会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 2. 发明申请
    • TWO STAGE CURE TWO COMPONENT COATING COMPOSITION CONTAINING HYDROXYL BUTYL ACRYLATE POLYMERS
    • 两阶段固化双组份涂料组合物含羟基丁酸丙烯酸酯聚合物
    • WO2005012440A2
    • 2005-02-10
    • PCT/US2004024644
    • 2004-07-28
    • DU PONTLEWIN LAURA ANNDEVLIN BRIAN PATRICKPAQUET DONALD ALBERT JRADAMS JAMES LAMONTE
    • LEWIN LAURA ANNDEVLIN BRIAN PATRICKPAQUET DONALD ALBERT JRADAMS JAMES LAMONTE
    • C08G18/62C08G18/79C08L61/00C09D20060101C09D133/06C09D175/04C09D
    • C08G18/6229C08G18/792C09D133/066C09D175/04Y10T428/31551Y10T428/31605
    • The invention is directed to a two-stage cure coating composition comprising a two component composition of a binder and a crosslinking component; the binder comprises an acrylic polymer having a weight average molecular weight of 3,000 to 50,000 and hydroxyl moieties in the range of 7.0 to 40.0 weight percent, based on the weight of the acrylic polymer; wherein at least 40.0 weight percent of the hydroxyl moieties are provided by hydroxy butyl acrylate; and the crosslinking component comprises an organic polyisocyanate; and the first stage curing of a finish of the composition on a substrate forms a water spot free finish within 90 minutes of application and the composition has a pot life of less than a 2 second rise in Zahn cup viscosity in 150 minutes; and the invention also is directed to a method of producing a finish on a substrate utilizing the two component coating composition which comprises forming a two stage cure coating composition by mixing together the above described binder component and a cross-linking component; applying a layer of the coating composition over the substrate; first stage curing the layer on the substrate to a water spot free finish; and second stage curing the first stage cured layer on the substrate into a finish having excellent appearance and excellent physical properties.
    • 本发明涉及包含粘合剂和交联组分的双组分组合物的两阶段固化涂料组合物; 粘合剂包含基于丙烯酸类聚合物的重量的重均分子量为3,000至50,000的丙烯酸聚合物和7.0至40.0重量%的羟基部分; 其中至少40.0重量%的羟基部分由丙烯酸羟基丁酯提供; 并且所述交联组分包含有机多异氰酸酯; 并且组合物在基材上的第一阶段固化在施用90分钟内形成无水斑结晶,并且组合物在150分钟内具有小于2秒钟的Zahn杯粘度上升的适用期; 本发明还涉及使用双组分涂料组合物在基材上生产精饰的方法,该组合物包括通过将上述粘合剂组分和交联组分混合在一起来形成两阶段固化涂料组合物; 将一层涂料组合物涂覆在基材上; 第一阶段将基材上的层固化成无水点光洁度; 第二阶段将基材上的第一阶段固化层固化成具有优异外观和优异物理性能的表面。