    • 4. 发明申请
    • CORDIERITE POROUS CERAMIC HONEYCOMB ARTICLES
    • CORDIERITE POROUS陶瓷蜂窝纸文章
    • WO2011150145A2
    • 2011-12-01
    • PCT/US2011/038030
    • 2011-05-26
    • CORNING INCORPORATEDMIAO, WeiguoWANG, Jianguo
    • MIAO, WeiguoWANG, Jianguo
    • C04B35/195
    • C04B38/0006B01D46/2425B01D46/2444B01D2046/2433B01D2046/2437B01D2046/2496B01J35/04C04B35/195C04B2111/00793C04B2111/0081F01N3/0222F01N2260/10Y10T428/24149C04B38/0074
    • Porous ceramic honeycomb articles for use as particulate filters and processes for making the same are described herein. The porous ceramic honeycomb articles include a fired cordierite body. The fired cordierite body has a microcrack parameter (Nb 3 ) of about 0.05 to about 0.25 prior to exposure to a microcracking condition. After exposure to the microcracking condition, the fired cordierite body has a microcrack parameter (Nb 3 ) at least 20% greater than the microcrack parameter prior to exposure to the microcracking condition. The fired cordierite body has a coefficient of thermal expansion (CTE) of about 7.0x10 -7 /°C to about 15.0x10 -7 /°C over from about 25°C to about 800°C prior to exposure to the microcracking condition and a coefficient of thermal expansion of about 1.0x10-7/°C to about 10.0x10 -7 /°C over from about 25°C to about 800°C after exposure to the microcracking condition. The microcrack parameter may include a thermal cycle or a chemical treatment.
    • 用作微粒过滤器的多孔陶瓷蜂窝体制品及其制造方法在此描述。 多孔陶瓷蜂窝体制品包括烧制的堇青石体。 烧制的堇青石体在暴露于微裂纹状态之前具有约0.05至约0.25的微裂纹参数(Nb 3)。 在暴露于微裂纹状态之后,烧结的堇青石体在暴露于微裂纹状态之前具有比微裂纹参数大至少20%的微裂纹参数(Nb 3)。 煅烧的堇青石体在暴露于微裂纹状态之前具有约7.0×10 -7 /℃至约15.0×10 -7 /℃的约25℃至约800℃的热膨胀系数(CTE),以及 暴露于微裂纹状态后约25℃至约800℃的热膨胀系数为约1.0×10 -7 /℃至约10.0×10 -7 /℃。 微裂纹参数可以包括热循环或化学处理。