会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 2. 发明授权
    • Method for the production of precision castings by centrifugal casting with controlled solidification
    • 通过离心铸造控制凝固生产精密铸件的方法
    • US06250366B1
    • 2001-06-26
    • US08937995
    • 1997-09-26
    • Alok ChoudhuryHarald ScholzMatthias BlumGeorg JarczykMarek GorywodaDavid Francis Lupton
    • Alok ChoudhuryHarald ScholzMatthias BlumGeorg JarczykMarek GorywodaDavid Francis Lupton
    • B22D1306
    • B22D13/04B22D27/003B22D27/045B22D27/15
    • In the production of precision castings by centrifugal casting with controlled solidification, a melt is cast under vacuum or shield gas into a pre-heated mold (15) with a central gate (19) and several mold cavities proceeding from the gate toward the outer circumference (Da) of the mold (15). To prevent the formation of shrinkholes and porous areas in the castings, to save energy, and to increase the production rate, the mold (15) is operated at temperatures which decrease from the inside toward the outside. The mold consists of a material or material combination with a coefficient of thermal conductivity lower than that of copper. Before the melt is poured, the mold (15) is heated, starting from the gate (19), by a heating device (20), which projects into the gate, so that the gate (19) reaches a temperature which is a function of the material being cast. Heating is carried out at a rate sufficient to produce a temperature gradient of at least 100° C., preferably of 200-600° C., even more preferably of 300-500° C., between the inside circumference (Di) and the outside circumference (Da). The invention is used preferably for the production of precision castings of metals of the group titanium, titanium alloys with at least 40 wt. % of the titanium, and superalloys.
    • 在通过具有受控凝固的离心铸造生产精密铸件时,将熔体在真空下或保护气体下铸入具有中心浇口(19)的预热模具(15)中,并且从浇口朝向外圆周 (15)的(Da)。 为了防止在铸件中形成收缩孔和多孔区域,为了节省能量并提高生产率,模具(15)在从内向外减小的温度下运行。 模具由材料或材料组合组成,其导热系数低于铜的导热系数。 在熔融物浇注之前,模具(15)从浇口(19)开始被加入装置(20)加热,加热装置(20)突入浇口,使得浇口(19)达到功能的温度 的材料被铸造。 以足以在内圆周(Di)和内径(Di)之间产生至少100℃,优选200-600℃,甚至更优选300-500℃的温度梯度的速率进行加热 外围(Da)。 本发明优选用于生产钛,钛合金金属的精密铸件,其具有至少40wt。 %的钛和超级合金。