    • 6. 发明授权
    • Inkjet recording sheet
    • 喷墨记录纸
    • US06777039B2
    • 2004-08-17
    • US10125580
    • 2002-04-19
    • Kazuyuki KoikeTakashi KobayashiKatsuyoshi SuzukiRyoichi Nakano
    • Kazuyuki KoikeTakashi KobayashiKatsuyoshi SuzukiRyoichi Nakano
    • B41M500
    • B41M5/52B41M5/5218B41M5/5227B41M5/5236B41M5/5245B41M5/5254Y10T428/24802
    • An inkjet recording sheet comprising a support and, on a surface of the support, a colorant-receiving layer formed by applying a first coating liquid, adding a second coating liquid, after application of the first coating liquid and before the same shows a decreasing rate of drying, and thereafter hardening and drying the coat layer to form a porous structure. The first coating liquid has a pH value of 5 or lower, and is obtained by adding a solution which includes polyvinyl alcohol, a nonionic surfactant and/or amphoteric surfactant and a high boiling point organic solvent, to a dispersion including a cationic resin and vapor-phase-process silica having a specific surface area of at least 200 m2/g as measured by the BET method. The second coating liquid has a pH value of 8.5 or higher and includes a cross-linking agent capable of cross-linking the polyvinyl alcohol, an organic mordant and a nonionic surfactant.
    • 一种喷墨记录纸,其包括支撑体,并且在所述支撑体的表面上,通过施加第一涂布液,添加第二涂布液,在施加所述第一涂布液之后并在其之前显示出降低率而形成的着色剂接收层 干燥,然后硬化和干燥涂层以形成多孔结构。 第一涂布液的pH值为5以下,通过将包括聚乙烯醇,非离子表面活性剂和/或两性表面活性剂和高沸点有机溶剂的溶液加入到包含阳离子树脂和蒸气的分散体中而获得 通过BET法测量的具有至少200m 2 / g的比表面积的相过程二氧化硅。 第二涂布液的pH值为8.5以上,并且包括能够交联聚乙烯醇的交联剂,有机媒染剂和非离子表面活性剂。
    • 7. 发明授权
    • Optical multilayer film and image display device
    • 光学多层膜和图像显示装置
    • US08000012B2
    • 2011-08-16
    • US12022640
    • 2008-01-30
    • Takashi KobayashiKatsuyoshi Suzuki
    • Takashi KobayashiKatsuyoshi Suzuki
    • G02B1/10
    • G02B1/111
    • A first adhesion layer and a second adhesion layer are formed on a base material formed of polyester biaxially stretched in this order from the side of the base material. Additionally, a hard coat layer and an antireflection layer are formed on the second adhesion layer to form a multilayer film. When refractive indices of the base material, the first adhesion layer, the second adhesion layer, and the hard coat layer are η1, η2, η3, and η4, respectively, the refractive indices are adjusted so as to satisfy the following formulae (1) to (3) to prevent rainbow unevenness. (η1/η4)1/2×0.95≦η2/η3≦(η1/η4)1/2×1.05  (1) η1
    • 第一粘合层和第二粘合层形成在从基材侧开始依次双轴拉伸聚酯的基材上。 此外,在第二粘合层上形成硬涂层和抗反射层以形成多层膜。 当基材,第一粘合层,第二粘合层和硬涂层的折射率分别为1,eegr 2,e 3和4时,折射率被调节为 以满足下述式(1)〜(3)来防止彩虹不均匀。 (&eegr; 1 /&eegr; 4)1/2×0.95&nlE;&eegr; 2 /&eegr; 3&nlE;(&eegr; 1 /&eegr; 4)1/2×1.05(1)&eegr; 1 <&eegr )&eegr; 2&lt; 3(3)两个粘合层可以增强与基材的粘合强度。