会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明授权
    • Method and apparatus for measuring thermal diffusivity by ac
joule-heating
    • 通过焦耳加热测量热扩散率的方法和装置
    • US5080495A
    • 1992-01-14
    • US573810
    • 1990-08-28
    • Toshimasa HashimotoAkira MiyamotoKohei ShizukaTeruo Hyugaji
    • Toshimasa HashimotoAkira MiyamotoKohei ShizukaTeruo Hyugaji
    • G01N25/18
    • G01N25/18
    • Disclosed is a method for measuring the thermal diffusivity in the thickness direction of a thin sample plate, which has the steps of forming a conductive thin layer on at least one surface of said thin sample plate to allow the thin film to function as an ac heater generating joule heat, applying an ac current modulated with a given modulation frequency to the ac heater (conductive thin layer) so as to produce ac joule-heating, generating an oscillation response corresponding to said ac joule-heating on the opposite surface of the ac heater, and measuring the phase shift between said oscillation response, and the ac joule-heating, thereby obtaining the thermal diffusivity in the thickness direction of said sample plate. Apparatus useful for the method are also disclosed.
    • 公开了一种用于测量薄样品板的厚度方向的热扩散率的方法,其具有在所述薄样品板的至少一个表面上形成导电薄层以允许薄膜用作交流加热器的步骤 产生焦耳热,将以给定调制频率调制的交流电流施加到交流加热器(导电薄层),以产生交流加热,在交流电流的相对表面上产生对应于所述交流焦耳加热的振荡响应 加热器,并测量所述振荡响应和交流焦加热之间的相移,从而获得所述样品板的厚度方向上的热扩散率。 还公开了对该方法有用的装置。
    • 2. 发明申请
    • SIMULATION DEVICE, SIMULATION SYSTEM, METHOD OF SIMULATION AND PROGRAM
    • 仿真器件,仿真系统,仿真和程序方法
    • US20130132046A1
    • 2013-05-23
    • US13638757
    • 2011-03-07
    • Akira MiyamotoMichihisa KoyamaKazuki Nakamura
    • Akira MiyamotoMichihisa KoyamaKazuki Nakamura
    • G06F17/50
    • G06F17/5009G01N15/0886
    • A simulation system (101) includes an X-ray CT device (11) that obtains a tomographic image of a porous sample, and a simulation device (14) that simulates a mercury intrusion method by processing a laminated tomographic image of the sample. The simulation device (14) includes a modeling means which processes the laminated tomographic image of the sample, and which models an internal structure of the sample, a minimum-diameter obtaining means that obtains a minimum entrance diameter when mercury enters in a pore of the sample at a predetermined pressure based on a surface energy of the sample and a pressure, and a means that simulates a liquid entering in the interior of the pore from one surface of the sample based on a diameter of the pore of the modeled sample and the minimum entrance diameter.
    • 模拟系统(101)包括获得多孔样品的断层图像的X射线CT装置(11),以及通过处理样品的层叠断层图像来模拟水银侵入方法的模拟装置(14)。 模拟装置(14)包括:模拟装置,其处理样品的层叠断层图像,并对样品的内部结构进行建模;最小直径获取装置,当汞进入到所述样品的孔中时获得最小入口直径 基于样品的表面能和压力的预定压力的样品,以及基于样品的孔的直径来模拟从样品的一个表面进入孔的内部的液体的装置,以及 最小入口直径
    • 8. 发明授权
    • Composite sinter of silicon nitride/boron nitride and method for
manufacturing thereof
    • 氮化硅/氮化硼的复合烧结体及其制造方法
    • US4412008A
    • 1983-10-25
    • US234939
    • 1981-02-11
    • Akira MiyamotoMasaru IshikawaMasaaki NishiKenki IshizawaAkira Shiranita
    • Akira MiyamotoMasaru IshikawaMasaaki NishiKenki IshizawaAkira Shiranita
    • C04B35/583C04B35/591C04B35/58
    • C04B35/591
    • A composite sinter of silicon nitride/boron nitride, which consists essentially of, in weight percentage, silicon nitride within the range of from 60 to 97% and boron nitride within the range of from 3 to 40%, and wherein said boron nitride is present as a dispersed phase in the network of said silicon nitride; said composite sinter of silicon nitride/boron nitride being manufactured by the steps of: kneading a silicon powder within the range of from 47.3 to 95.1 wt.% and a boron nitride powder within the range of from 4.9 to 52.7 wt. %, as raw materials, with the use of an organic solvent solution containing a dispersant and a binder; press-forming the resultant kneaded mixture to prepare a green compact; sintering said green compact in a non-oxidizing atmosphere at a temperature within the range of from 1,100.degree. to 1,300.degree. C. to prepare a sinter having a strength permitting machining; machining said sinter into prescribed dimensions; and sintering again the resultant machined sinter in a nitrogen atmosphere at a temperature within the range of from 1,250.degree. to 1,450.degree. C. to nitrify the same, thereby improving strength and thermal shock resistance of said sinter.
