    • ADDITIVES FOR GALVANIC CELLS
    • 加尔万尼细胞的添加剂
    • WO2014060077A3
    • 2014-09-04
    • PCT/EP2013003026
    • 2013-10-09
    • ROCKWOOD LITHIUM GMBH
    • WIETELMANN ULRICHHARTNIG CHRISTOPHEMMEL UTE
    • H01M10/0567H01M4/38H01M10/052
    • H01M10/0567H01M10/052H01M10/0568H01M2300/0022
    • The invention relates to additives for galvanic cells. Fluorine-free sodium, potassium, cesium, and/or rubidium salts that are soluble in polar organic solvents are used as electrolyte components (additives). In particular, such additives are Na-, K-, Cs-, and Rb salts having organoborate anions of the general structure 1 , having organophosphate anions of the general structure 2 , and/or having perchlorate anion (CIO4) 3 (M = Na, K, Rb, Cs), formulas 1 , 2 , 3 , X, Y and Z in formulas 1, 2 denote a bridge connection of two oxygen atoms to the boron or phosphorus atom, which is selected from formula (A) or formula (B) n = 0.1, or formula (C), formula (D) whereas Z = N, N=C; S, S=C; O, O=C; C=C Y1 and Y2 together = O, m = 1, n = 0 and Y3 and Y4 independently from one another are H or an alkyl radical with 1 to 5 C-atoms, or Y1, Y2, Y3, Y4 each independently from one another, are OR (whereas R = alkyl radical having 1 to 5 C-atoms), H or an alkyl radical are R1, R2 having 1 to 5 C-atoms, and wherein m, n = 0 or 1.
    • 本发明涉及用于原电池的添加剂。 无氟,在极性有机溶剂中使用可溶性钠,钾,铯和/或铷盐作为电解质成分(添加剂)。 特别是,那些添加剂的Na,K,Cs和Rb Organoboratanionen具有通式结构 1 与Organophosphatanionen通式结构 2 和/或高氯酸盐[ClO 4 ] 3 (M =钠,钾,铷,铯),公式 1 2 3 ,X ,Y和在式Z 1,2被连接到两个氧原子与硼或选自式磷原子的桥(a)或式(B)N = 0,1或式(C),式(d )其中Z = N,N = C; S,S = C; O,O = C; C = C Y1和Y2一起是= O平均值m = 1,n = 0且Y3和Y4独立地是H或具有1到5个C原子的烷基,或Y1,Y2,Y3,Y4各自独立地是OR( 其中R =烷基基团具有1至5个碳原子),H或具有1至5个碳原子的烷基R 1,R 2,和其中m,n是0或第一
    • 6. 发明申请
    • VERFAHREN ZUR HYDROMETALLURGISCHEN RÜCKGEWINNUNG VON LITHIUM, NICKEL, KOBALT AUS DER LITHIUM-ÜBERGANGSMETALLOXID HALTIGEN FRAKTION GEBRAUCHTER GALVANISCHER ZELLEN
    • 用于水力冶金回收锂,镍方法,钴FROM锂含过渡FRACTION USED原电池
    • WO2014056609A1
    • 2014-04-17
    • PCT/EP2013/003028
    • 2013-10-09
    • ROCKWOOD LITHIUM GMBH
    • WOHLGEMUTH, DavidSCHNEIDER, Mark, AndreSPEILAU, RebeccaWILLEMS, JohannesSTEINBILD, Martin
    • C22B7/00C22B26/12
    • C22B26/12C01B25/45C01G51/42C01G53/42C01P2006/40C22B7/007C22B23/043C22B23/0461H01M10/54Y02P10/234Y02W30/84
    • Die Erfindung betrifft ein Verfahren zur hydrometallurgischen Rückgewinnung von Lithium aus der Lithium-Übergangsmetalloxid haltigen Fraktion gebrauchter galvanischer Zellen, bei dem eine Lithium-Übergangsmetalloxid haltige Fraktion, wobei es sich bei den Übergangsmetallen um Nickel, Kobalt und/oder Mangan handelt, mit einem Aluminiumgehalt bis 5 Gew.-% oder um solche der Metalle Nickel, Kobalt und/oder Aluminium und einer Partikelgröße bis 500 μηι in die bezogen auf den Oxidgehalt der Lithium-Übergangsmetalloxid haltigen Fraktion mindestens stöchiometrischen Menge Schwefelsäure oder Salzsäure mit einer Konzentration von 0,5 bis 4 mol/l und einem Feststoff zu Flüssigkeits-Verhältnis im Bereich von 10 bis 300 g/l eingebracht und unter Zusatz der gleichfalls bezogen auf den zu reduzierenden Übergangsmetallgehalt der Lithium-Übergangsmetalloxid haltigen Fraktion mindestens stöchiometrischen Menge Wasserstoffperoxid bei Temperaturen von 35 bis 70°C aufgeschlossen, die gebildete Lithiumsalze und die Salze der genannten Übergangsmetalle haltige Lösung abgetrennt und der verbleibende Rückstand mindestens zweimal gewaschen, die abgetrennte Salze und die Salz haltigen Wasch-Lösungen vereinigt, die Übergangsmetalle im pH-Wert-Bereich von 9 bis 1 1 als Hydroxide ausgefällt, abgetrennt und gewaschen werden und die verbleibenden Lithiumsulfat haltigen Lösungen vereinigt sowie mittels Elektrodialyse mit bipolaren Membranen in Lithiumhydroxid umgewandelt wird.
