    • Rolling part steel
    • 轧制钢
    • US5447579A
    • 1995-09-05
    • US164840
    • 1993-12-09
    • Kiyoshi HirakawaNorifumi Ikeda
    • Kiyoshi HirakawaNorifumi Ikeda
    • C22C38/00C22C38/60F16C33/32F16C33/34F16C33/62
    • C22C38/60F16C33/62Y10S148/906
    • A rolling part steel with which the strength of a rolling part of a cold-worked bearing is improved compared with that of a conventional turned part by controlling the length and number of sulfide inclusions in the steel to an optimal range, when a rolling part steel is prepared so that the maximum length of sulfide inclusions in the steel is 100 .mu.m or less and that a number of sulfide inclusions whose lengths exceed 40 .mu.m is 50 or less per unit area (160 mm.sup.2) , the roughness of its bore surface is improved to have a greater strength. As a result, for example, a thus formed raceway ring has a longer life against fatigue-induced cracks than a turned raceway ring.
    • 通过将轧制部分钢中的硫化物夹杂物的长度和数量控制在最佳范围内,与现有的轧制部分相比,冷轧轴承的轧制部分的强度提高了的滚动部件钢 制成钢的硫化物夹杂物的最大长度为100μm以下,长度超过40μm的硫化物夹杂物的数量为每单位面积(160mm 2)为50以下,其孔面的粗糙度 被改进以具有更大的实力。 结果,例如,如此形成的滚道环比转动的滚道环具有比疲劳引起的裂纹更长的寿命。