    • In one embodiment, a method of modifying a surface of a substrate includes activating the surface of the substrate, and polymerizing the surface of the substrate. The polymerizing including subjecting the surface of the substrate to a monomer solution at a temperature of between 105° C. and 130° C. for a first period of time and subjecting the surface of the substrate to the monomer solution at a temperature of between 70° C. and 90° C. for a second period of time different than the first period of time. In another embodiment, a method of modifying a surface of a substrate includes activating the surface of the substrate, and graft polymerizing a vinyl monomer onto the surface of the substrate. The polymerizing including subjecting the surface of the substrate to a mixture including a monomer solution and 2,2,6,6-tetramethyl-1-piperidinyloxy at a concentration of between 5 and 20 mM. In another embodiment, an apparatus includes a substrate having a surface. The surface has a set of polymers terminally graphed thereon. The apparatus being configured to sorb a chemical solute. The terminally grafter polymer layer being formed on the surface of the substrate by a controlled graft polymerization process.
    • 在一个实施方案中,修饰基材表面的方法包括活化基材的表面,并使基材的表面聚合。 聚合包括将基材表面在105℃和130℃之间的温度下将单体溶液经历第一段时间,并将基材表面在70℃的温度下进行单体溶液 °C和90°C,持续第二个时间段不同于第一个时间段。 在另一个实施方案中,修饰基材表面的方法包括活化基材的表面,以及将乙烯基单体接枝聚合到基材的表面上。 聚合包括将基材表面经受包含单体溶液和浓度为5至20mM的2,2,6,6-四甲基-1-哌啶氧基的混合物。 在另一个实施例中,一种装置包括具有表面的基底。 该表面具有一组端接在其上的聚合物。 该装置构造成吸附化学溶质。 通过受控的接枝聚合方法在基材的表面上形成末端接枝聚合物层。