    • 1. 发明授权
    • Resin composition, heat seal film and layered film
    • 树脂组合物,热封膜和层状膜
    • US08716405B2
    • 2014-05-06
    • US13700521
    • 2011-05-27
    • Shigenori NakanoKaoru Suzuki
    • Shigenori NakanoKaoru Suzuki
    • C08F8/00C08L33/02C08L23/06C08L23/10
    • C09D133/02C08L23/0869C08L23/10C08L2205/02C08L23/0876
    • The present invention provides a resin composition including (1) at least one selected from the group consisting of ethylene-α,β-unsaturated carboxylic acid copolymers and ionomers thereof, which have a melt flow rate of from 0.5 g/10 min to 6 g/10 min, (2) at least one selected from the group consisting of ethylene-α,β-unsaturated carboxylic acid copolymers and ionomers thereof, which have a melt flow rate of from 10 g/10 min to 30 g/10 min, and (3) at least one selected from the group consisting of propylene homopolymers and copolymers obtained by copolymerization using propylene and one or more α-olefins excluding propylene, in which a structural unit derived from an α,β-unsaturated carboxylic acid ester is substantially not contained in the total amount of the ethylene-α,β-unsaturated carboxylic acid copolymers and the ionomers thereof.
    • 本发明提供一种树脂组合物,其包含(1)选自乙烯-α,β-不饱和羧酸共聚物及其离聚物中的至少一种,熔体流动速率为0.5g / 10min至6 g / 10分钟,(2)选自乙烯-α,β-不饱和羧酸共聚物及其离聚物中的至少一种,熔体流动速率为10g / 10min至30g / 10 min,和(3)选自丙烯均聚物和通过使用丙烯和除丙烯以外的一种或多种α-烯烃共聚获得的共聚物中的至少一种,其中衍生自α,β-不饱和羧酸的结构单元 乙烯-α,β-不饱和羧酸共聚物及其离聚物的总量基本上不含酯。
    • 2. 发明申请
    • RESIN COMPOSITION, HEAT SEAL FILM AND LAYERED FILM
    • 树脂组合物,热密封膜和层状膜
    • US20130079457A1
    • 2013-03-28
    • US13700521
    • 2011-05-27
    • Shigenori NakanoKaoru Suzuki
    • Shigenori NakanoKaoru Suzuki
    • C09D133/02
    • C09D133/02C08L23/0869C08L23/10C08L2205/02C08L23/0876
    • The present invention provides a resin composition including (1) at least one selected from the group consisting of ethylene-α,β-unsaturated carboxylic acid copolymers and ionomers thereof, which have a melt flow rate of from 0.5 g/10 min to 6 g/10 min, (2) at least one selected from the group consisting of ethylene-α,β-unsaturated carboxylic acid copolymers and ionomers thereof, which have a melt flow rate of from 10 g/10 min to 30 g/10 min, and (3) at least one selected from the group consisting of propylene homopolymers and copolymers obtained by copolymerization using propylene and one or more α-olefins excluding propylene, in which a structural unit derived from an α,β-unsaturated carboxylic acid ester is substantially not contained in the total amount of the ethylene-α,β-unsaturated carboxylic acid copolymers and the ionomers thereof.
    • 本发明提供一种树脂组合物,其包含(1)选自乙烯-α,β-不饱和羧酸共聚物及其离聚物中的至少一种,熔体流动速率为0.5g / 10min至6 g / 10分钟,(2)选自乙烯-α,β-不饱和羧酸共聚物及其离聚物中的至少一种,熔体流动速率为10g / 10min至30g / 10 min,和(3)选自丙烯均聚物和通过使用丙烯和除丙烯以外的一种或多种α-烯烃共聚获得的共聚物中的至少一种,其中衍生自α,β-不饱和羧酸的结构单元 乙烯-α,β-不饱和羧酸共聚物及其离聚物的总量基本上不含酯。
    • 9. 发明申请
    • Image Forming Apparatus
    • 图像形成装置
    • US20130202323A1
    • 2013-08-08
    • US13760401
    • 2013-02-06
    • Kenji TakeuchiKei IshidaKaoru SuzukiYuki Fukusada
    • Kenji TakeuchiKei IshidaKaoru SuzukiYuki Fukusada
    • G03G15/20
    • G03G15/2039G03G15/205G03G2215/2035
    • An image forming apparatus includes: a fixing device having a heating member, a heat source, a rotating member, and a temperature sensor; and a control device configured to control the heat source, wherein, in a case of a low temperature state where the temperature of the heating member is lower than a predetermined temperature, the control device to control the heat source such that the temperature of the heating member rises with a gradient equal to or greater than a predetermined value, and wherein, in a case of a high temperature state where the temperature of the heating member at the print-instruction receiving time is equal to or higher than the predetermined temperature, the control device to control the heat source such that the temperature of the heating member rises with a gradient smaller than that in the normal mode.
    • 图像形成装置包括:具有加热构件,热源,旋转构件和温度传感器的定影装置; 以及控制装置,其被配置为控制所述热源,其中,在所述加热构件的温度低于预定温度的低温状态的情况下,所述控制装置控制所述热源,使得所述加热温度 构件以等于或大于预定值的梯度升高,并且其中,在打印指令接收时间处的加热构件的温度等于或高于预定温度的高温状态的情况下, 控制装置来控制热源,使得加热构件的温度以比正常模式小的梯度上升。