    • ポリパラキシリレンおよびその誘導体膜の熱安定性向上方法ならびにポリパラキシリレン誘導体
    • 用于改善聚对苯二甲酸或其衍生物的薄膜的热稳定性的方法,以及聚对苯二甲酸衍生物
    • WO2005061576A1
    • 2005-07-07
    • PCT/JP2003/016371
    • 2003-12-19
    • 第三化成株式会社丸山 宏望月 励井上 崇
    • 丸山 宏望月 励井上 崇
    • C08G61/02
    • C08G61/025C08G61/02C08G2261/3424C08L65/04
    • A method for improving the heat stability of a film of poly-p-xylylene or a derivative thereof as represented by the general formula (1), which comprises forming a film through chemical deposition from a raw material prepared by mixing a (2.2)-paracyclophane represented by the general formula (2) with an amino-(2.2)-paracyclophane represented by the general formula (3) and by which the heat resistance of the film can be improved without impairing the deposition properties or the economic efficiency; and poly-p-xylylene derivatives improved in heat resistance: (1) [wherein X1 and X2 are each hydrogen, lower alkyl, or halogeno, and they may be the same or different from each other; and n is a degree of polymerization], (2) [wherein X1 and X2 are each the same as defined for the general formula (1)], and (3) [wherein X3 is hydrogen or lower alkyl; and Y1 and Y2 are each hydrogen or amino, with the proviso that both of Y1 and Y2 must be not hydrogen].
    • 一种用于提高由通式(1)表示的聚对二甲苯或其衍生物的膜的热稳定性的方法,其包括通过化学沉积从通过混合(2.2) - 由通式(2)表示的对环芳烷与由通式(3)表示的氨基 - (2.2) - 对环烷基,并且可以改善膜的耐热性,而不损害沉积性质或经济效率; 和聚对二甲苯衍生物耐热性提高:(1)[其中X1和X2各自为氢,低级烷基或卤代,并且它们可以相同或不同; n是聚合度],(2)[其中X1和X2各自与通式(1)所定义相同],和(3)[其中X3是氢或低级烷基; 并且Y 1和Y 2各自为氢或氨基,条件是Y 1和Y 2都不能为氢]。