    • METHOD OF MANUFACTURE OF PRODUCTS FROM GEOPOLYMER COMPOSITE
    • 从地质复合材料制造产品的方法
    • WO2013071899A3
    • 2013-08-08
    • PCT/CZ2012000087
    • 2012-08-29
    • IQ STRUCTURES S R OTETHAL TOMASSTEINEROVA MICHAELAHOUFEK JIRI
    • TETHAL TOMASSTEINEROVA MICHAELAHOUFEK JIRI
    • C04B41/88
    • B29C39/003B29C33/58C04B41/009C04B41/51C04B41/88Y02P40/165C04B28/006
    • A method of manufacture of products from geopolymer composite shaped in a mold which is filled by casting of geopolymer composite in form of a precursor and after its hardening the casting is taken out from the mold and the casting surface is provided with a metallic layer. Before metal-plating casting surface with absorption capacity greater than 5 % is treated to make it chemically stable so that pH of a leachate from 100 g of the bulk product in 1000 g distilled water after 24 hours does not exceed 9. In order to reduce the absorption capacity of the casting surface it is penetrated with polymer substances or particles of a non-porous filler are added into the geopolymer composite in the precursor state. The metallic layer on the casting surface is made by a method from the group of methods that include vacuum deposition, vacuum sputtering, galvanization, cold metal spraying, dip coating in melted metal, plasma spraying of melted metal, deposition of metal from metal salt solution or colloid solution or sintering of powder metal.
    • 由模具中形成的地质聚合物复合材料制成的产品的方法是从模具中取出,并且铸造表面设置有金属层。 在金属镀覆前,吸附能力大于5%的铸造表面进行处理,使其化学稳定,24小时后,1000克蒸馏水中的100g产品的渗滤液pH值不超过9.为了减少 将其用聚合物物质或无孔填料颗粒渗透的铸造表面的吸收能力以前体状态加入到地质聚合物复合材料中。 铸造表面上的金属层由包括真空沉积,真空溅镀,镀锌,冷金属喷涂,熔融金属浸涂,熔融金属等离子喷涂,金属盐溶液沉积的方法组成的方法制成 或胶体溶液或粉末金属的烧结。