会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 4. 发明申请
    • INTERCALATION AGENT FREE COMPOSITIONS USEFUL TO MAKE NANOCOMPOSITE POLYMERS
    • 交联剂自由组合物有助于制备纳米聚合物聚合物
    • US20100063183A1
    • 2010-03-11
    • US12515692
    • 2007-11-16
    • Luyi SunJae Boo WoongHung-Jue SueMaurice J. MarksRichard F. FibigerMichael S. Paquette
    • Luyi SunJae Boo WoongHung-Jue SueMaurice J. MarksRichard F. FibigerMichael S. Paquette
    • C04B14/04C04B14/20C04B14/10C08L63/00C08L23/00C08L33/24C08L33/00C08L69/00C08L81/00C08L71/00C08L27/00C08L83/04
    • C08J3/2053B82Y30/00C08J5/005C08J2363/00Y10S977/778Y10S977/779Y10S977/783Y10S977/785Y10S977/786Y10S977/787
    • A two step method for preparing a filler composition, the filler composition useful to prepare a nanocomposite polymer. The first step is to disperse a water dispersible filler material in a liquid comprising water to form a dispersion. The second step is to replace at least a portion of the water of the liquid with an organic solvent to form the filler composition, the water concentration of the liquid of the filler composition being less than six percent by weight, the average size of at least one dimension of the filler material being less than two hundred nanometers upon examination by transmission electron microscopy of a representative freeze dried sample of the dispersion of the first step. A nanocomposite polymer can be prepared by mixing the above-made filler composition with one or more polymer, polymer component, monomer or prepolymer to produce a polymer containing a filler having an average size of at least one dimension of the filler of less than two hundred nanometers upon examination by transmission electron microscopy of a representative sample of the polymer. In addition, an epoxy resin composition useful for making a cured epoxy nanocomposite polymer, the epoxy resin composition made by a two step process. The first step is to mix an epoxy resin with the filler composition to form an epoxy resin mixture. The second step is to remove organic solvent from the epoxy resin mixture to form the epoxy resin composition. And, a nanocomposite polymer, made by the step of mixing the filler composition with one or more polymer, polymer component, monomer or prepolymer to produce a polymer containing a filler having an average size of at least one dimension of the filler of less than two hundred nanometers upon examination by transmission electron microscopy of a representative sample of the polymer.
    • 用于制备填料组合物的两步法,该填料组合物可用于制备纳米复合材料聚合物。 第一步是将水分散性填料分散在包含水的液体中以形成分散体。 第二步是用有机溶剂代替液体的至少一部分水以形成填料组合物,填料组合物的液体的水浓度小于6重量%,至少平均尺寸 通过透射电子显微镜检查第一步骤的分散体的代表性冷冻干燥样品,填充材料的一个尺寸小于二百纳米。 可以通过将上述填充剂组合物与一种或多种聚合物,聚合物组分,单体或预聚物混合来制备纳米复合聚合物,以制备含有填料的至少一维尺寸小于二百 通过透射电子显微镜检查聚合物的代表性样品的纳米。 另外,用于制备固化的环氧纳米复合材料聚合物的环氧树脂组合物,通过两步法制备环氧树脂组合物。 第一步是将环氧树脂与填料组合物混合以形成环氧树脂混合物。 第二步是从环氧树脂混合物中除去有机溶剂,形成环氧树脂组合物。 而且,纳米复合聚合物通过将填料组合物与一种或多种聚合物,聚合物组分,单体或预聚物混合以制备含有填料平均尺寸至少小于二维填料小于2的填料的步骤制备 通过透射电子显微镜检查聚合物的代表性样品的百纳米。