    • 7. 发明授权
    • Optical recording media and process for preparing same
    • 光记录介质及其制备方法
    • US5061597A
    • 1991-10-29
    • US566039
    • 1990-08-13
    • Hisaharu ToibanaMitsuyuki KuroiwaAkira TodoTakeshi Minoda
    • Hisaharu ToibanaMitsuyuki KuroiwaAkira TodoTakeshi Minoda
    • G11B7/243
    • G11B7/243G11B2007/24306G11B2007/24316G11B2007/24328G11B7/2533G11B7/2572G11B7/2578Y10S430/146Y10S430/165
    • The optical recording media disclosed herein comprises a substrate and a recording layer formed thereon, wherein the recording layer is irradiated with beam of energy to form thereon bits corresponding to given pieces of information and thereby record the pieces of information. The recording layer comprises Te, Cr, C and H, the proportion of Cr contained in said recording layer, based on all atoms constituting the recording layer, is 0.1-40 atom % and that of C contained in said recording layer is 0.1-40 atom %. In another aspect, the proportion of Cr contained in said recording layer, based on the sum total of Te and Cr atoms present in said recording layer, is 0.1-60 atom %, and the proportion, based on the sum total of Te, Cr and C atoms present in said recording layer, of C is 0.1-40 atom %. According to the optical recording media as disclosed above, the recording layer improves in oxidation resistance and long duration of life of the optical recording media can be expected, because the recording layer comprising Te, Cr, C and H. In this connection, the distribution of C contained in the recording layer is not always uniform, and C may be distributed in the recording layer so that the content of C becomes smaller in the direction receding from the substrate side.
    • 本文公开的光记录介质包括基板和形成在其上的记录层,其中记录层用能量束照射以在其上形成与给定条信息对应的位,从而记录信息。 记录层包括Te,Cr,C和H,基于构成记录层的所有原子,所述记录层中包含的Cr的比例为0.1-40原子%,并且所述记录层中包含的C的比例为0.1-40 原子%。 在另一方面,所述记录层中所含的Cr的比例,基于存在于所述记录层中的Te和Cr原子的总和为0.1-60原子%,并且所述比例基于Te,Cr的总和 存在于所述记录层中的C原子为C为0.1-40原子%。 根据如上所述的光记录介质,由于记录层包括Te,Cr,C和H,所以记录层的抗氧化性能提高,光记录介质的使用寿命可以延长,因此,分布 记录层中所含的C不总是均匀的,并且C可以分布在记录层中,使得C的含量在从基板侧退出的方向上变小。
    • 10. 发明申请
    • Propylene polymer composition and use thereof
    • 丙烯聚合物组合物及其用途
    • US20060057321A1
    • 2006-03-16
    • US10543360
    • 2004-01-16
    • Ryoji MoriTakashi NakagawaMamoru KagamiAkira Todo
    • Ryoji MoriTakashi NakagawaMamoru KagamiAkira Todo
    • B65D1/02C08L23/04
    • A61L29/041C08L23/10C08L23/142C08L2205/02C08L2207/12Y10T428/1397C08L2666/06
    • The invention provides a propylene polymer composition well balanced and excellent in transparency, flexibility, heat resistance, scratch resistance and rubber elasticity, and a medical tube made from the propylene polymer composition. The propylene polymer composition satisfies all the following properties (A), (B), (C) and (D): (A) the composition shows a loss tangent (tan δ) peak at a temperature in the range of −20 to 25° C. according to dynamic viscoelasticity measurement (10 rad/s) in a torsion mode, and the peak is 0.5 or above; (B) the storage elastic modulus G′ at 20° C. from the dynamic viscoelasticity measurement is in the range of 1.0×107 to 4.9×108 dyn/cm2; (C) the penetration temperature (° C.) determined in accordance with JIS K 7196 is in the range of 60 to 160° C.; and (D) the composition has a permanent set of not more than 30% as determined after the composition fixed between chucks 30 mm apart is 100% strained at a stress rate of 30 mm/min, maintained for 10 minutes and released for 10 minutes. The medical tube is made from the propylene polymer composition.
    • 本发明提供了一种丙烯聚合物组合物,其透明性,柔韧性,耐热性,耐刮擦性和橡胶弹性优良的平衡性以及由丙烯聚合物组合物制成的医用管。 丙烯聚合物组合物满足以下所有性质(A),(B),(C)和(D):(A)组合物在-20至25℃的温度范围内显示损耗角正切(tanδ)峰 根据动态粘弹性测量(10rad / s)在扭转模式下,峰值为0.5或更高; (B)来自动态粘弹性测量的20℃下的储能弹性模量G'在1.0×10 -7至4.9×10 8 dyn / cm 2的范围内 > 2 ; (C)根据JIS K 7196测定的穿透温度(℃)为60〜160℃的范围。 和(D)组合物具有不超过30%的永久变形,如在固定在30mm间距的卡盘之间的组合物以30mm / min的应力速率100%应变之后确定的,保持10分钟并释放10分钟 。 医用管由丙烯聚合物组合物制成。