    • Method of molding aromatic polyimide resin
    • 芳香族聚酰亚胺树脂成型方法
    • US5718855A
    • 1998-02-17
    • US817927
    • 1997-05-09
    • Kiyokazu AkahoriKazunari Iwamoto
    • Kiyokazu AkahoriKazunari Iwamoto
    • B29C71/02B29C43/00B29C43/02B29C43/56B29C67/04B29K27/12B29K77/00
    • B29C67/04B29C43/003B29C43/56B29C2791/005B29K2079/08B29K2105/251B29K2427/12
    • A method of molding an aromatic polyimide resin, comprising compression molding an aromatic polyimide resin composition powder comprising an aromatic polyimide resin and a fluorine resin added thereto, and then sintering the compression molded product in a mixed gas atmosphere of oxygen and inert gas, having the oxygen concentration of 0.1 to 10% at 360.degree. to 480.degree. C., or sintering the compression molded product in an inert gas atmosphere and then heat treating the same in a mixed gas atmosphere of oxygen and inert gas at 360.degree. to 480.degree. C. This method can solve the problems on color shade and strength due to sintering in the case of molding an aromatic polyimide resin having a fluorine resin added thereto, and can provide a polyimide molding having excellent quality.
    • PCT No.PCT / JP95 / 02266 Sec。 371日期:1996年5月9日 102(e)日期1996年5月9日PCT提交1995年11月6日PCT公布。 第WO96 / 14977号公报 日期:1996年5月23日一种芳香族聚酰亚胺树脂的成型方法,包括将包含芳香族聚酰亚胺树脂和氟树脂的芳香族聚酰亚胺树脂组合物粉末压缩成型,然后在氧气和惰性气体的混合气体气氛中烧结压缩成型体 气体,在360〜480℃下氧浓度为0.1〜10%,或在惰性气体气氛下烧结压缩成型体,然后在氧气和惰性气体的混合气体气氛中在360℃下进行热处理 该方法可以解决在加入氟树脂的芳族聚酰亚胺树脂成型的情况下由于烧结引起的色调和强度问题,并且可以提供具有优良品质的聚酰亚胺成型体。