    • METHOD OF PROVIDING CURED COATING FILMS FREE OF POPPING DEFECTS
    • 提供固化涂层膜的方法,不含POPPING缺陷
    • WO2004031309A1
    • 2004-04-15
    • PCT/US2003/020852
    • 2003-07-01
    • BASF CORPORATIONOHRBOM, WalterBALATAN, SergioWEISE, RobertLAW, David
    • OHRBOM, WalterBALATAN, SergioWEISE, RobertLAW, David
    • C09D201/02
    • C09D201/00C08F212/14C08K5/205C09D5/002C09D5/033C09D7/63C09D133/08C09D201/02C08L2666/28C08L2666/36
    • Method for providing cured coating films free of popping defects. Method requires the application to a substrate of at least 2.0 mils/50.8µm of a uncured curable coating composition comprising an anti-popping component (a), a film-forming component (b), and a crosslinking component (c), wherein anti-popping component (a) has from 12 to 72 carbon atoms, is substantially free of any heteroatoms, is not a crystalline solid at room temperature and comprises a mixture of two or more structures selected from the group consisting of aliphatic structures for anti-popping component (a), aromatic-containing structures for anti-popping component (a), cycloaliphatic-containing structures for anti-popping component (a), and mixtures thereof, at least one of the two or more structures being a cycloaliphatic-containing structure or an aromatic-containing structure. Coated uncured substrate is cured to provide a cured film free of popping defects with an average film build of at least 2.0 mils/50.8µm.
    • 提供没有突出缺陷的固化涂膜的方法。 方法要求将至少2.0密耳/50.8μm的包含抗爆组分(a),成膜组分(b)和交联组分(c)的未固化的可固化涂料组合物的基材施用于其中, 具有12至72个碳原子的杂原子组分(a)基本上不含任何杂原子,在室温下不是结晶固体,并且包含两种或更多种结构的混合物,所述结构选自由抗突变的脂肪族结构组成的组 组分(a),抗起泡组分(a)的含芳族化合物结构,抗起泡组分(a)的含脂环族的结构及其混合物,两种或更多种结构中的至少一种是含脂环族结构 或含芳香族结构。 固化未固化的基材以提供没有突出缺陷的固化膜,其平均膜构成为至少2.0密耳/50.8μm。
    • 4. 发明申请
    • POWDER COATING COMPOSITIONS AND POWDER SLURRY COATING COMPOSITIONS CONTAINING MONOMERIC DIFUNCTIONAL COMPOUNDS
    • 粉末涂料组合物和含有单体二官能化合物的粉末涂料组合物
    • WO2004031307A2
    • 2004-04-15
    • PCT/US2003/020853
    • 2003-07-01
    • BASF CORPORATIONOHRBOM, WalterWEISE, RobertLAW, David
    • OHRBOM, WalterWEISE, RobertLAW, David
    • C09D7/00
    • C09D133/14C09D5/02C09D5/033C09D201/00C09D201/02C09D201/025Y10S525/934
    • The curable coating compositions of the invention comprise a particulate component having at least one binder component (a) which is a solid at 75°F/24°C, and an additive component (b). The curable coating compositions further comprise a crosslinking component (c) reactive with the at least one binder component (a). Additive component (b) has from 12 to 72 carbon atoms, is substantially free of any heteroatoms, is not a crystalline solid at 75°F/24°C and comprises a mixture of two or more structures selected from the group consisting of aliphatic structures for additive component (b), aromatic-containing structures for additive component (b), cycloaliphatic-containing structures for additive component (b), and mixtures thereof, wherein at least one of the two or more structures is either a cycloaliphatic-containing structure or an aromatic-containing structure. The curable coating compositions are useful as powder coating compositions and powder slurry coating compositions having improved application performance properties.
    • 本发明的可固化涂料组合物包含具有至少一种在75°F / 24℃下为固体的粘合剂组分(a)和添加剂组分(b)的颗粒组分。 可固化涂料组合物还包含与至少一种粘合剂组分(a)反应的交联组分(c)。 添加剂组分(b)具有12至72个碳原子,基本上不含任何杂原子,在75°F / 24℃下不是结晶固体,并且包含两种或多种选自脂肪族结构 用于添加剂组分(b),用于添加剂组分(b)的含芳族化合物结构,用于添加剂组分(b)的含脂环族基团的结构物及其混合物),其中两种或多种结构中的至少一种是含脂环族的结构 或含芳香族结构。 可固化涂料组合物可用作具有改进的应用性能性质的粉末涂料组合物和粉末淤浆涂料组合物。
    • 8. 发明申请
    • METHOD FOR OBTAINING COATING COMPOSITIONS HAVING REDUCED VOC
    • 用于获得具有降低VOC的涂料组合物的方法
    • WO2003050146A1
    • 2003-06-19
    • PCT/US2002/027788
    • 2002-09-03
    • BASF CORPORATIONOHRBOM, WalterLAUGAL, JamesWEISE, Robert
    • OHRBOM, WalterLAUGAL, JamesWEISE, Robert
    • C08F2/06
    • C08F2/44C08F2/06
    • The invention relates to an economical method of making a polymer having reduced VOCs and coating compositions containing such polymers. In one embodiment, the method of invention requires providing a reactant mixture (a), providing a solvent mixture (b) comprising a reactive component (c) which is substantially free of any heteroatoms and is not a crystalline solid at room temperature and comprises (i) from 12 to 72 carbon atoms, and (ii) at least two functional groups, and subjecting the reactant mixture (a) in the solvent mixture (b) to polymerization conditions sufficient to polymerize reactant mixture (a) to provide a mixture (d) of a polymer (a') in solvent mixture (b), wherein reactive component (c) under the polymerization conditions is substantially nonreactive: (1) with the components of reactive mixture (a), (2) in the polymerization of reactant mixture (a) and (3) with the polymer (a'). Coating compositions of the invention comprising polymers made by the disclosed method provide low VOCs without any reduction in application or performance properties.
    • 本发明涉及制备具有降低的VOC的聚合物和含有这种聚合物的涂料组合物的经济方法。 在一个实施方案中,本发明的方法需要提供反应物混合物(a),提供包含基本上不含任何杂原子并且在室温下不是结晶固体的反应性组分(c)的溶剂混合物(b),并且包含 i)12至72个碳原子,和(ii)至少两个官能团,并使溶剂混合物(b)中的反应物混合物(a)经受足以聚合反应混合物(a)的聚合条件以提供混合物 d)在溶剂混合物(b)中的聚合物(a'),其中在聚合条件下的反应性组分(c)基本上是非反应性的:(1)在反应混合物(a),(2) 反应物混合物(a)和(3)与聚合物(a')。 包含通过所公开的方法制备的聚合物的本发明的涂料组合物提供低VOC,而不会降低应用或性能。