    • 1. 发明申请
    • THERMOPLASTIC POLYESTER ELASTOMER COMPOSITION INCLUDING IONOMER
    • 热塑性聚酯弹性体组合物,包括离子
    • WO2011150304A3
    • 2012-03-29
    • PCT/US2011038286
    • 2011-05-27
    • DU PONTAKIBA KAZUKI
    • AKIBA KAZUKI
    • C08L67/00C08J5/00C08K3/10C08L23/08C08L71/12
    • C08L67/025C08L23/0876C08L23/0884C08L71/12C08L2666/02C08L67/00
    • Disclosed is a composition including a melt mixed blend including (a) 58 to 96,8 weight percent one or more copolyester thermoplastic elastomers; (b) 3 to 40 weight percent polyphenylene ether; (c) 0.1 to 8 weight % ionomer and (d) 0.1 to 8 weight percent of polymeric toughener selected from the group consisting ethylene copolymers of the formula E/X/Y wherein: E is the radical formed from ethylene; X is selected from the group consisting of radicals formed from CH2=CH(R1)-C(0)-OR2 wherein R1 is H, CH3 or C2H5, and R2 is an alkyl group having 1-8 carbon atoms; vinyl acetate; and mixtures thereof; wherein X comprises 0 to 50 weight % of E/X/Y copolymer; and Y is a radical formed from giycidyl (meth)acrylate; and wherein the composition has one or more low temperature glass transition(s) between minus 100 and plus 150 °C. Also disclosed are molded articles including the compositions, including CVJ boots and air ducts for automotive applications.
    • 公开了包含熔融混合共混物的组合物,其包含(a)58至96.8重量%的一种或多种共聚酯热塑性弹性体; (b)3〜40重量%的聚苯醚; (c)0.1至8重量%的离聚物和(d)0.1至8重量%的选自式E / X / Y的乙烯共聚物的聚合物增韧剂,其中:E是由乙烯形成的自由基; X选自由CH 2 = CH(R 1)-C(O)-OR 2形成的基团,其中R 1是H,CH 3或C 2 H 5,R 2是具有1-8个碳原子的烷基; 乙酸乙烯酯; 及其混合物; 其中X包含0〜50重量%的E / X / Y共聚物; 并且Y是由(甲基)丙烯酸环己基酯形成的基团; 并且其中所述组合物在-100至+ 150℃之间具有一个或多个低温玻璃化转变。 还公开了包括组合物的模制品,包括用于汽车应用的CVJ靴和空气管。
    • 2. 发明申请
    • THERMOPLASTIC POLYESTER ELASTOMER COMPOSITIONS
    • 热塑性聚酯弹性体组合物
    • WO2011150303A2
    • 2011-12-01
    • PCT/US2011/038284
    • 2011-05-27
    • E. I. DU PONT DE NEMOURS AND COMPANYAKIBA, Kazuki
    • AKIBA, Kazuki
    • C08L67/00C08L71/12C08L23/08C08J5/00
    • C08L67/025C08L23/0884C08L71/12C08L2666/02C08L67/00
    • Disclosed is a composition including a melt mixed blend including (a) 52 to 96.9 weight percent one or more copolyester thermoplastic elastomers; (b) 3 to 40 weight percent polyphenylene ether; and (c) 0.1 to 8 weight percent of polymeric toughener selected from the group consisting ethylene copolymers of the formula E/X/Y wherein: E is the radical formed from ethylene; X is selected from the group consisting of radicals formed from CH 2 =CH(R 1 )-C(O)-OR 2 wherein R 1 is H, CH 3 or C 2 H 5 , and R 2 is an alkyl group having 1-8 carbon atoms; vinyl acetate; and mixtures thereof; wherein X comprises 0 to 50 weight % of E/X/Y copolymer; and Y is a radical formed from glycidyl (meth)acrylate; and wherein the composition has one or more low temperature glass transition(s) between between minus 100 and plus 150 °C. Also disclosed are molded articles including the compositions, including CVJ boots and air ducts for automotive applications.
