    • A corrugated board comprising a polyolefin composition comprising (per cent by weight): a) from 50% to 85 of a propylene polymer having a fraction of xylene solubles measured at 25°C lower than 3%; b) from 5% to 20%, of a copolymer of ethylene and propylene, the copolymer having an amount of recurring units deriving from ethylene ranging from 30 to 60%, and being partially soluble in xylene at soluble in xylene at 25°C; the polymer fraction soluble in xylene at soluble in xylene at 25°C having an intrinsic viscosity value ranging from 2.0 to 4.0 dl/g; and c) 5% to 30%), of ethylene homopolymer having having a xylene soluble fraction at 25°C ranging from 5% to 30%; the sum of a)+b) +c) being 100; said composition having a value of melt flow rate ranging from 0.5 to 30.0 g/10 min.
    • 一种包含聚烯烃组合物的瓦楞纸板,其包含(重量百分比):a)50%至85%的在25℃下测得的二甲苯可溶物的分数低于3%的丙烯聚合物; b)5%至20%的乙烯和丙烯的共聚物,所述共聚物具有衍生自乙烯的重复单元的量为30至60%,并且在25℃下可溶于二甲苯中部分溶于二甲苯; 在25℃下可溶于二甲苯的二甲苯中的聚合物部分的特性粘度值为2.0-4.0dl / g; 和c)5%至30%)的在25℃下具有5%至30%的二甲苯可溶组分的乙烯均聚物; a)+ b)+ c)的和为100; 所述组合物的熔体流动速率范围为0.5至30.0g / 10min。