    • 1. 发明授权
    • Method for producing carbon fiber, carbon fiber, prepreg, and molded article from fiber-reinforced composite material
    • 从纤维增强复合材料制造碳纤维,碳纤维,预浸料和模塑制品的方法
    • US06171696B2
    • 2001-01-09
    • US09316246
    • 1999-05-21
    • Shinichi TakemuraYoshio SodaHideyuki OhnoYutaka AraiTomohiro Nakanishi
    • Shinichi TakemuraYoshio SodaHideyuki OhnoYutaka AraiTomohiro Nakanishi
    • D01F9145
    • D01F9/15D01F9/145Y10T428/24994Y10T428/29Y10T428/2964Y10T428/298Y10T442/2008Y10T442/603
    • The resent invention provides a carbon fiber which enables a molded article produced from a fiber-reinforced composite material using the carbon fiber to exhibit excellent flexibility and to be freed from defects such as bending. According to the method of the present invention the carbon fiber is produced by a two-stage infusibilizing process, namely carrying out a first-stage infusibilization of a pitch-based fiber, which is obtained from mesophase pitch having a softening point of 200 to 400° C. and a true density of 1.30 to 1.38 g/cm3, in a mixed gas atmosphere having a nitrogen dioxide concentration of 1 to 5% by volume and an oxygen concentration of 5 to 50% by volume, the balance being an inert gas or steam, at a temperature between 100 and 200° C. and then carrying out a second-stage infusibilization of the product of the first-stage infusibilization in a mixed gas atmosphere having a nitrogen dioxide concentration of 0.1 to 5% by volume and an oxygen concentration of 5 to 40% by volume, the balance being an inert gas or a mixture of the inert gas and steam, at a temperature between 200 and 350° C.
    • 本发明提供了一种碳纤维,其使得使用碳纤维的纤维增强复合材料制成的模制品显示出优异的柔性并且不会产生诸如弯曲的缺陷。根据本发明的方法,碳纤维是 通过两阶段渗透法生产,即进行沥青基纤维的第一阶段熔融,其由软化点为200-400℃的中间相沥青获得,真密度为1.30-1.38g / cm3,在二氧化氮浓度为1〜5体积%,氧浓度为5〜50体积%,余量为惰性气体或蒸汽的混合气体气氛中,温度为100〜200℃ 然后在二氧化氮浓度为0.1〜5体积%,氧浓度为5〜40体积%的混合气体气氛中进行第一阶段生产的产品的第二阶段的混合, 在余量为惰性气体或惰性气体与蒸汽的混合物之间,温度为200-350℃。
    • 3. 发明授权
    • Tapered hollow shaft
    • 锥形空心轴
    • US06273830B1
    • 2001-08-14
    • US09384385
    • 1999-08-27
    • Shinichi TakemuraHideyuki OhnoTomohiro NakanishiYutaka AraiMikio Shima
    • Shinichi TakemuraHideyuki OhnoTomohiro NakanishiYutaka AraiMikio Shima
    • A63B5310
    • B29C70/30A63B53/10A63B60/06A63B60/08A63B60/10A63B60/54A63B2060/0081A63B2209/02A63B2209/026B29K2995/0089B29L2031/5227B32B5/28Y10T428/139
    • A tapered hollow shaft made of a fiber reinforced composite material, which comprises: (a) at least one angle layer consisting essentially of polyacrylonitrile-based carbon fibers having a tensile modulus ranging from 200 to 500 GPa and a tensile strength ranging from 4000 to 5600 MPa; (b) at least one straight layer consisting essentially of polyacrylonitrile-based carbon fibers having a tensile modulus ranging from 200 to 460 GPa and a tensile strength ranging from 3500 to 5600 MPa; (c) at least one reinforcing layer consisting essentially of pitch-based carbon fibers or polyacrylonitrile-based carbon fibers each having a compressive breaking strain of 1.7 to 5.0%, a tensile modulus ranging from 5 to 160 GPa, a tensile strength ranging from 500 to 3000 MPa and a density ranging from 1.5 to 1.9 g/cm3 with the carbon fibers in the reinforcing layer being oriented to incline at an angle of 0° to ±5° to the axial direction of the shaft, with the reinforcing layer being arranged at the thinner portion of the shaft to extend from a tip thereof up to at least {fraction (1/20)} and not more than ¾ of the entire length of the shaft, and with the reinforcing layer being arranged at the outermost portion of the shaft.
    • 一种由纤维增强复合材料制成的锥形空心轴,其包括:(a)至少一个角度层,其基本上由聚丙烯腈基碳纤维组成,拉伸模量范围为200-500GPa,拉伸强度为4000-5600 MPa; (b)至少一个直层,其基本上由聚丙烯腈基碳纤维组成,拉伸模量范围为200-460GPa,拉伸强度为3500-5600MPa; (c)基本上由沥青类碳纤维或聚丙烯腈类碳纤维组成的至少一种增强层,其各自的压缩断裂应变为1.7〜5.0%,拉伸弹性模量为5〜160GPa,拉伸强度为500 至3000MPa,密度范围为1.5至1.9g / cm 3,加强层中的碳纤维相对于轴的轴向以0°至±5°的角度倾斜,并且加强层被布置 在所述轴的较薄部分处从其尖端延伸到所述轴的整个长度的至少{分数(1/20)}且不大于3/4,并且所述加强层布置在所述轴的最外部 轴。