    • 公开了包含熔融混合共混物的组合物,其包含(a)52至96.9重量%的一种或多种共聚酯热塑性弹性体; (b)3〜40重量%的聚苯醚; 和(c)0.1至8重量%的选自式E / X / Y的乙烯共聚物的聚合物增韧剂,其中:E是由乙烯形成的自由基; X选自由CH 2 = CH(R 1)-C(O)-OR 2形成的基团,其中R 1是H,CH 3或C 2 H 5,R 2是具有1-8个碳原子的烷基; 乙酸乙烯酯; 及其混合物; 其中X包含0至50重量%的E / X / Y共聚物; Y是由(甲基)丙烯酸缩水甘油酯形成的自由基; 并且其中所述组合物在-100至+ 150℃之间具有一个或多个低温玻璃化转变。 还公开了包括组合物的模制品,包括用于汽车应用的CVJ靴和空气管。
    • 3. 发明申请
    • THERMOPLASTIC POLYESTER ELASTOMER COMPOSITIONS
    • 热塑性弹性体弹性体组合物
    • WO2011150303A3
    • 2012-03-29
    • PCT/US2011038284
    • 2011-05-27
    • DU PONTAKIBA KAZUKI
    • AKIBA KAZUKI
    • C08L67/00C08J5/00C08L23/08C08L71/12
    • C08L67/025C08L23/0884C08L71/12C08L2666/02C08L67/00
    • Disclosed is a composition including a melt mixed blend including (a) 52 to 96.9 weight percent one or more copolyester thermoplastic elastomers; (b) 3 to 40 weight percent polyphenylene ether; and (c) 0.1 to 8 weight percent of polymeric toughener selected from the group consisting ethylene copolymers of the formula E/X/Y wherein: E is the radical formed from ethylene; X is selected from the group consisting of radicals formed from CH2=CH(R1)-C(O)-OR2 wherein R1 is H, CH3 or C2H5 , and R2 is an alkyl group having 1-8 carbon atoms; vinyl acetate; and mixtures thereof; wherein X comprises 0 to 50 weight % of E/X/Y copolymer; and Y is a radical formed from glycidyl (meth)acrylate; and wherein the composition has one or more low temperature glass transition(s) between between minus 100 and plus 150 °C. Also disclosed are molded articles including the compositions, including CVJ boots and air ducts for automotive applications.
    • 公开了包含熔融混合共混物的组合物,其包含(a)52至96.9重量%的一种或多种共聚酯热塑性弹性体; (b)3〜40重量%的聚苯醚; 和(c)0.1至8重量%的选自式E / X / Y的乙烯共聚物的聚合物增韧剂,其中:E是由乙烯形成的自由基; X选自由CH 2 = CH(R 1)-C(O)-OR 2形成的基团,其中R 1是H,CH 3或C 2 H 5,R 2是具有1-8个碳原子的烷基; 乙酸乙烯酯; 及其混合物; 其中X包含0〜50重量%的E / X / Y共聚物; Y为由(甲基)丙烯酸缩水甘油酯形成的基团; 并且其中所述组合物在-100至+ 150℃之间具有一个或多个低温玻璃化转变。 还公开了包括组合物的模制品,包括用于汽车应用的CVJ靴和空气管。
    • 4. 发明申请
    • IMPROVED SOLID STATE POLYMERIZATIONS OF POLYESTER ELASTOMERS
    • 改进聚酯弹性体的固态聚合
    • WO2012071187A1
    • 2012-05-31
    • PCT/US2011/060218
    • 2011-11-10
    • E. I. DU PONT DE NEMOURS AND COMPANYAKIBA, Kazuki
    • AKIBA, Kazuki
    • C08G63/66C08G63/80C08G63/91
    • C08G63/80C08L67/025Y10T428/139
    • Disclosed is an improved process for solid state polymerization of copolyester thermoplastic elastomers that results in a reduction of solid state polymerization reaction time while producing a high molecular weight product. The addition of 10 wt% or less of polar polymers i) having melting points at least 40 °C below the melting temperature or melting point of a copolyester thermoplastic elastomer and ii) having a solubility parameter greater than 18.4 (J/cm 3 ) 1/2 results in a copolyester thermoplastic elastomer composition which, after solid state polymerization, has either a melt flow rate which is less than or equal to 1/100 the melt flow rate of the copolyester thermoplastic elastomer/polar polymer blend and/or which exhibits a polymerization rate value of greater than or equal to 0.2 [ln(g/10min.)] / hour.
