会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 4. 发明授权
    • Ethylene/alpha-olefin interpolymer suitable for use in fiber applications, and fibers made therefrom
    • 适用于纤维应用的乙烯/α-烯烃互聚物和由其制成的纤维
    • US08907030B2
    • 2014-12-09
    • US13820795
    • 2010-09-29
    • Mehmet DemirorsLawrence J. EfflerLonnie G. HazlittTeresa P. KarjalaCristina Serrat
    • Mehmet DemirorsLawrence J. EfflerLonnie G. HazlittTeresa P. KarjalaCristina Serrat
    • C08F210/16C08F10/00D01F6/30
    • C08F210/16C08F10/00D01F6/30C08F210/14C08F2500/03C08F2500/06C08F2500/12C08F4/6546
    • The instant invention provides an ethylene/alpha-olefin interpolymer suitable for use in fiber applications, and fibers made therefrom. The ethylene/alpha-olefin interpolymer according to the present invention has a CDBI of less than 60%, and comprises at least two fractions in crossfractionation of the ethylene/alpha-olefin interpolymer, eluting from 85° C. to 90° C. and from 90° C. to 95° C., comprising a weight fraction ratio of >0.68 and a molecular weight homogeneity index of greater than 0.65; wherein the weight fraction ratio is the ratio of the weight of polymer in each fraction divided by the weight of polymer eluting between 95° C. and 100° C. and the molecular weight homogeneity index is the ratio of the weight average molecular weight of the polymer in the fraction divided by the weight average molecular weight of the polymer eluting between 95° C. and 100° C., and wherein the ethylene/alpha-olefin interpolymer has a density in the range of from 0.920 to 0.965 g/cm3, and a melt index (I2) in the range of from 0.5 to 100 g/10 minutes, and melt flow ratio (I10/I2) in the range of from 5.8 to 8.
    • 本发明提供了适用于纤维应用的乙烯/α-烯烃互聚物和由其制成的纤维。 根据本发明的乙烯/α-烯烃互聚物的CDBI小于60%,并且在85℃至90℃下从乙烯/α-烯烃互聚物的交叉分级中至少包含两个馏分, 包括重量分数比> 0.68且分子量均匀度指数大于0.65的90℃至95℃; 其中重量分数比是每个级分中聚合物的重量比除以95℃和100℃之间洗脱的聚合物的重量的比例,分子量均匀度指数是重均分子量 所述级分中的聚合物除以在95℃和100℃之间洗脱的聚合物的重均分子量,并且其中所述乙烯/α-烯烃互聚物的密度在0.920至0.965g / cm 3的范围内, 熔体指数(I 2)为0.5-100g / 10分钟,熔体流动比(I10 / I2)为5.8-8。
    • 5. 发明申请
    • ETHYLENE/ALPHA-OLEFIN INTERPOLYMER SUITABLE FOR USE IN FIBER APPLICATIONS, AND FIBERS MADE THEREFROM
    • 适用于光纤应用的乙烯/丙烯酰胺嵌段共聚物及其制备的纤维
    • US20130190465A1
    • 2013-07-25
    • US13820795
    • 2010-09-29
    • Mehmet DemirorsLawrence J. EfflerLonnie G. HazlittTeresa P. KarjalaCristina Serrat
    • Mehmet DemirorsLawrence J. EfflerLonnie G. HazlittTeresa P. KarjalaCristina Serrat
    • C08F210/16
    • C08F210/16C08F10/00D01F6/30C08F210/14C08F2500/03C08F2500/06C08F2500/12C08F4/6546
    • The instant invention provides an ethylene/alpha-olefin interpolymer suitable for use in fiber applications, and fibers made therefrom. The ethylene/alpha-olefin interpolymer according to the present invention has a CDBI of less than 60%, and comprises at least two fractions in crossfractionation of the ethylene/alpha-olefin interpolymer, eluting from 85° C. to 90° C. and from 90° C. to 95° C., comprising a weight fraction ratio of >0.68 and a molecular weight homogeneity index of greater than 0.65; wherein the weight fraction ratio is the ratio of the weight of polymer in each fraction divided by the weight of polymer eluting between 95° C. and 100° C. and the molecular weight homogeneity index is the ratio of the weight average molecular weight of the polymer in the fraction divided by the weight average molecular weight of the polymer eluting between 95° C. and 100° C., and wherein the ethylene/alpha-olefin interpolymer has a density in the range of from 0.920 to 0.965 g/cm3, and a melt index (I2) in the range of from 0.5 to 100 g/10 minutes, and melt flow ratio (I10/I2) in the range of from 5.8 to 8.
    • 本发明提供了适用于纤维应用的乙烯/α-烯烃互聚物和由其制成的纤维。 根据本发明的乙烯/α-烯烃互聚物的CDBI小于60%,并且在85℃至90℃下从乙烯/α-烯烃互聚物的交叉分级中至少包含两个馏分, 包括重量分数比> 0.68且分子量均匀度指数大于0.65的90℃至95℃; 其中重量分数比是每个级分中聚合物的重量比除以95℃和100℃之间洗脱的聚合物的重量的比例,分子量均匀度指数是重均分子量 所述级分中的聚合物除以在95℃和100℃之间洗脱的聚合物的重均分子量,并且其中所述乙烯/α-烯烃互聚物的密度在0.920至0.965g / cm 3的范围内, 熔体指数(I 2)为0.5-100g / 10分钟,熔体流动比(I10 / I2)为5.8-8。