    • Poly-2-isopropenylnaphthalene-poly-butadiene-1,3-block copolymers and method for their production. Di- or tri-block polymers with molecular weights of at least 10,000 are formed from, respectively, a poly-2-isopropenylnaphthalene block and a poly-butadiene-1,3 block, and a poly-2-isopropenylnaphthalene block and a poly-butadiene-1,3 block as well as a further poly-2-isopropenylnaphthalene block. The products display rubber-elastic characteristics of the known block polymerizates, with improved high-temperature stability. The polymers are formed by reacting 2-isopropenylnaphthalene in an inert, aliphatic or cycloaliphatic hydrocarbon solvent, at low temperature, with alkalimetal, alkalimetalalkylene, -arylene or -hydride catalyst, into a poly-2-isopropenylnaphthalene block. This formed polymeric anion then has poly-butadiene-1,3-block added to it at its active chain end. If necessary, a second poly-2-isopropenylnaphthalene block is added. The reaction becomes terminated in known manner through the addition of water, alcohol or acid. Lithium-alkyl is the preferred catalyst; tetrahydrofuran is the preferred solvent; the reaction is performed at temperatures between 0.degree. and -80.degree. C., preferably between about -50.degree. C. and -80.degree. C. It is also preferred to initially provide the 2-isopropenylnaphthalene in the solvent at about 0.degree. to 5.degree. C.
    • 聚-2-异丙烯基萘 - 聚丁二烯-1,3-嵌段共聚物及其制备方法。 分子量至少为10,000的二嵌段或三嵌段聚合物分别由聚-2-异丙烯基萘嵌段和聚丁二烯-1,3-嵌段和聚-2-异丙烯基萘嵌段和聚 - 丁二烯-1,3-嵌段以及另外的聚-2-异丙烯基萘嵌段。 该产品展示了已知的嵌段聚合物的橡胶弹性特性,具有改善的高温稳定性。 聚合物是通过使2-异丙烯基萘在惰性,脂族或脂环族烃溶剂中在低温下与碱金属,碱金属亚烷基, - 亚芳基 - 酐催化剂反应,形成聚-2-异丙烯基萘嵌段。 然后,形成的聚合物阴离子在其活性链端加入聚丁二烯-1,3-嵌段。 如果需要,加入第二聚-2-异丙烯基萘嵌段。 反应以已知方式通过加入水,醇或酸终止。 锂 - 烷基是优选的催化剂; 四氢呋喃是优选的溶剂; 该反应在0℃至-80℃之间的温度下进行,优选在约-50℃至-80℃之间进行。最好在约0℃至5℃下最初在溶剂中提供2-异丙烯基萘 DEG C.