    • 本发明涉及一种用于锂从使用原电池的锂含过渡金属的分数,湿法冶金回收其中的锂含过渡金属的分数,其中,它是在过渡金属是镍,钴和/或锰,可高达铝含量 5重量%,或由这些金属镍,钴和/或铝,和多达500个μ.eta的粒径;ι中的相对含锂的过渡金属组分的氧化物含量为以0.5:1的浓度的硫酸或盐酸的至少化学计量量的 〜4摩尔/升,并引入了固体在10至300克/升,并与另外的也基于材料的范围内的液体比例来减少锂含过渡金属的级分包含在35的温度下过氧化氢的至少化学计量量至70°的过渡金属含量 头脑C,双 È锂形成的盐,所述的过渡金属的盐分离出的含水溶液和剩余的残余物进行洗涤至少两次,所分离的盐和联合含有洗涤溶液的盐,沉淀的pH范围内的过渡金属从一月9日至1日氢氧化物,分离 和洗涤,并含有剩余硫酸锂溶液合并,并通过电渗析来转化成氢氧化锂与双极性膜。
    • 8. 发明申请
    • METHOD FOR THE HYDROMETALLURGICAL RECOVERY OF LITHIUM FROM THE FRACTION OF USED GALVANIC CELLS CONTAINING LITHIUM, IRON AND PHOSPHATE
    • 海德鲁冶炼金属回收率从锂磷酸铁锂含分数的方法中使用的原电池
    • WO2014056608A3
    • 2015-01-08
    • PCT/EP2013003027
    • 2013-10-09
    • ROCKWOOD LITHIUM GMBH
    • WOHLGEMUTH DAVIDSCHNEIDER MARK ANDRESPIELAU REBECCAWILLEMS JOHANNESSTEINBILD MARTIN
    • C22B7/00C22B26/12
    • C22B26/12B01D61/445B01D61/58C01B25/45C01D15/02C22B7/007Y02P10/234
    • The invention relates to a method for the hydrometallurgical recovery of lithium from the fraction of used galvanic cells containing lithium, iron and phosphate. According to the invention, a fraction containing lithium, iron and phosphate having an aluminum content of up to 5% by weight, and having a particle size of up to 150 μm, is introduced into sulfuric acid having a concentration of 0.5 to 3 mol/l in an amount that is at least stoichiometric relative to the lithium content of the fraction containing lithium, iron and phosphate and in a solid-to-liquid ratio in the range of 100 to 750 g/l, hydrogen peroxide is added in an amount that is at least stoichiometric relative to the iron content which is to be oxidized of the lithium iron phosphate-containing fraction or a lithium iron phosphate-containing fraction having an aluminum content of up to 5% by weight, and having a particle size of up to 500 μm, is introduced into hydrochloric acid having a concentration of 0.5 to 3 mol/l in an amount that is at least stoichiometric relative to the lithium content of the lithium iron phosphate-containing fraction and in a solid-to-liquid ratio in the range of 50 to 450 g/l, hydrogen peroxide is solublized at temperature of between 25 - 70°C in an amount that is at least stoichiometric relative to the iron content which is to be oxidised of the lithium iron phosphate-containing fraction or a lithium iron phosphate-containing fraction, the solution that contains the lithium sulphate solution or lithium chloride solution is separated off and the remaining residue is washed at least twice, the wash solution containing the separated lithium sulphate and the lithium sulphate and the wash solutions containing the lithium chloride and the lithium chloride are combined, and are converted to lithium hydroxide by electrodialysis on bipolar membranes.
