    • Rapidly solidified magnesium base alloy sheet
    • 快速凝固的镁基合金板
    • US5078807A
    • 1992-01-07
    • US586179
    • 1990-09-21
    • Chin-Fong ChangSantosh K. Das
    • Chin-Fong ChangSantosh K. Das
    • B22F3/18C22C1/04C22C23/02C22F1/06
    • C22C1/0408C22F1/06
    • Magnesium base metal alloy sheet is produced by rolling the rolling stock extruded or forged from a billet at a temperature ranging from 200.degree. C. to 300.degree. C. The billet is consolidated from rapidly solidified magnesium based alloy powder that consists of the formula Mg.sub.bal Al.sub.a Zn.sub.b X.sub.c, wherein X is at least one element selected from the group consisting of manganese, cerium, neodymium, praseodymium, and yttrium, "a" ranges from about 0 to 15 atom percent, "b" ranges from about 0 to 4 atom percent, "c" ranges from about 0.2 to 3 atom percent, the balance being magnesium and incidental impurities, with the proviso that the sum of aluminum and zinc present ranges from about 2 to 15 atom percent. The alloy has a uniform microstructure comprised of fine grain size ranging from 0.2-1.0 .mu.m together with precipitates of magnesium and aluminum containing intermetallic phases of a size less than 0.1 .mu.m. The sheets have a good combination of mechanical strength and ductility and are suitable for military, space, aerospace and automotive application.
    • 镁贱金属合金板是通过在200℃〜300℃的温度范围内轧制从坯料中挤出或锻造的轧制坯料来制造的。坯料由快速固化的镁基合金粉末固结,该粉末由式MgbalAlaZnbXc, 其中X是选自锰,铈,钕,镨和钇中的至少一种元素,“a”为约0至15原子百分比,“b”为约0至4原子百分数,“c “范围为约0.2至3原子%,余量为镁和附带杂质,条件是存在的铝和锌的总和范围为约2至15原子%。 该合金具有由0.2-1.0μm的细晶粒尺寸以及尺寸小于0.1μm的含有金属间化合物的镁和铝的析出物组成的均匀微观结构。 这些板材具有机械强度和延展性的良好组合,适用于军事,太空,航空航天和汽车应用。
    • 9. 发明授权
    • Superplastically formed product from rolled magnesium base metal alloy
sheet
    • 轧制镁基金属合金板材的超塑性产品
    • US5316598A
    • 1994-05-31
    • US890199
    • 1992-05-29
    • Chin-Fong ChangSantosh K. Das
    • Chin-Fong ChangSantosh K. Das
    • C22C1/04C22F1/06C22F1/00C22C23/00
    • C22C1/0408C22F1/06
    • Magnesium base metal alloy sheet is produced by rolling the rolling stock extruded or forged from a billet at a temperature ranging from 200.degree. C. to 300.degree. C. The billet is consolidated from rapidly solidified magnesium based alloy powder that consists essentially of the formula Mg.sub.bal Al.sub.a Zn.sub.b X.sub.c, wherein X is at least one element selected from the group consisting of manganese, cerium, neodymium, praseodymium, and yttrium, "a" ranges from about 0 to 15 atom percent, "b" ranges from about 0 to 4 atom percent, "c" ranges from about 0.2 to 3 atom percent, the balance being magnesium and incidental impurities, with the proviso that the sum of aluminum and zinc present ranges from about 2 to 15 atom percent. The alloy has a uniform microstructure comprised of fine grain size ranging from 0.2-1.0 .mu.m together with precipitates of magnesium and aluminum containing intermetallic phases of a size less than 0.1 .mu.m. The sheets have a good combination of mechanical strength and ductility and are suitable for military, space, aerospace and automotive application. The sheets can be superplastically formed at temperatures ranging from 275.degree. C. to 300.degree. C. and at strain rates ranging from 10.sup.-1 to 10.sup.-2. The condition which maximizes superplastic ductility is a temperature of 300.degree. C. and a strain rate of 0.1/s. An elongation of 436%, combined with uniform deformation within the gage length, allows fabrication of complex shapes.
    • 通过在200℃至300℃的温度范围内轧制从坯料中挤出或锻造的轧制坯料来生产镁贱金属合金板。该坯料由基本上由式MgbalAlaZnbXc组成的快速固化的镁基合金粉末固结 其中X为选自锰,铈,钕,镨和钇中的至少一种元素,“a”为约0至15原子百分数,“b”为约0至4原子百分数,“ c“为约0.2至3原子%,余量为镁和附带杂质,条件是存在的铝和锌的总和范围为约2至15原子%。 该合金具有由0.2-1.0μm的细晶粒尺寸以及尺寸小于0.1μm的含有金属间化合物的镁和铝的析出物组成的均匀微观结构。 这些板材具有机械强度和延展性的良好组合,适用于军事,太空,航空航天和汽车应用。 片材可以在275℃至300℃的温度范围内以10-1至10-2的应变速率超塑性地形成。 使超塑性延展性最大化的条件是温度为300℃,应变速率为0.1 / s。 伸长率为436%,结合量规长度内的均匀变形,允许制造复杂的形状。