会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明申请
    • METHOD OF PRODUCING RECORDING MEDIUM
    • 制作记录媒体的方法
    • US20100243160A1
    • 2010-09-30
    • US12749537
    • 2010-03-30
    • Ryoichi NAKANOJun NAITO
    • Ryoichi NAKANOJun NAITO
    • B29C63/00
    • B41M5/506D21H19/385D21H19/40D21H19/822Y10T156/1153
    • A method of producing a recording medium includes: providing a substrate, the substrate including a resin layer containing a polyolefin resin formed on one or both sides of a base paper; subjecting a resin layer-side surface of the substrate to a cooling-separation treatment using a cooling-separation belt-fixing smoother apparatus, the apparatus including a heating and pressurizing unit and the unit including a belt member, by applying heat and pressure to the surface at a temperature of at least 80° C. and less than 140° C. using the heating and pressurizing unit, cooling the surface to a temperature of 60° C. or lower, and separating the surface from the belt member; and forming an image recording layer on the resin layer-side surface of the substrate.
    • 制造记录介质的方法包括:提供基板,所述基板包括在原纸的一面或两面上形成有聚烯烃树脂的树脂层; 使用冷却分离带固定平滑装置将基板的树脂层侧表面进行冷却分离处理,该装置包括加热加压单元,并且包括带构件的单元通过向 使用加热和加压单元在至少80℃和小于140℃的温度下表面,将表面冷却至60℃或更低的温度,并将表面与带部件分离; 以及在所述基板的树脂层侧表面上形成图像记录层。
    • 5. 发明申请
    • RECORDING MEDIUM AND PRODUCING METHOD THEREOF, AND INKJET RECORDING METHOD
    • 记录介质及其制作方法,以及喷墨记录方法
    • US20090130347A1
    • 2009-05-21
    • US12272509
    • 2008-11-17
    • Ryoichi NAKANO
    • Ryoichi NAKANO
    • B32B29/00B05D3/02
    • B41M5/502B41M5/0017B41M7/009
    • The invention provides a recording medium excellent in the water resistance and image fixability and a producing method thereof and an inkjet recording method using the recording medium, comprising: sequentially laminated, a base paper; a first layer containing a binder; and a second layer containing a white pigment and at least one selected from the group consisting of a urethane resin and an acrylic resin, each having a glass transition temperature of 50° C. or less, wherein a Cobb water absorption degree during a contact time of 120 sec in a water absorption test in accordance with JIS P8140 on a surface of the first layer disposed on the base paper is 2.0 g/m2 or less and an amount of water absorption during a contact time of 0.5 sec in the Bristow method on a surface of the second layer is 2 to 8 mL/m2.
    • 本发明提供了耐水性和图像定影性优良的记录介质及其制造方法和使用该记录介质的喷墨记录方法,包括:依次层压原纸; 含有粘合剂的第一层; 和含有白色颜料的第二层和选自聚氨酯树脂和丙烯酸树脂中的至少一种,其中玻璃化转变温度为50℃以下,其中接触时间期间的Cobb吸水度 在布置于基纸上的第一层的表面上,根据JIS P8140的吸水试验中的120秒的吸水率为2.0g / m 2以下,布里斯托方法接触时间为0.5秒时的吸水量为 第二层的表面为2〜8mL / m 2。
    • 8. 发明申请
    • INKJET RECORDING METHOD
    • 喷墨记录方法
    • US20100245512A1
    • 2010-09-30
    • US12714559
    • 2010-03-01
    • Hideki KAIMOTORyoichi NAKANO
    • Hideki KAIMOTORyoichi NAKANO
    • B41J2/01
    • B41M5/0011B41M5/0023C09D11/328C09D11/54
    • Disclosed is an inkjet recording method including recording an image by applying at least one of an ink containing a water-soluble dye of Formula (M), an ink containing a water-soluble dye of Formula (BK), an ink containing a water-soluble dye of Formula (Y), and an ink containing a water-soluble dye of Formula (C) according to an inkjet process, to an inkjet recording medium produced by a method including forming an undercoat layer containing a binder resin and a water-soluble divalent metal salt, to a support; forming a coating film containing at least inorganic fine particles and an acetoacetyl-modified polyvinyl alcohol, on the undercoat layer; and applying a curing solution containing a water-soluble multifunctional compound having two or more amino groups in the molecule, to the coating film, either simultaneously with the forming of the coating film or before the coating film undergoes decreasing-rate drying during drying of the coating film.
    • 公开了一种喷墨记录方法,包括通过涂布含有式(M)的水溶性染料的油墨,含有式(BK)的水溶性染料的油墨,含有水溶性染料的油墨, 将通式(Y)的可溶性染料和根据喷墨方法的含有式(C)的水溶性染料的油墨用于通过包括形成含有粘合剂树脂和水溶性粘合剂树脂的底涂层的方法制备的喷墨记录介质, 可溶性二价金属盐; 在底涂层上形成至少含有无机细颗粒和乙酰乙酰基改性的聚乙烯醇的涂膜; 以及在分子中含有含有两个或多个氨基的水溶性多官能化合物的固化溶液涂布到涂膜上,或者同时形成涂膜,或者在涂膜干燥之前经过降低速率的干燥 涂膜。
    • 10. 发明申请
    • RECORDING MEDIUM AND PRODUCING METHOD THEREOF, AND INKJET RECORDING METHOD
    • 记录介质及其制作方法,以及喷墨记录方法
    • US20090126584A1
    • 2009-05-21
    • US12272369
    • 2008-11-17
    • Ryoichi NAKANO
    • Ryoichi NAKANO
    • B05C17/06
    • B41M5/502B41M5/0017B41M5/504B41M5/506B41M5/52B41M5/5218B41M5/5254B41M7/0036B41M2205/36B41M2205/38
    • The present invention provides a recording medium which can form a high quality image in which curling, image blur, and mixing of colors occurring with image recording are prevented and separation of ink does not easily occur; a method of producing the recording medium; and an ink jet recording method allowing formation of a high quality image at low cost and high speed, including: a stencil (11), a first layer (12) containing a binder, and a second layer (13) containing kaolin and polyvinyl alcohol, the stencil (11), the first layer (12), and the second layer (13) being successively laminated, in which a Cobb water absorption degree during a contact time of 120 seconds by a water absorption test according to JIS P8140 on the surface of the first layer (12) formed on the stencil (11) is 2.0 g/m2 or less; and the water absorption during a contact time of 0.5 second by the Bristow method on the surface of the second layer (13) is from 2 mL/m2 to 8 mL/m2.
    • 本发明提供一种能够形成高质量图像的记录介质,其中防止了图像记录发生的卷曲,图像模糊和混合,并且不容易发生墨的分离; 一种制造该记录介质的方法; 以及允许以低成本和高速度形成高质量图像的喷墨记录方法,包括:模版(11),含有粘合剂的第一层(12)和含有高岭土和聚乙烯醇的第二层(13) ,连续层压模板(11),第一层(12)和第二层(13),其中通过根据JIS P8140的吸水试验在120秒的接触时间内的Cobb吸水度 在模板(11)上形成的第一层(12)的表面为2.0g / m 2以下; 并且通过Bristow方法在0.5秒的接触时间在第二层(13)的表面上的吸水量为2mL / m 2至8mL / m 2。