    • 本发明涉及一种用于锂从含使用原电池的分数的磷酸铁锂,其具有铝含量为5重量%和粒径至多150微米的含锂铁磷酸盐分数湿法冶金回收 基于所述含磷酸盐的锂铁馏分的锂含量包括在引入具有0.5〜3摩尔/升的浓度和固液比的范围为100至750克/升或添加的硫酸至少化学计量的量 基于所述含磷酸盐的锂铁馏分的氧化铁的含量包括在过氧化氢或在其中至少化学计量量的具有铝含量为5重量%和粒径至多500微米的含有磷酸铁锂分数,其中,基于所述锂含量 含磷酸盐的锂铁级分包含至少化学计量量Salzsä 酸与0.5〜3摩尔/升的浓度,并介绍了固体在50至450g / l的范围内的液体比和含有另外的,基于所述锂铁磷酸盐的化学计量组分的至少氧化铁含量 在25的温度至70℃的过氧化氢的消化量,所形成的硫酸锂溶液或氯化锂溶液中分离出来,剩余的残余物洗涤至少两次,所分离的Lithiumsulfat-和锂含硫酸盐洗涤溶液或氯化锂和锂含氯化物的洗涤 解决方案相结合,并通过电渗析来转化成氢氧化锂与双极性膜。
    • 10. 发明申请
    • LITHIUMPULVERANODE
    • 锂粉末阳极
    • WO2014095561A1
    • 2014-06-26
    • PCT/EP2013/076364
    • 2013-12-12
    • ROCKWOOD LITHIUM GMBH
    • WIETELMANN, UlrichEMMEL, UteHARTNIG, Christoph
    • B22F1/00H01M4/134H01M4/1395H01M4/38H01M4/62H01M4/04H01M10/052
    • B22F1/0062B22F3/22B22F7/08H01M4/0404H01M4/0435H01M4/134H01M4/1395H01M4/366H01M4/382H01M4/622H01M10/052H01M2004/021H01M2004/027Y02P70/54
    • Die Erfindung betrifft eine Lithiumanode enthaltend sphärische Lithiummetallpartikel mit einem mittleren Durchmesser zwischen 5 und 200 μm, und ein fluorfreies kautschukartiges Bindemittel ausgewählt aus den Gruppen gesättigte Polyolefine und Polyolefin-Copolymere wie EPM (Ethylen- Propylen-Copolymere), EPDM (Ethylen-Propylen-Terpolymere) und Polybutene sowie ungesättigte Polymere (Dienpolymere und Diencopolymere) wie Naturkautschuke (NR), Butadienkautschuke (BR), Styrol-Butadien- Kautschuke (SBR), Poyisoprenkautschuke und Butylkautschuke (IIR, wie Polyisobutylenisoprenkautschuke, PIBI) sowie heteroelementhaltige Copolymere, beispielsweise gesättigte Copolymerkautschuke wie Ethylen-Vinylacetate (EVM), Hydrierte Nitril-Butadien-Kautschuke (HNBR), Epichlorhydrin-Kautschuke (ECO), Acrylat-Kautschuke (ACM) und Silikon-Kautschuke (Sl) sowie ungesättigte Copolymere wie beispielsweise Nitril-Kautschuke (NBR)
    • 本发明涉及一种含有具有5到200微米之间的平均直径的球形锂金属颗粒的锂阳极,并且从组饱和聚烯烃和聚烯烃共聚物如EPM(乙烯 - 丙烯共聚物),EPDM(乙烯 - 丙烯三元共聚物中选择的无氟橡胶粘合剂 )和聚丁烯和不饱和聚合物(二烯聚合物和共轭二烯共聚物),如天然橡胶(NR),丁二烯橡胶(BR),苯乙烯 - 丁二烯橡胶(SBR),Poyisoprenkautschuke和丁基橡胶(IIR,如Polyisobutylenisoprenkautschuke,被毙)以及含杂元素的共聚物,例如,饱和共聚物橡胶,如 乙烯乙酸乙烯酯(EVM),氢化丁腈橡胶(HNBR),氯醇橡胶(ECO),丙烯酸酯橡胶(ACM),和硅橡胶(SI),和不饱和共聚物,如丁腈橡胶(NBR)