    • Process for producing refractory particles
    • 耐火材料颗粒的制造方法
    • US08025824B2
    • 2011-09-27
    • US12794839
    • 2010-06-07
    • Yukihiro Ushimaru
    • Yukihiro Ushimaru
    • B29B9/00C04B35/48C04B35/49C04B35/00
    • C04B33/1324B09B3/005C04B35/107C04B35/109C04B35/484C04B35/657C04B35/66C04B2235/3201C04B2235/3206C04B2235/3208C04B2235/3232C04B2235/327C04B2235/3272C04B2235/3418C04B2235/5427C04B2235/72C04B2235/721Y02P40/69
    • To provide a process for producing high-purity highly oxidized refractory particles easily with good productivity by treating a spent refractory containing ZrO2 and Al2O3 to reduce components other than ZrO2 and Al2O3 to levels unproblematic for practical use as raw material for electrofused refractories and to increase the content of the ZrO2 and/or Al2O3 component.A process for producing refractory particles, which comprises introducing to and melting in a melting furnace both a spent refractory which contains, by mass % as chemical components, from 75 to 97% of ZrO2 and/or Al2O3, from 2 to 25% of SiO2, from 0.4 to 7% in total of Na2O, K2O and Li2O(Na2O+K2O+Li2O), at most 2% of CaO and at most 2% of MgO, and carbon particles in an amount of from 1 to 8% by outer mass percentage based on the spent refractory, and after the melting, tapping the melt while blowing compressed air against the melt to form refractory particles having the content of ZrO2 and/or Al2O3 increased.
    • 为了提供通过处理含有ZrO 2和Al 2 O 3的废耐火材料以便将ZrO 2和Al 2 O 3以外的成分除去以外的其他成分,作为电熔耐火材料的原料的实用化水平,能够容易地以高生产率制造高纯度高氧化物的耐火材料粒子的方法, ZrO 2和/或Al 2 O 3组分的含量。 一种耐火材料颗粒的制造方法,其特征在于,在熔融炉中,将以质量%计的化学成分含有75〜97%的ZrO 2和/或Al 2 O 3,2〜25%的SiO 2, ,Na2O,K2O和Li2O(Na2O + K2O + Li2O)的总和为0.4〜7%,CaO最多为2%,MgO为2%以下,外部为1〜8%的碳粒子 基于消耗的耐火材料的质量百分比,熔融之后,将熔融物吹入熔融物中,形成具有ZrO 2和/或Al 2 O 3的含量的耐火材料粒子。