    • 1. 发明授权
    • Use of low unsaturated polyether polyols in high resilience slabstock foam applications
    • 在高弹性板坯泡沫应用中使用低不饱和聚醚多元醇
    • US06201035B1
    • 2001-03-13
    • US09578208
    • 2000-05-24
    • Roeland TuinmanThomas B. LeeThomas L. FishbackCurtis J. Reichel
    • Roeland TuinmanThomas B. LeeThomas L. FishbackCurtis J. Reichel
    • C08G1848
    • C08G18/4866C08G18/4072C08G18/4816C08G2101/0008C08G2101/005C08G2101/0083Y10S521/914
    • The present invention discloses a method for the formation of and a flexible slabstock polyurethane foam having substantially improved indentation force deflection and resilience characteristics while maintaining the other physical properties. The method comprises the steps of: forming a polyol blend having a nominal functionality of at least 2.3 by combining at least one polyether polyol having a plurality of terminal ethylene oxide caps of from 5 to 25% by weight based on the total weight of the polyether polyol, a molecular weight of greater than or equal to 4000 Daltons, and an unsaturation of greater than 0.04 meq/g KOH; at least one graft polyether polyol having an equivalent weight of greater than 1000 Daltons, a solids content of at least 28%, and a plurality of terminal ethylene oxide caps of from 5 to 25% by weight based on the total weight of the graft polyether polyol; and at least one very low unsaturated polyether polyol having an unsaturation of less than or equal to 0.018 meq/g KOH and a plurality of terminal ethylene oxide caps of from 5 to 25% by weight based on the total weight of the polyether polyol; providing at least one polyisocyanate component; providing a catalyst; providing water as a blowing agent at a level of between 3 to 7% by weight; and combining the polyol blend with the polyisocyanate component, the catalyst and the water to form a slabstock polyurethane foam.
    • 本发明公开了一种用于形成柔性板坯聚氨酯泡沫的方法,其具有显着改善的压痕力偏转和弹性特性,同时保持其它物理性能。 该方法包括以下步骤:通过组合至少一种具有多个端基环氧乙烷盖的聚醚多元醇形成多元醇共混物,所述多元醇共混物具有至少2.3的标称官能度,基于聚醚的总重量为5至25重量% 多元醇,分子量大于或等于4000道尔顿,不饱和度大于0.04meq / g KOH; 至少一种接枝聚醚多元醇,其当量重量大于1000道尔顿,固体含量至少为28%,多个末端环氧乙烷盖为5至25重量%,基于接枝聚醚的总重量 多元醇 和至少一种具有小于或等于0.018meq / g KOH的不饱和度的非常低的不饱和聚醚多元醇和基于聚醚多元醇总重量的5至25重量%的多个末端环氧乙烷盖; 提供至少一种多异氰酸酯组分; 提供催化剂; 以3至7重量%的水平提供水作为发泡剂; 并将多元醇共混物与多异氰酸酯组分,催化剂和水混合以形成板块聚氨酯泡沫。
    • 2. 发明授权
    • Use of low unsaturated polyether polyols in slabstock foam applications
    • 在块状泡沫塑料应用中使用低不饱和聚醚多元醇
    • US06344494B1
    • 2002-02-05
    • US09579239
    • 2000-05-24
    • Roeland TuinmanThomas L. FishbackCurtis J. Reichel
    • Roeland TuinmanThomas L. FishbackCurtis J. Reichel
    • C08G1814
    • C08G18/4841C08G18/4866C08G2101/0008C08G2101/005C08G2101/0083
    • The present invention discloses a method for the formation of a flexible slabstock polyurethane foam having substantially improved indentation force deflection and resilience characteristics while maintaining the other physical properties. The method comprises the steps of reacting a triol polyoxyalkylene polyether polyol having a plurality of internal blocks formed from oxyalkylene monomers with a plurality of terminal caps comprising ethylene oxide attached to said plurality of internal blocks, the internal blocks containing at least 80% by weight propylene oxide based on the total weight of all of the oxyalkylenes in said internal blocks and the amount of ethylene oxide in the terminal caps comprising from 5 to 25% by weight based on the total weight of the polyol, said polyol having a degree of unsaturation of less than or equal to 0.015 meq/g KOH with a polyisocyanate component in the presence of a catalyst and water as a blowing agent at a level of between 3 to 7% by weight.
    • 本发明公开了一种用于形成柔性板状聚氨酯泡沫的方法,其具有显着改善的压痕力偏转和弹性特性,同时保持其它物理特性。 该方法包括使具有多个由氧化烯单体形成的多个内部嵌段的三醇聚氧化烯聚醚多元醇与多个连接到所述多个内部嵌段上的环氧乙烷的端帽反应的步骤,内部嵌段含有至少80重量%的丙烯 氧化物,基于所述内部嵌段中所有的氧化烯的总重量,末端盖中的环氧乙烷的量为5至25重量%,基于多元醇的总重量,所述多元醇的不饱和度为 在催化剂存在下,多异氰酸酯成分的含量小于或等于0.015meq / g KOH,发泡剂水为3〜7重量%。
    • 8. 发明授权
    • Sealants made using low unsaturation polyoxyalkylene polyether polyols
    • 使用低不饱和度的聚氧化烯聚醚多元醇制成的密封剂
    • US6103850A
    • 2000-08-15
    • US754565
    • 1996-11-21
    • Curtis J. ReichelThomas L. FishbackGladys M. Aviles
    • Curtis J. ReichelThomas L. FishbackGladys M. Aviles
    • C08G18/10C08G18/12C08G18/48C08G65/26C08G18/06
    • C08G18/12C08G18/4854C08G18/4866C08G65/2609C08G65/2696C08G2190/00
    • There is provided an sealant made with an isocyanate or hydroxyl terminated prepolymer made by reacting a stoichiometric excess of an organic polyisocyanate with polyols made of at least a polyoxyalkylene polyether triol or a mixture thereof with a polyoxyalkylene polyether diol. The triol or diol has within its structure the nucleus of an initiator compound, an internal blocks of oxypropylene groups, and external blocks of oxyalkylene groups, wherein the internal blocks of oxypropylene are between said nucleus and said external blocks, said external blocks are made of oxyalkylene groups derived from a C.sub.4 or higher alkylene oxide. The amount of the internal blocks of oxypropylene groups is from 25 weight percent to 80 weight percent based on the weight of all oxyalkylene groups and initiator in the prepolymer The triol or diol has a compatibility index of 25.degree. C. or less, and may be part of a two component or a one component moisture cured sealant.
    • 提供了由异氰酸酯或羟基封端的预聚物制成的密封剂,其通过使化学计量过量的有机多异氰酸酯与由聚氧化烯聚醚三醇或其与聚氧化烯聚醚二醇的混合物制成的多元醇反应制备。 三醇或二醇在其结构内具有引发剂化合物的核,氧化丙烯基的内部嵌段和氧化烯基的外部嵌段,其中氧化丙烯的内部嵌段位于所述核和所述外部嵌段之间,所述外部嵌段由 衍生自C4或更高级烯化氧的氧化烯基。 基于所有氧化烯基团的重量和预聚物中的引发剂,氧化丙烯基团的内部嵌段的量为25重量%至80重量%。三醇或二醇的相容指数为25℃以下,可以为 一部分是双组分或一种组分的湿气固化密封剂。