    • 4. 发明授权
    • Manufacture of thermoplastic polyester molding compositions of high
viscosity
    • 制造高粘度热塑性聚酯成型组合物
    • US4031065A
    • 1977-06-21
    • US660137
    • 1976-02-23
    • Claus CordesHans-Josef Sterzel
    • Claus CordesHans-Josef Sterzel
    • C08G63/00C08G63/52C08L67/06C09D167/06
    • C08L67/06C08G63/52C09D167/06
    • Thermoplastic polyesters having a melt viscosity of more than 6,000 poise, as measured at 250.degree. C, and a relative solution viscosity of more than 1.6, as measured on a 2:1 mixture of phenol/o-dichlorobenzene at 25.degree. C, composed of aliphatic and/or cycloaliphatic diols on the one hand and dicarboxylic acids or esters thereof on the other hand and of from 0.1 to 10% molar of an aliphatic diol containing at least one olefinic double bond and/or of an aliphatic dicarboxylic acid containing at least one olefinic double bond or an ester thereof, said olefinic double bond not being directly adjacent to the carboxyl or ester groups. The polyesters are manufactured by melt polycondensation of diols with dicarboxylic acids or esters thereof, which polycondensation is carried out for at least some of the time at a temperature above 220.degree. C and preferably above 230.degree. C, the reaction being carried out in the presence of from 0.1 to 10% molar of an aliphatic diol containing at least one olefinic double bond and/or of an aliphatic dicarboxylic acid containing at least one olefinic double bond or an ester thereof, said olefinic double bond not being directly adjacent to the carboxyl or ester groups.
    • 在250℃下测量的熔体粘度大于6000泊的热塑性聚酯,和在25℃下苯酚/邻二氯苯的2:1混合物测量的相对溶液粘度大于1.6的热塑性聚酯,由 一方面是脂族和/或脂环族二醇,另一方面是二羧酸或其酯,和0.1-10%摩尔含有至少一个烯属双键的脂族二醇和/或至少含有脂族二羧酸 一个烯属双键或其酯,所述烯属双键不直​​接与羧基或酯基相邻。 聚酯通过二醇与二羧酸或其酯的熔融缩聚制备,其在220℃以上,优选230℃以上的温度进行至少一段时间的缩聚,该反应在存在下进行 含有至少一个烯属双键的脂族二醇和/或含有至少一个烯属双键的脂族二羧酸的0.1至10摩尔%或其酯,所述烯属双键不直​​接与羧基或 酯基。
    • 10. 发明授权
    • Preparation of terpolymers
    • 三元共聚物的制备
    • US4282342A
    • 1981-08-04
    • US072985
    • 1979-09-06
    • Walter DenzingerClaus Cordes
    • Walter DenzingerClaus Cordes
    • C08F220/00C08F220/04C08F222/06
    • C08F222/06
    • Terpolymers which have Fikentscher K-values of from 8 to 100 and comprise 50 mole percent of maleic anhydride units, from 35 to 45 mole percent of 2,4,4'-trimethylpent-1-ene units and from 5 to 15 mole percent of 2,4,4'-trimethylpent-2-ene units, and processes for their preparation by polymerizing 50 parts by weight of maleic anhydride, from 35 to 180 parts by weight of 2,4,4'-trimethylpent-1-ene and from 0.6 to 6 parts by weight of 2,4,4'-trimethylpent-2-ene per part by weight of 2,4,4'-trimethylpent-1-ene employed, in the presence of a free-radical initiator at from 60.degree. to 200.degree. C. and a pressure of from 1 to 20 bar, and separating the terpolymers from the unconverted monomers.
    • 具有8至100的Fikentscher K值和包含50摩尔%马来酸酐单元,35至45摩尔%的2,4,4'-三甲基戊-1-烯单元和5至15摩尔%的马来酸酐单元的三元共聚物 2,4,4'-三甲基戊-2-烯单元,以及它们通过聚合50重量份马来酸酐制备的方法,35至180重量份的2,4,4'-三甲基戊-1-烯和 在使用自由基引发剂的存在下,使用0.6至6重量份的2,4,4'-三甲基戊-2-烯每重量份的2,4,4'-三甲基戊-1-烯, 60℃至200℃,压力为1至20巴,并将三元共聚物与未转化的单体分离。