    • 公开了一种改进的共聚酯热塑性弹性体的固态聚合方法,其导致固态聚合反应时间的降低,同时产生高分子量产物。 添加10wt%或更少的极性聚合物i)具有低于共聚酯热塑性弹性体的熔融温度或熔点至少40℃的熔点,和ii)溶解度参数大于18.4(J / cm 3)1 / 2产生共聚酯热塑性弹性体组合物,其在固态聚合之后具有小于或等于共聚酯热塑性弹性体/极性聚合物共混物的熔体流动速率的1/100的熔体流动速率和/或显示出 聚合速率值大于或等于0.2 [ln(g / 10min。)] /小时。
    • 6. 发明申请
    • THERMOPLASTIC POLYESTER ELASTOMER COMPOSITION INCLUDING IONOMER
    • 热塑性聚酯弹性体组合物,包括离子
    • WO2011150304A2
    • 2011-12-01
    • PCT/US2011/038286
    • 2011-05-27
    • E. I. DU PONT DE NEMOURS AND COMPANYAKIBA, Kazuki
    • AKIBA, Kazuki
    • C08L67/00C08L71/12C08L23/08C08K3/10C08J5/00
    • C08L67/025C08L23/0876C08L23/0884C08L71/12C08L2666/02C08L67/00
    • Disclosed is a composition including a melt mixed blend including (a) 58 to 96,8 weight percent one or more copolyester thermoplastic elastomers; (b) 3 to 40 weight percent polyphenylene ether; (c) 0.1 to 8 weight % ionomer and (d) 0.1 to 8 weight percent of polymeric toughener selected from the group consisting ethylene copolymers of the formula E/X/Y wherein: E is the radical formed from ethylene; X is selected from the group consisting of radicals formed from CH 2 =CH(R 1 )-C(0)-OR 2 wherein R 1 is H, CH 3 or C 2 H 5 , and R 2 is an alkyl group having 1-8 carbon atoms; vinyl acetate; and mixtures thereof; wherein X comprises 0 to 50 weight % of E/X/Y copolymer; and Y is a radical formed from giycidyl (meth)acrylate; and wherein the composition has one or more low temperature glass transition(s) between minus 100 and plus 150 °C. Also disclosed are molded articles including the compositions, including CVJ boots and air ducts for automotive applications.
    • 公开了包含熔融混合共混物的组合物,其包含(a)58至96.8重量%的一种或多种共聚酯热塑性弹性体; (b)3〜40重量%的聚苯醚; (c)0.1至8重量%的离聚物和(d)0.1至8重量%的选自式E / X / Y的乙烯共聚物的聚合物增韧剂,其中:E是由乙烯形成的自由基; X选自由CH 2 = CH(R 1)-C(O)-OR 2形成的基团,其中R 1是H,CH 3或C 2 H 5,R 2是具有1-8个碳原子的烷基; 乙酸乙烯酯; 及其混合物; 其中X包含0〜50重量%的E / X / Y共聚物; 并且Y是由(甲基)丙烯酸环己基酯形成的基团; 并且其中所述组合物在-100至+ 150℃之间具有一个或多个低温玻璃化转变。 还公开了包括组合物的模制品,包括用于汽车应用的CVJ靴和空气管。