least about 65%, more preferably between about 80% to about 100%.
    • 将低辐射率(低E)涂层施加到火炬尖端的表面上,以在宽范围的操作条件下实现更长的火炬尖端使用寿命,改善的火炬尖结构完整性和/或更稳定的火焰模式。 根据本发明的一些实施例,低E涂层可以施加到火炬尖端燃烧器以及相关联的内部和/或外部部件表面,以减少直接火焰辐射和导电传热。 低-E涂层材料的发射率优选小于约0.80,更优选在约0.20至约0.78之间。 低E材料的涂层厚度优选在约1密耳至约25密耳之间,更优选在约2密耳至约8密耳之间。 涂层中低E材料的涂层密度优选为至少约65%,更优选约80%至约100%。