    • 5. 发明授权
    • Method for producing concentrates
    • 生产精矿的方法
    • US07510593B2
    • 2009-03-31
    • US10564477
    • 2004-07-14
    • Seppo HeimalaMikko Ruonala
    • Seppo HeimalaMikko Ruonala
    • C22B3/04C22B3/44
    • C22B15/0008C22B15/0071C22B15/0089Y02P10/236
    • The invention relates to a method for processing concentrates, particularly concentrates produced from copper sulfide-based ores. According to the method, the concentrate (4) to be processed, obtained from ore concentration, is divided into two parts, to a concentrate (7) mainly containing poorly soluble components, and to a concentrate (8) mainly containing well soluble components. The concentrate (8) containing well soluble components is conducted to a leaching step (9), and the solution (13) obtained from said leaching step is conducted to at least one conversion step (11, 16), and to the conversion step (11) that is located first in the flowing direction, there is fed the concentrate (7) containing poorly soluble components. In the conversion step (11) that is located first in the flowing direction, at least the copper contained in the solution is converted into sulfidic form by means of the sulfide-form iron of the concentrate (7) containing poorly soluble components, and at least part of the solution (12) obtained from the conversion step (11, 16) is returned to the leaching step (9).
    • 本发明涉及一种处理浓缩物的方法,特别是由硫化铜基矿石生产的浓缩物。 根据该方法,将从矿石浓度得到的待处理浓缩物(4)分为主要含有不溶性成分的浓缩物(7)和主要含有可溶性成分的浓缩物(8)两部分。 将含有良好溶解成分的浓缩物(8)进行浸出步骤(9),将由所述浸出步骤得到的溶液(13)进行至少一个转化步骤(11,16),并进行转化步骤 11)首先位于流动方向,供给含有不易溶解成分的浓缩物(7)。 在首先位于流动方向的转化步骤(11)中,至少含有溶液中的铜通过含有不易溶解成分的浓缩物(7)的硫化物形式的铁转化成硫化物形式,并且在 将从转化步骤(11,16)获得的溶液(12)的至少一部分返回到浸出步骤(9)。
    • 8. 发明申请
    • Method for producing concentrates
    • 生产精矿的方法
    • US20060272454A1
    • 2006-12-07
    • US10564477
    • 2004-07-14
    • Seppo HeimalaMikko Ruonala
    • Seppo HeimalaMikko Ruonala
    • C22B15/00
    • C22B15/0008C22B15/0071C22B15/0089Y02P10/236
    • The invention relates to a method for processing concentrates, particularly concentrates produced from copper sulfide-based ores. According to the method, the concentrate (4) to be processed, obtained from ore concentration, is divided into two parts, to a concentrate (7) mainly containing poorly soluble components, and to a concentrate (8) mainly containing well soluble components. The concentrate (8) containing well soluble components is conducted to a leaching step (9), and the solution (13) obtained from said leaching step is conducted to at least one conversion step (11, 16), and to the conversion step (11) that is located first in the flowing direction, there is fed the concentrate (7) containing poorly soluble components. In the conversion step (11) that is located first in the flowing direction, at least the copper contained in the solution is converted into sulfidic form by means of the sulfide-form iron of the concentrate (7) containing poorly soluble components, and at least part of the solution (12) obtained from the conversion step (11, 16) is returned to the leaching step (9).
    • 本发明涉及一种处理浓缩物的方法,特别是由硫化铜基矿石生产的浓缩物。 根据该方法,将从矿石浓度得到的待处理浓缩物(4)分为主要含有不溶性成分的浓缩物(7)和主要含有可溶性成分的浓缩物(8)两部分。 将含有良好溶解成分的浓缩物(8)进行浸出步骤(9),将由所述浸出步骤得到的溶液(13)进行至少一个转化步骤(11,16),并进行转化步骤 11)首先位于流动方向,供给含有不易溶解成分的浓缩物(7)。 在首先位于流动方向的转化步骤(11)中,至少含有溶液中的铜通过含有不易溶解成分的浓缩物(7)的硫化物形式的铁转化成硫化物形式,并且在 将从转化步骤(11,16)获得的溶液(12)的至少一部分返回到浸出步骤(9)。