    • 8. 发明申请
    • MODIFIED POLYETHYLENE RESINS AND METHOD FOR MAKING THE SAME
    • 改性聚乙烯树脂及其制备方法
    • WO2017172273A1
    • 2017-10-05
    • PCT/US2017/020936
    • 2017-03-06
    • DOW GLOBAL TECHNOLOGIES LLC
    • WILLIAMSON, AlexanderBALASUBRAMANIAM, SharavananGOMES, Jorge Caminero
    • C08L23/04
    • A method for increasing the melt strength and/or low shear viscosity of a polyethylene resin, the method comprising: a) providing a first polyethylene resin having a density ranging from 0.900 g/cm 3 to 0.970 g/cm 3 , a melt index ranging from 0.01 g/10 min to 30 g/10 min, and at least 0.20 vinyl groups per 1,000 total carbons; b) providing a masterbatch composition comprising a free radical generator and a second polyethylene resin, wherein the free radical generator has a half-life at 220°C of less than 200 seconds, and a decomposition energy higher than -250 kJ/mol, and wherein the second polyethylene resin has a density ranging from 0.900 g/cm 3 to 0.970 g/cm 3 , melt index ranging from 0.01 g/10 min to 100 g/10 min; and c) reacting the first polyethylene resin with the masterbatch composition to form a modified polyethylene resin.
    • 提高聚乙烯树脂的熔体强度和/或低剪切粘度的方法,所述方法包括:a)提供密度范围为0.900g / cm 3的第一聚乙烯树脂 0.970克/厘米3,熔体指数为0.01克/ 10分钟至30克/ 10分钟,每1000总碳至少0.20个乙烯基; b)提供包含自由基产生剂和第二聚乙烯树脂的母料组合物,其中自由基产生剂在220℃下的半衰期小于200秒,分解能高于-250kJ / mol,以及 其中所述第二聚乙烯树脂的密度范围为0.900g / cm 3至0.970g / cm 3,熔体指数范围为0.01g / 10min至100g / 10 分钟; 和c)使第一聚乙烯树脂与母料组合物反应以形成改性聚乙烯树脂。