    • 1. 发明申请
    • IMPROVING THE BENDING BEHAVIOUR OF MECHANICALLY-LINED RIGID PIPE
    • 改进机械式刚性管的弯曲性能
    • WO2016103038A1
    • 2016-06-30
    • PCT/IB2015/002551
    • 2015-12-18
    • ACERGY FRANCE SAS
    • TOGUYENI, Grégory Alexandre
    • F16L58/10B21C37/15B21D39/04B21D39/20F16L1/20F16L9/02
    • B21C37/154B21D39/04F16L1/203F16L9/02F16L58/08F16L58/1081
    • A method of making mechanically-lined pipe comprises primary expansion by plastically expanding a liner sleeve within an outer pipe, under lining pressure applied internally to the liner sleeve. On relieving the lining pressure, elastic radial contraction of the outer pipe makes a mechanical bond between the outer pipe and the liner sleeve. Then, secondary expansion of the outer pipe (12) is performed under fixing pressure, which may be greater than the lining pressure, applied internally to the liner sleeve (14) at an end portion of the pipe (10). This makes or strengthens a mechanical bond (26) at the end portion. The resulting pipe joint comprises an end portion and a body portion inboard of the end portion. The body portion has a first, lesser bonding pressure between the outer pipe and the liner sleeve. The end portion has a second, greater bonding pressure between the outer pipe and the liner sleeve.
    • 制造机械衬里管的方法包括通过在衬套内部施加的内衬压力下将衬套膨胀在外管内的初级膨胀。 在减轻内衬压力时,外管的弹性径向收缩在外管和衬套之间形成机械结合。 然后,外管12的二次膨胀是在固定压力下进行的,所述固定压力可大于在管道(10)的端部处向衬套(14)内部施加的内衬压力。 这在端部处产生或加强了机械结合(26)。 所得到的管接头包括端部和端部内侧的主体部分。 主体部分在外管和衬套之间具有第一较小的结合压力。 端部在外管和衬套之间具有第二较大的结合压力。
    • 2. 发明申请
    • REPAIR OF PIPELINE WELDS USING FRICTION STIR PROCESSING
    • 使用摩擦加工处理管道维修
    • WO2017017532A1
    • 2017-02-02
    • PCT/IB2016/001311
    • 2016-07-28
    • ACERGY FRANCE SAS
    • TOGUYENI, Grégory Alexandre
    • B23K20/12B23P6/00B23K101/10
    • B23K20/122B23K20/124B23K2201/10B23P6/00
    • A method of using friction stir processing to repair a defect in a pre-existing weld of a pipeline of steel or other ferrous alloy. The method comprises attaching run-on and run-off tabs to the pipeline on respective sides of the defect and then advancing a friction stir processing tool into the run-on tab. The tool is moved from the run-on tab to the run-off tab along a weld-processing path that incorporates the defect. Once the defect is repaired, the tool is removed from the run-off tab. The run-on and run-off tabs may then be removed from the pipeline. The run-on and run-off tabs are generally wedge-shaped, each comprising an inner seating face and an outer running face that converges with the inner seating face. When attached to the pipeline, the tabs toward each other about the circumference of the pipeline.
    • 一种使用摩擦搅拌处理来修复钢或其他铁合金管道的预先存在的焊缝中的缺陷的方法。 该方法包括将穿通和脱落突出部附接到缺陷的相应侧上的管道,然后将摩擦搅拌处理工具推进到连续突出部。 该工具沿着包含缺陷的焊接处理路径从运行选项卡移动到径向选项卡。 修复缺陷后,该工具将从流出选项卡中移除。 然后可以从流水线中删除运行和运行选项卡。 跑步和径流片通常是楔形的,每个包括内座面和与内座面会聚的外运行面。 当连接到管道时,突片相对于管道的圆周彼此相向。