热词
    • 5. 发明授权
    • Color cathode ray tube
    • 彩色阴极射线管
    • US4734615A
    • 1988-03-29
    • US884615
    • 1986-07-11
    • Norio KoikeHidemi MatsudaKiyoshi TokitaKaneharu Kida
    • Norio KoikeHidemi MatsudaKiyoshi TokitaKaneharu Kida
    • H01J9/14H01J29/07
    • H01J29/07H01J2229/0783
    • The shadow mask of a color cathode ray tube is arranged in the vicinity of a phosphor screen. The shadow mask is provided with through-holes that select the electron beams emitted from the electron guns. A layer comprising, as a filler, one or other of a metal, metal oxide, metal carbide, metal nutride, or a mixture of two or more of these, for example zirconium powder and, as a binder, one of an amorphous metal oxide compound, amorphous metal hydroxide compound or a mixture of these, for example silicon oxide, is formed on the surface of the shadow mask. This layer increases thermal radiation of the shadow mask, reduces electron scattering, and raises the residual emissivity.
    • 彩色阴极射线管的荫罩布置在荧光屏附近。 荫罩设置有选择从电子枪发射的电子束的通孔。 包含作为填料的金属,金属氧化物,金属碳化物,金属金刚石或其中的两种或更多种的混合物作为填料的层,例如锆粉末和作为粘合剂的无定形金属氧化物之一 化合物,无定形金属氢氧化物化合物或其混合物,例如氧化硅,形成在荫罩的表面上。 该层增加了荫罩的热辐射,减少了电子散射,并提高了剩余发射率。
    • 9. 发明授权
    • Method for manufacturing lepidocrocite
    • 菱镁矿生产方法
    • US4729846A
    • 1988-03-08
    • US4943
    • 1987-01-20
    • Yasushi MatsuiNorio KoikeKunio TakahashiHiroshi Matsue
    • Yasushi MatsuiNorio KoikeKunio TakahashiHiroshi Matsue
    • H01F1/11C01G49/02C01G49/06
    • C01G49/06C01P2004/52C01P2006/42
    • Lepidocrocite (.gamma.-FeOOH) with an large specific surface area and a uniform particle size is provided by a method comprising preparing a suspension of ferrous hydroxide at a pH of 6.5 to 7.5 by adding a ferrous salt solution with an alkali solution in an amount of 0.4 to 0.7 times the theoretical amount for converting all the ferrous salt to ferrous hydroxide, blowing an oxygen-containing gas into the suspension to form a seed crystal of .gamma.-FeOOH, completing the generation reaction of .gamma.-FeOOH by blowing an oxygen-containing gas into the suspension while adding an alkali solution to keep the pH of the suspension within a range of 3 to 5, in which an Si concentration of the suspensions for seed reaction and for generation reaction of .gamma.-FeOOH is controlled to be within 5 to 30 ppm.
    • 通过以下方法提供具有大的比表面积和均匀粒径的鳞状赤铁矿(γ-FeOOH),该方法包括通过将亚铁盐溶液与碱溶液一起加入至pH 6.5至7.5的方法制备氢氧化亚铁悬浮液 将所有亚铁盐转化为氢氧化亚铁的理论量的0.4〜0.7倍,向混悬液中吹入含氧气体,形成γ-FeOOH晶种,通过吹入含氧气体完成γ-FeOOH的发生反应 将气体加入到悬浮液中,同时加入碱溶液以将悬浮液的pH保持在3至5的范围内,其中用于种子反应的悬浮液和γ-FeOOH的发生反应的Si浓度被控制在5〜 30 ppm。