    • Lamp reflector substrate, glass, glass-ceramic materials and process for making the same
    • 灯反射器基板,玻璃,玻璃陶瓷材料及其制造方法
    • US07091141B2
    • 2006-08-15
    • US10804482
    • 2004-03-18
    • William E. HorsfallRonald L. Stewart
    • William E. HorsfallRonald L. Stewart
    • C03C10/14G02B5/08
    • C03C3/085C03C3/093C03C3/097C03C3/118C03C10/0009C03C10/0027C03C10/0054
    • The present invention relates to glass, glass-ceramic materials, lamp reflectors and processes for making them. The glass material has a composition, by weight of the total composition, comprising 56–67% SiO2; 9–22% Al2O3; 3.4–3.8% Li2O; 1.8–2.6% ZnO; 1.5–2.5% MgO; 3.3–5% TiO2; 0–2.5% ZrO2; 1.5–3% B2O3; 0–6% P2O5; 0–0.6% F; less than 500 ppm Fe; and components resulting from effective amount of at least one refining agent. The glass-ceramic material of the present invention contains β-quartz solid solution as the predominant crystalline phase, and can be obtained by proper thermal treatment of the glass-ceramic material. The glass-ceramic material is particularly suitable for heat-resistant lamp reflectors which require a high surface smoothness Ra of lower than 75 nm, a low CTE between 25 and 300° C. of less than 10×10−7 K−1, and IR transmission at about 1050 nm of over 80% at a thickness of 3 mm.
    • 本发明涉及玻璃,玻璃陶瓷材料,灯反射体及其制造方法。 该玻璃材料具有按总组合物的重量计包含56-67%SiO 2的组成; 9-22%的Al 2 O 3 3; 3.4-3.8%Li 2 O; 1.8-2.6%ZnO; 1.5-2.5%MgO; 3.3-5%TiO 2; 0-2.5%ZrO 2 2; 1.5-3%B 2 O 3 3; 0-6%P 5 0-0.6%F; 小于500ppm Fe; 以及由有效量的至少一种澄清剂产生的成分。 本发明的玻璃 - 陶瓷材料含有作为主要结晶相的β-石英固溶体,可以通过玻璃 - 陶瓷材料的适当热处理获得。 玻璃陶瓷材料特别适用于要求低于75nm的高表面平滑度Ra,25-300℃之间的低CTE,小于10×10 -7 -7℃的耐热灯反射器, K 0〜-1,在约1050nm处的IR透射超过80%,厚度为3mm。