    • The invention provides a method of manufacturing an electrochemical cell housing wherein a beta-alumina tube has an open end attached to a casing via an alpha-alumina ring. In the method the alpha-alumina ring is thermocompression bonded to a metal ring by hot isostatic pressing, the alpha-alumina ring is then glass welded to the open end of the tube, and the metal ring is metal welded to the casing. The invention also provides a cell housing wherein a beta-alumina tube is located in spaced relationship within a metal casing. The tube is glass welded to an alpha-alumina ring which is thermocompression bonded on a curved radially facing surface thereof to a metal ring, the metal ring being metal welded to the casing.
    • 本发明提供了一种制造电化学电池壳体的方法,其中β-氧化铝管具有通过α-氧化铝环连接到壳体的开口端。 在该方法中,通过热等静压将α-氧化铝环热压接合到金属环上,然后将α-氧化铝环玻璃焊接到管的开口端,金属环被金属焊接到壳体上。 本发明还提供了一种电池壳体,其中β-氧化铝管在金属壳体内以间隔的关系定位。 该管被玻璃焊接到α-氧化铝环上,该α-氧化铝环在其弯曲的径向对置的表面上被热压粘合到金属环上,金属环被金属焊接到壳体上。