    • 氮化硅/氮化硼的复合烧结体,其重量百分比基本上由60至97%的氮化硅和3至40%的氮化硼组成,并且其中存在所述氮化硼 作为所述氮化硅网络中的分散相; 所述氮化硅/氮化硼的复合烧结体通过以下步骤制造:将硅粉末在47.3至95.1重量%的范围内捏合并且硼氮化物粉末在4.9至52.7重量%的范围内。 %,作为原料,使用含有分散剂和粘合剂的有机溶剂溶液; 压制所得捏合混合物以制备生坯; 在非氧化性气氛中在1100〜1300℃的温度下烧结所述生坯,制备具有允许加工强度的烧结体; 将烧结体加工成规定的尺寸; 并在氮气气氛中再次烧结得到的机械加工的烧结体,温度范围为1250℃至1450℃,对其进行硝化,从而提高了所述烧结体的强度和耐热冲击性。
    • 10. 发明授权
    • Aromatic polycarbonate molded article and resin composition
    • 芳香族聚碳酸酯成型品和树脂组合物
    • US08048955B2
    • 2011-11-01
    • US11587817
    • 2005-04-25
    • Kazuhiro ShibuyaAkira MiyamotoKazuharu Yasuda
    • Kazuhiro ShibuyaAkira MiyamotoKazuharu Yasuda
    • C08G64/00C08G64/04C08K3/16C08K5/42C08K5/521C08K5/02
    • C08K5/09Y10T428/24942Y10T428/24967Y10T428/269C08L69/00
    • A polycarbonate thin molded article containing a resin composition, the resin composition containing: 100 parts by weight of a resin (A), the resin (A) being an aromatic polycarbonate or a resin mainly containing an aromatic polycarbonate;0.1 to 200 parts by weight of an inorganic compound (B); 0.001 to 10 parts by weight of at least one compound (C) selected from an organic acidic compound and an organic acidic compound derivative; and 0.001 to 1 part by weight of at least one metal salt (D) selected from an organic acid alkali metal salt and an organic acid alkaline earth metal salt, a part corresponding to at least 50% of the surface area of the polycarbonate thin molded article having a thickness of less than 0.7 mm, and a shrinkage ratio S1(%) in a molding flow direction of the polycarbonate thin molded article upon its being left under an atmosphere of 170° C. for 30 minutes satisfying the following formula (1): −60
    • 含有树脂组合物的聚碳酸酯薄模制品,该树脂组合物含有:100重量份的树脂(A),树脂(A)是芳族聚碳酸酯或主要含有芳族聚碳酸酯的树脂; 0.1〜200重量份无机化合物(B); 0.001至10重量份的至少一种选自有机酸性化合物和有机酸性化合物衍生物的化合物(C); 和0.001至1重量份的至少一种选自有机酸碱金属盐和有机酸碱土金属盐的金属盐(D),其对应于聚碳酸酯薄模制品的至少50%的表面积 制品的厚度小于0.7mm,聚碳酸酯薄模制品的成型流动方向上的收缩率S1(%)在170℃的气氛下放置30分钟,满足下式(1 ):-60