热词
    • 2. 发明申请
    • METHOD OF TREATING LITHIUM MANGANESE OXIDE SPINEL
    • 处理锂锰氧化物磁珠的方法
    • WO1998002930A1
    • 1998-01-22
    • PCT/US1997011816
    • 1997-07-08
    • DURACELL, INC.WANG, Enoch, I.
    • DURACELL, INC.
    • H01M04/50
    • H01M4/505C01G45/1242C01P2002/32C01P2002/52C01P2002/54C01P2004/61C01P2004/80C01P2006/40H01M4/131H01M10/0525
    • A method of treating lithium manganese oxide of spinel structure is disclosed. The method involves heating the lithium manganese oxide spinel in an atmosphere of an inert gas, e.g. argon, helium, nitrogen or carbon dioxide, which does not react with the spinel. Alternatively, the spinel may be first coated with an alkali metal hydroxide, preferably lithium, sodium or potassium hydroxide and then heated in an atmosphere preferably containing carbon dioxide. Such treatment of lithium manganese oxide spinel improves the performance of the spinel when employed as an electrode in rechargeable cells such as lithium-ion cells. Alternatively, the spinel may be first treated in an aqueous solution of a soluble metal salt of a carboxylic acid prior to treatment with heated carbon dioxide or inert gas. In such latter case the spinel may optionally also be treated with an alkali metal hydroxide prior to treatment with carbon dioxide or inert gas.
    • 公开了一种处理尖晶石结构的锰酸锂的方法。 该方法包括在惰性气体气氛中加热锂锰氧化物尖晶石。 氩,氦,氮或二氧化碳,其不与尖晶石反应。 或者,尖晶石可以首先用碱金属氢氧化物,优选氢氧化锂,氢氧化钠或氢氧化钾涂覆,然后在优选含有二氧化碳的气氛中加热。 这种锂锰氧化物尖晶石的处理改善了尖晶石在用作可再充电电池如锂离子电池中的电极时的性能。 或者,尖晶石可以在用加热的二氧化碳或惰性气体处理之前首先在可溶性羧酸金属盐的水溶液中处理。 在这种后一种情况下,在用二氧化碳或惰性气体处理之前,尖晶石也可以任选地用碱金属氢氧化物处理。