    • 1. 发明申请
    • Coating Compositions With Anticorrosion Properties
    • 具有防腐蚀性能的涂料组合物
    • US20120094130A1
    • 2012-04-19
    • US12905999
    • 2010-10-15
    • Raymond E. FoscanteFernando GalembeckMelissa Braga
    • Raymond E. FoscanteFernando GalembeckMelissa Braga
    • C23F11/00B32B15/082B32B15/092
    • C09D5/084Y10T428/31529Y10T428/31699
    • Anticorrosive coating compositions comprise a binding polymer and an amorphous aluminum phosphate corrosion inhibiting pigment. The composition comprises from about 1 to 25 percent by weight amorphous aluminum phosphate. The amorphous aluminum phosphate has a water adsorption potential of up to about 25 percent by weight water. The composition provides a controlled phosphate delivery of from about 50 to 500 ppm, and preferably of from about 100 to 200 ppm. The composition has a total solubles content of less than about 1,500 ppm. The amorphous aluminum phosphate is preferably substantially free of alkali metals. The amorphous aluminum phosphate is made by combining aluminum hydroxide with phosphoric acid and sodium aluminate. The amorphous aluminum phosphate is treated to reduce the level of unwanted solubles, and the treated amorphous aluminum phosphate is dried at less than about 300° C. The composition is used as a primer coat, a mid-coat, and/or a top-coat coating.
    • 防腐涂料组合物包含结合聚合物和无定形磷酸铝腐蚀抑制颜料。 该组合物包含约1至25重量%的无定形磷酸铝。 无定形磷酸铝具有高达约25重量%水的吸水势。 组合物提供约50至500ppm,优选约100至200ppm的受控磷酸盐递送。 该组合物的总可溶物含量小于约1,500ppm。 无定形磷酸铝优选基本上不含碱金属。 无定形磷酸铝由氢氧化铝与磷酸和铝酸钠组合而成。 处理无定形磷酸铝以降低不需要的可溶物的水平,并将处理的无定形磷酸铝在小于约300℃下干燥。该组合物用作底漆,中涂层和/ 涂层涂层。
    • 8. 发明申请
    • Aluminum Phosphate, Polyphosphate, and Metaphosphate Particles and Their Use as Pigments in Paints and Method of Making Same
    • 磷酸铝,多磷酸盐和偏磷酸盐颗粒及其在油漆中的颜料用途及其制备方法
    • US20100292382A1
    • 2010-11-18
    • US12844625
    • 2010-07-27
    • Fernando GalembeckJoäo de Brito
    • Fernando GalembeckJoäo de Brito
    • C08K3/32
    • C09D7/61C01B25/36C01B25/40C01B25/44C01B25/45C01B25/451C08K3/32C08K7/24C08K2003/327C09D7/67C09D7/68C09D11/037
    • An aluminum phosphate composition comprising aluminum phosphate, aluminum polyphosphate, aluminum metaphosphate, or a mixture thereof. The composition may be characterized by, when in powder form, having particles wherein some of the particles have at least one or more voids per particle. In addition, the composition is characterized by exhibiting two endothermic peaks in Differential Scanning Calorimetry between about 90 degrees to about 250 degrees Celsius. The composition is also characterized by, when in powder form, having a dispersibility of at least 0.025 grams per 1.0 gram of water. The composition is made by a process comprising contacting phosphoric acid with aluminum sulfate and an alkaline solution to produce an aluminum phosphate based product; and optionally calcining the aluminum phosphate, polyphosphate or metaphosphate based product at an elevated temperature. The composition is useful in paints and as a substitute for titanium dioxide.
    • 一种磷酸铝组合物,其包含磷酸铝,多磷酸铝,偏磷酸铝,或其混合物。 组合物的特征可以在于粉末形式时具有颗粒,其中一些颗粒每个颗粒具有至少一个或多个空隙。 此外,组合物的特征在于在差示扫描量热法中在约90摄氏度至约250摄氏度之间显示出两个吸热峰。 组合物的特征还在于,当其为粉末形式时,其具有至少0.025克/ 1.0克水的分散性。 该组合物通过包括使磷酸与硫酸铝和碱性溶液接触以制备磷酸铝基产物的方法制备; 并且任选地在升高的温度下煅烧磷酸铝,多磷酸盐或偏磷酸盐基产品。 该组合物可用于涂料和作为二氧化钛的替代物。
    • 9. 发明授权
    • Aluminum phosphate, polyphosphate and metaphosphate particles and their use as pigments in paints and method of making same
    • 磷酸铝,多磷酸盐和偏磷酸盐颗粒及其在油漆中的用途及其制备方法
    • US07763359B2
    • 2010-07-27
    • US11364798
    • 2006-02-27
    • Fernando GalembeckJoäo de Brito
    • Fernando GalembeckJoäo de Brito
    • B32B15/16C01B15/16C08K3/32
    • C09D7/61C01B25/36C01B25/40C01B25/44C01B25/45C01B25/451C08K3/32C08K7/24C08K2003/327C09D7/67C09D7/68C09D11/037
    • An aluminum phosphate composition comprising aluminum phosphate, aluminum polyphosphate, aluminum metaphosphate, or a mixture thereof. The composition may be characterized by, when in powder form, having particles wherein some of the particles have at least one or more voids per particle. In addition, the composition is characterized by exhibiting two endothermic peaks in Differential Scanning Calorimetry between about 90 degrees to about 250 degrees Celsius. The composition is also characterized by, when in powder form, having a dispersibility of at least 0.025 grams per 1.0 gram of water. The composition is made by a process comprising contacting phosphoric acid with aluminum sulfate and an alkaline solution to produce an aluminum phosphate based product; and optionally calcining the aluminum phosphate, polyphosphate or metaphosphate based product at an elevated temperature. The composition is useful in paints and as a substitute for titanium dioxide.
    • 一种磷酸铝组合物,其包含磷酸铝,多磷酸铝,偏磷酸铝,或其混合物。 组合物的特征可以在于粉末形式时具有颗粒,其中一些颗粒每个颗粒具有至少一个或多个空隙。 此外,组合物的特征在于在差示扫描量热法中在约90摄氏度至约250摄氏度之间显示出两个吸热峰。 组合物的特征还在于,当其为粉末形式时,其具有至少0.025克/ 1.0克水的分散性。 该组合物通过包括使磷酸与硫酸铝和碱性溶液接触以制备磷酸铝基产物的方法制备; 并且任选地在升高的温度下煅烧磷酸铝,多磷酸盐或偏磷酸盐基产品。 该组合物可用于涂料和作为二氧化钛的替代物。